Microstructural modifications of lime-based mortars induced by ceramics and nanoparticle additives

被引:0
|
作者
Sierra-Fernandez, Aranzazu [1 ]
Sotiriadis, Konstantinos [2 ,3 ]
Ergenc, Duygu [4 ]
Gomez-Villalba, Luz S. [1 ]
Barbero-Barrera, M. Mar [5 ]
Len, Adel [6 ,7 ]
Slizkova, Zuzana [2 ]
Fort, Rafael [1 ]
机构
[1] UCM, CSIC, Inst Geociencias, C-Doctor Severo Ochoa 7, Madrid 28040, Spain
[2] Inst Theoret, Appl Mech Czech Acad Sci, Prosecka 809-76, Prague 19000, Czech Republic
[3] South Ural State Univ, Natl Res Univ, Dept Bldg Mat & Prod, Pr Lenina 76, RU-454080 Chelyabinsk, Russia
[4] Middle East Tech Univ, Conservat & Cultural Heritage Grad Program, Ankara, Turkiye
[5] Univ Politecn Madrid, Escuela Tecn Super Arquitectura, Avda Juan de Herrera 4, Madrid 28040, Spain
[6] REN Ctr Energy Res, HUN, Konkoly Thege Miklo Sut 29-33, H-1121 Budapest, Hungary
[7] Univ Pecs, Fac Engn & Informat Technol, Boszorkany Ut 2, H-7624 Pecs, Hungary
来源
关键词
Air lime-based mortar; Nanoparticles; Red-clay ceramic waste; Microstructure; Pozzolanity; Mechanical performance; S-H GEL; MECHANICAL-PROPERTIES; HYDRATING CEMENT; HARDENED STATE; X-RAY; CARBONATION; POZZOLANA; CONSOLIDATION; BYZANTINE; PRODUCTS;
D O I
10.1016/j.jobe.2024.109672
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Lime-based mortars are one of the principal choices for building and restoration projects, owing to their unique qualities and material compatibility. Admixtures have long been incorporated to enhance the performance and durability of mortars, with ceramics being a traditional choice. More recently, the addition of nanoparticles has been explored as a means to further improve these properties. However, the effective optimization of the complex interplay between additives in lime-based mortars, which is crucial for enhancing their sustainability, remains an ongoing area of research. This study investigated the effects of red-clay ceramic aggregates (RCC) and nanoparticle-based solutions of Ca(OH)2 and SiO2 on the mineralogy, hydraulicity, surface properties, pore structure, and mechanical properties of lime-based mortars. The addition of nanoparticle-based solutions increased the carbonation reactivity, whereas the ceramic aggregates caused a more extensive conversion of portlandite to calcite on the external faces, indicating reduced porosity during the carbonation process. Pozzolanic reactions and the formation of new calcium silicate compounds were observed, along with improved compaction, smoother surfaces, and microcrack formation. The porosity increased with the addition of the ceramic aggregates, whereas the addition of nanoparticles significantly increased the number of pores in the mesoporous range. The specific surface area of the mortars increased with the inclusion of ceramic aggregates and nanoparticles, whereas the open porosity increased and the density and compressive strength decreased with the addition of nanoparticles and associated pozzolanic reactions that occurred with the inclusion of ceramic aggregates. These findings lay the groundwork for future improvements in the formulation of lime-based mortars to balance hydraulicity, surface characteristics, and mechanical performance while preserving porosity.
引用
收藏
页数:19
相关论文
共 50 条
  • [41] Contribution of thermal analysis in the characterization of lime-based mortars with oxblood addition
    Zhang, Kun
    Grimoldi, Alberto
    Rampazzi, Laura
    Sansonetti, Antonio
    Corti, Cristina
    THERMOCHIMICA ACTA, 2019, 678
  • [42] Micro-destructive evaluation of the mechanical properties of lime-based mortars
    Kyriakou, Loucas
    Theodoridou, Magdalini
    Ioannou, Ioannis
    JOURNAL OF CULTURAL HERITAGE, 2022, 58 : 219 - 228
  • [43] Proposal of New Natural Hydraulic Lime-Based Mortars for the Conservation of Historical Buildings
    Destefani, Marco
    Falchi, Laura
    Zendri, Elisabetta
    COATINGS, 2023, 13 (08)
  • [44] A State-of-the-art Review on Lime-based Mortars for Restoration of Ancient Buildings
    Lan M.
    Nie S.
    Wang J.
    Zhang Q.
    Chen Z.
    Cailiao Daobao/Materials Reports, 2019, 33 (05): : 1512 - 1516
  • [45] Crystal development during carbonation of lime-based mortars in different environmental conditions
    Ergenc, Duygu
    Gomez-Villalba, Luz S.
    Fort, Rafael
    MATERIALS CHARACTERIZATION, 2018, 142 : 276 - 288
  • [46] Experimental testing of the durability of lime-based mortars used for rendering historic buildings
    Arizzi, A.
    Viles, H.
    Cultrone, G.
    CONSTRUCTION AND BUILDING MATERIALS, 2012, 28 (01) : 807 - 818
  • [47] THERMAL-ANALYSIS (TA) OF LIME-BASED AND GYPSUM-BASED MEDIEVAL MORTARS
    ADAMS, J
    KNELLER, W
    DOLLIMORE, D
    THERMOCHIMICA ACTA, 1992, 211 : 93 - 106
  • [48] Influence of Aggregate Stiffness on Fracture-Mechanical Properties of Lime-Based Mortars
    Tesarek, Pavel
    Nezerka, Vaclav
    Padevet, Pavel
    Antos, Jakub
    Plachy, Tomas
    EXPERIMENTAL STRESS ANALYSIS 51, 2014, 486 : 289 - 294
  • [49] Effect of water-repellent admixtures on the behaviour of aerial lime-based mortars
    Izaguirre, A.
    Lanas, J.
    Alvarez, J. I.
    CEMENT AND CONCRETE RESEARCH, 2009, 39 (11) : 1095 - 1104
  • [50] Textile-to-mortar bond behaviour in lime-based textile reinforced mortars
    Dalalbashi, Ali
    Ghiassi, Bahman
    Oliveira, Daniel V.
    CONSTRUCTION AND BUILDING MATERIALS, 2019, 227