Microstructure, mechanical properties and sensitization of ultra-low nickel Cr-Mn austenitic stainless steels

被引:0
|
作者
Ambade, Sachin P. [1 ]
Tembhurkar, Chetan K. [2 ,3 ]
Patil, Awanikumar [4 ]
Tidke, Atul V. [1 ]
Shelare, Sagar D. [2 ,5 ]
Prakash, Chander [3 ]
Djukic, Milos B. [6 ]
Khosravi, Nima [7 ]
Paramasivam, Prabhu [8 ]
机构
[1] Yeshwantrao Chavan Coll Engn, Mech Engn Dept, Nagpur 441110, Maharashtra, India
[2] Priyadarshini Coll Engn, Mech Engn Dept, Nagpur 440019, Maharashtra, India
[3] Chitkara Univ, Ctr Res Impact & Outcome, Rajpura 140401, Punjab, India
[4] VNIT, Met & Mat Engn Dept, Nagpur 440010, Maharashtra, India
[5] Chitkara Univ, Chitkara Ctr Res & Dev, Baddi 174103, Himachal Prades, India
[6] Univ Belgrade, Fac Mech Engn, Kraljice Marije 16, Belgrade 11120, Serbia
[7] R&D Management Persian Gulf Petrochem Ind Co PGP, Dept Elect & Instrumentat Engn, Tehran, Iran
[8] SIMATS, Saveetha Sch Engn, Dept Res & Innovat, Chennai 602105, Tamil Nadu, India
关键词
Ultra -low nickel Cr -Mn ASS; Gas metal arc welding process; Welding speed; Shielded metal arc welding process; CORROSION BEHAVIOR; HIGH-NITROGEN; HEAT;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present study deals with the effect of shielded metal arc welding (SMAW) and gas metal arc welding (GMAW) processes with different welding speeds on microstructural and mechanical properties including intergranular corrosion susceptibility of ultra-low nickel chrome-manganese austenitic stainless steel (ASS). The microstructural analysis was performed by an optical microscope. The Fisher Ferritscope was used for determining ferrite content in the weldment. The microstructural analysis shows that the size of dendrites of delta ferrite and the width of heat affected zone (HAZ) decreases when welding speed increases. It was found more delta-ferrite in SMAW weld compared to GMAW weld. It was also found that when welding speed increases, tensile strength, impact strength and hardness values decrease for both welding processes. From the U-bending test, it was found that the welded joints are strong enough to withstand bend at 1800 without any cracks for both welding processes. It was also found that Cr-Mn ASS weld becomes susceptible to intergranular corrosion on welding. For both welding processes, the degree of sensitization value decreases with an increase in welding speed for both the welding processes as evaluated by the double loop electrochemical potentiodynamic reactivation (DLEPR) test. Also, the weld joint made using the GMAW process is more susceptible to intergranular corrosion than that made using the SMAW process.
引用
收藏
页码:4353 / 4365
页数:13
相关论文
共 50 条
  • [41] Microstructure and mechanical properties of austenitic stainless steels after cold rolling
    Hadji, M
    Badji, R
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2002, 11 (02) : 145 - 151
  • [42] Microstructure and mechanical properties of austenitic stainless steels after cold rolling
    M. Hadji
    R. Badji
    Journal of Materials Engineering and Performance, 2002, 11 : 145 - 151
  • [43] PERMEABILITY, DIFFUSION, AND SOLUBILITY OF HYDROGEN IN CR-NI AND CR-MN AUSTENITIC STEELS
    GROMOV, AI
    KOVNERISTYI, YK
    METAL SCIENCE AND HEAT TREATMENT, 1980, 22 (5-6) : 321 - 324
  • [44] Research Progress on Ultra-Low Temperature Steels: A Review on Their Composition, Microstructure, and Mechanical Properties
    Xiong, Jianchao
    Zhang, Xiaodan
    Wang, Yuhui
    METALS, 2023, 13 (12)
  • [45] Development of high nitrogen, low nickel, 18%Cr austenitic stainless steels
    Di Schino, A
    Kenny, JM
    Mecozzi, MG
    Barteri, M
    JOURNAL OF MATERIALS SCIENCE, 2000, 35 (19) : 4803 - 4808
  • [46] Low Temperature Sensitization of Austenitic Stainless Steels.
    Zucchi, R.
    Zucchini, M.
    Trabanelli, G.
    Rocchini, G.
    Colombo, E.
    Metallurgia Italiana, 1981, 73 (05): : 199 - 206
  • [47] Development of high nitrogen, low nickel, 18%Cr austenitic stainless steels
    A. Di Schino
    J. M. Kenny
    M. G. Mecozzi
    M. Barteri
    Journal of Materials Science, 2000, 35 : 4803 - 4808
  • [48] CONTROLLING THE MARTENSITIC-TRANSFORMATION IN CR-MN AUSTENITIC STEELS UNDER LOAD
    MALINOV, LS
    KONOP, VI
    METAL SCIENCE AND HEAT TREATMENT, 1978, 20 (7-8) : 616 - 621
  • [49] Mechanical and Corrosion Properties of Fe-Cr-Mn-C-N Austenitic Stainless Steels for Drill Collars
    Lee, Eunkyung
    Ryu, Jiseung
    Jeon, Seol
    Mishra, Brajendra
    Palmer, Bruce R.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2016, 47A (06): : 2550 - 2554
  • [50] Mechanical and Corrosion Properties of Fe-Cr-Mn-C-N Austenitic Stainless Steels for Drill Collars
    Eunkyung Lee
    Jiseung Ryu
    Seol Jeon
    Brajendra Mishra
    Bruce R. Palmer
    Metallurgical and Materials Transactions A, 2016, 47 : 2550 - 2554