Wire arc additive manufacturing of ER70S-6/S355 bimetal component

被引:5
|
作者
Zhai, Wengang [1 ]
Guo, Yibo [1 ]
Aishwarya [2 ]
Canturri, Carla [2 ]
Shandro, Robert [2 ]
Zhou, Wei [1 ]
机构
[1] Nanyang Technol Univ, Singapore Ctr 3D Printing, Sch Mech & Aerosp Engn, 50 Nanyang Ave, Singapore 639798, Singapore
[2] CETIM Matcor Technol & Serv Pte Ltd, 3 Seletar Aerosp Link, Singapore 797550, Singapore
关键词
Additive manufacturing; Dissimilar joining; Multimaterial structure; Heat treatment; Tensile properties; 316L STAINLESS-STEEL; MECHANICAL-PROPERTIES; ALLOY; MICROSTRUCTURE; PARTS; GMAW;
D O I
10.1016/j.msea.2024.146498
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Among the various fusion-based additive manufacturing processes, wire arc additive manufacturing (WAAM) has the highest deposition rate, which is beneficial for fabricating large volume components. The WAAM process usually begins with printing on a substrate, that could act as a functional part of the component. To study the possibilities of fabricating multimaterial structure, a highly dense ER70S-6 was directly fabricated on an S355 substrate using the WAAM process. Microstructural studies revealed a good fusion and bonding at the interface. Equiaxed grains were observed in the plasma WAAM process fabricated ER70S-6 and the interface. For the asbuilt condition, the WAAM-built ER70S-6/S355 bimetal joint has a yield strength of 349 MPa; a UTS of 503.5 MPa; and an elongation of 30%. The yield strength and UTS of WAAM-built ER70S-6 and as-received S355 are close. The fracture occurs on the S355 side of the as-built ER70S-6/S355 bimetal joint because the as-built ER70S-6 has a higher elongation than S355 (40.2% vs 33.2%). After quenching heat treatment, the WAAMbuilt ER70S-6/S355 bimetal joint has a yield strength of 511.6 MPa; a UTS of 740.7 MPa; and an elongation of 20.1%. The fracture occurs on the ER70S-6 side because it has a low yield strength and UTS. This work demonstrates that dissimilar substrate can be used for WAAM process to fabricate multimaterial structures.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] ER70S-6盘条拉拔断裂分析
    王晓华
    关玉佐
    孙孝男
    张利红
    天津冶金, 2002, (06) : 26 - 27
  • [42] ER70S-6连铸坯高温塑性研究
    张永军
    韩静涛
    孔俊其
    侯月华
    张素萍
    马富平
    李军
    甄琴英
    金属材料与冶金工程, 2009, 37 (05) : 3 - 6+56
  • [43] ER70S-6焊丝钢拉拔断裂原因分析
    涛雅
    赵晓敏
    周乐育
    谭晓东
    吕刚
    热加工工艺, 2019, 48 (01) : 259 - 262
  • [44] ER70S-6焊丝钢可浇性研究
    常凤
    李硕
    刘善喜
    河北冶金, 2017, (10) : 32 - 34
  • [45] ER70S-6气体保护焊丝钢的试制
    李正嵩
    冶金标准化与质量, 2010, 48 (05) : 39 - 41+56
  • [46] ER70S-6盘条拉拔试验分析
    于同仁
    刘开升
    金属制品, 2004, (02) : 16 - 18
  • [47] Effect of travel speed and number of layers on surface waviness of ER70S6 deposits fabricated through non-transferred wire arc additive manufacturing
    Pattanayak, Suvranshu
    Sahoo, Susanta Kumar
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2023, 37 (24) : 3622 - 3651
  • [48] Microstructure and Properties of ER50-6 Steel Fabricated by Wire Arc Additive Manufacturing
    Hu, Qingxian
    Miao, Junyan
    Wang, Xiaoli
    Li, Chengtao
    Fang, Kewei
    SCANNING, 2021, 2021
  • [49] Effect of controlled cooling rate in phase transformation zone on structure and properties of wire rod of steel ER70S-6
    Ding, Hua
    Wang, Li
    Liu, Yazheng
    Zhang, Lifen
    Teshugang/Special Steel, 2001, 22 (06):
  • [50] 提高ER70S-6焊丝钢质量的工艺措施
    梁鹏
    梅忠
    刘春森
    河北冶金, 2017, (05) : 37 - 40