Deformation mechanisms of the Fe 40 Mn 20 Cr 20 Ni 20 high entropy alloy upon dynamic tension

被引:1
|
作者
Wang, Shikang [1 ]
Liu, Kunyang [1 ]
Wang, Zhong [2 ]
Jin, Xi [1 ]
Zhang, Min [1 ]
Qiao, Junwei [1 ,3 ]
Wang, Zhihua [2 ]
机构
[1] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan 030024, Peoples R China
[2] Taiyuan Univ Technol, Inst Appl Mech, Coll Mech & Vehicle Engn, Taiyuan 030024, Peoples R China
[3] Taiyuan Univ Technol, Key Lab Interface Sci & Engn Adv Mat, Minist Educ, Taiyuan 030024, Peoples R China
基金
中国国家自然科学基金;
关键词
High entropy alloys (HEAs); Dynamic tension; Controlled strain; Deformation mechanism; Work hardening; CRYOGENIC STRENGTH; SIGMA-PHASE; TRANSFORMATION; COMPRESSION; BEHAVIOR; STEELS;
D O I
10.1016/j.msea.2024.146583
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, the Fe 40 Mn 20 Cr 20 Ni 20 HEA is successfully prepared, and the deformation mechanism and microstructure evolution upon dynamic tension are investigated. The alloy achieves excellent strength -ductility synergies and extraordinary work -hardening capabilities under conditions of decreasing the temperature or increasing the strain rate. After cold rolling and annealing, the Fe 40 Mn 20 Cr 20 Ni 20 HEA exhibited apparent secondary work hardening during dynamic tension (the temperature is 298 K and the strain rate is -1400 s -1 ). The yield strength and ultimate tensile strength increased from -416 to -555 MPa and from -742 to higher than 950 MPa, respectively. At the same time, the plasticity is increased. This improvement is similar to that at cryogenic temperature and quasi -static tension (the temperature is 77 K and the strain rate is -10 -3 s -1 ). The above two cases have a different deformation mechanism. The activation and evolution of the deformation mechanism under dynamic loading at room temperature with increasing strain are determined through dynamic interruption experiments. Deformation mechanisms such as dislocations, nano -twins, stacking faults & deformation twin networks, precipitated phases, and possibly 9R phases undergo evolutions with increasing plastic deformation. Their extensive interactions are the dominant reasons for the improved mechanical performance, which is rarely identified under quasi -static deformation. The sigma phase plays a crucial role during the plastic deformation of the alloy at high strain rates, delaying the onset of necking together with deformation twins.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Microstructures and deformation mechanisms of Cr26Mn20Fe20Co20Ni14 alloys
    Ming, Kaisheng
    Bi, Xiaofang
    Wang, Jian
    MATERIALS CHARACTERIZATION, 2017, 134 : 194 - 201
  • [22] Point Defects and Their Properties in the Fe20Ni20Cr20Co20Cu20High-Entropy Alloy
    Kretova, M. A.
    Konchakov, R. A.
    Kobelev, N. P.
    Khonik, V. A.
    JETP LETTERS, 2020, 111 (12) : 679 - 684
  • [23] Effect of 0.3 at. % Ce on the corrosion resistance of Fe40Ni20Co20Cr20 40 Ni 20 Co 20 Cr 20 high-entropy alloy in 3.5 wt% NaCl solution
    Guo, Qiang
    Liu, Bin
    Li, Qiang
    Xie, Jiuqi
    MATERIALS LETTERS, 2024, 364
  • [24] High-temperature tensile behavior and constitutive model in Co-free Fe40Mn20Cr20Ni20 high-entropy alloy
    Li, Fan
    Han, Lina
    Wang, Xuejiao
    Lan, Aidong
    Qiao, Junwei
    JOURNAL OF APPLIED PHYSICS, 2024, 135 (20)
  • [25] Formation of texture and twinning at 296 K of " Artificial " polycrystals of an equiatomic Co 20 Cr 20 Fe 20 Ni 20 Mn 20 High-entropy alloy
    Kireeva, I. V.
    Chumlyakov, Yu. I.
    Kuksgauzen, I. V.
    Kuksgauzen, D. A.
    MATERIALS LETTERS, 2024, 367
  • [26] The tension-compression asymmetry of martensite phase transformation in a metastable Fe40Co20Cr20Mn10Ni10 high-entropy alloy
    An, Xinglong
    Wang, Zhangwei
    Ni, Song
    Song, Min
    SCIENCE CHINA-MATERIALS, 2020, 63 (09) : 1797 - 1807
  • [27] High strength and ductility in partially recrystallized Fe40Mn20Cr20Ni20 high-entropy alloys at cryogenic temperature
    Ma, Qi-Xin
    Yang, Hui-Jun
    Wang, Zhong
    Shi, Xiao-Hui
    Liaw, Peter K.
    Qiao, Jun-Wei
    MICROSTRUCTURES, 2022, 2 (03):
  • [28] Point Defects and Their Properties in the Fe20Ni20Cr20Co20Cu20 High-Entropy Alloy
    M. A. Kretova
    R. A. Konchakov
    N. P. Kobelev
    V. A. Khonik
    JETP Letters, 2020, 111 : 679 - 684
  • [29] The chromization on hot-rolled Fe40Mn20Cr20Ni20 high-entropy alloys by pack cementation
    Yang, Rui
    Lan, Aidong
    Yang, Huijun
    Jin, Xi
    Qiao, Junwei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 947
  • [30] Recovery stress and strain behavior of Cr20Mn20Fe20Co35Ni5 high entropy alloy deformed via severe plastic deformation
    Park, K. W.
    Kim, W. J.
    MATERIALS CHARACTERIZATION, 2023, 197