Corrosion behavior of calcium-magnesium-alumino-silicate on (La,Gd) 2 Zr 2 O 7 / YSZ multilayer for thermal barrier coatings

被引:0
|
作者
Kim, Seung-Hyeon [1 ]
Osada, Toshio [1 ]
Lee, Kee-Sung [2 ]
Oh, Yoon-Suk [3 ]
Nagashima, Nobuo [1 ]
Jang, Byung-Koog [4 ]
机构
[1] Natl Inst Mat Sci, Res Ctr Struct Mat, 1-2-1 Sengen, Tsukuba, Ibaraki 3050047, Japan
[2] Kookmin Univ, Sch Mech Engn, Seoul 02707, South Korea
[3] Korea Inst Ceram Engn & Technol, 3321 Gyeongchung Rd, Icheon 17303, South Korea
[4] Kyushu Univ, Interdisciplinary Grad Sch Engn Sci, 6-1 Kasuga Koen, Kasuga, Fukuoka 8168580, Japan
关键词
Thermal barrier coatings; Corrosion; CMAS; Rare-earth zirconate; YOUNGS MODULUS; RESIDUAL-STRESS; VOLCANIC ASH; INDENTATION; HARDNESS; POROSITY; ALUMINOSILICATE; OPTIMIZATION; DEGRADATION; DESIGN;
D O I
10.2109/jcersj2.23096
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, the high-temperature corrosion behavior was evaluated for (La,Gd) 2 Zr 2 O 7 (LGZ) used as a promising thermal barrier coatings (TBCs) material. (La,Gd) 2 Zr 2 O 7 + YSZ multilayer prepared from atmospheric plasma spray (APS) were exposed to calcium-magnesium-alumino-silicate (CMAS) melt at 1300 degrees C for 2, 12, 48, and 100 h. Molten CMAS and (La,Gd) 2 Zr 2 O 7 reacted to form reaction layer Ca 2 Gd 8 (SiO 4 ) 6 O 2 (apatite) at 1300 degrees C. The thickness of the reaction layer increased with increasing heat-treatment time. A correlation between the hardness and Young ' s modulus relationship for the reaction layer of the coating was observed for the microstructure using nanoindentation. It was con fi rmed that the pores of the coating were reduced through the in fi ltration of molten CMAS in the initial stage of the corrosion reaction, and the hardness and Young ' s modulus were increased due to densi fi cation. Fracture toughness increased with heat treatment time in both directions (in -plane and through-thickness). The fracture toughness in the in -plane direction is 0.19 - 0.23 MPa ../ . On the other hand, the fracture resistance in the thickness direction was 0.87 - 1.26 MPa ffiffiffiffi ffiffiffiffi m ../ , which was m higher than that in the in -plane direction. These results show that the crack propagates in the in -plane direction and causes TBC delamination.
引用
收藏
页码:205 / 213
页数:9
相关论文
共 50 条
  • [31] Oxidation Behavior of Single-Layer Gd2Zr2O7, and Gd2Zr2O7/YbSZ, and Double-Layer YSZ + Gd2Zr2O7/YbSZ Thermal Barrier Coatings
    Mohadese Tabeshfar
    Ghasem Dini
    Mehdi Salehi
    Kjell Wiik
    High Temperature Corrosion of Materials, 2023, 99 : 133 - 149
  • [32] Evaluation of oxidation and thermal cyclic behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 TBCs
    Doleker, Kadir Mert
    Ozgurluk, Yasin
    Ahlatci, Hayrettin
    Karaoglanli, Abdullah Cahit
    SURFACE & COATINGS TECHNOLOGY, 2019, 371 : 262 - 275
  • [33] Comparison of calcium-magnesium-alumina-silicate (CMAS) resistance behavior of produced with electron beam physical vapor deposition (EB-PVD) method YSZ and Gd2Zr2O7/YSZ thermal barrier coatings systems
    Ozgurluk, Yasin
    Karaoglanli, Abdullah Cahit
    Ahlatci, Hayrettin
    VACUUM, 2021, 194
  • [34] Performance of YSZ and Gd2Zr2O7/YSZ double layer thermal barrier coatings in burner rig tests
    Vassen, Robert
    Bakan, Emine
    Mack, Daniel
    Schwartz-Lueckge, Sigrid
    Sebold, Doris
    Sohn, Yoo Jung
    Zhou, Dapeng
    Guillon, Olivier
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (02) : 480 - 490
  • [35] Performance of single YSZ, Gd2Zr2O7 and double-layered YSZ/Gd2Zr2O7 thermal barrier coatings in isothermal oxidation test conditions
    Doleker, Kadir Mert
    Karaoglanli, Abdullah Cahit
    Ozgurluk, Yasin
    Kobayashi, Akira
    VACUUM, 2020, 177
  • [36] Investigation of Isothermal Oxidation Behavior of Thermal Barrier Coatings (TBCs) Consisting of YSZ and Multilayered YSZ/Gd2Zr2O7 Ceramic Layers
    Kadir Mert Doleker
    Hayrettin Ahlatci
    Abdullah Cahit Karaoglanli
    Oxidation of Metals, 2017, 88 : 109 - 119
  • [37] Investigation of Isothermal Oxidation Behavior of Thermal Barrier Coatings (TBCs) Consisting of YSZ and Multilayered YSZ/Gd2Zr2O7 Ceramic Layers
    Doleker, Kadir Mert
    Ahlatci, Hayrettin
    Karaoglanli, Abdullah Cahit
    OXIDATION OF METALS, 2017, 88 (01): : 109 - 119
  • [38] Design, Preparation, and Characterization of Graded YSZ/La2Zr2O7 Thermal Barrier Coatings
    Chen, Hongfei
    Liu, Yun
    Gao, Yanfeng
    Tao, Shunyan
    Luo, Hongjie
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (06) : 1732 - 1740
  • [39] Degradation of La(2)Zr(2)O(7)thermal barrier coatings
    Mikuskiewicz, Marta
    Moskal, Grzegorz
    Jasik, Anna
    OCHRONA PRZED KOROZJA, 2018, 61 (06): : 155 - 158
  • [40] Investigation of Thermal Shock Behavior of Nanostructured (Gd0.9Yb0.1)2Zr2O7/ YSZ Thermal Barrier Coatings
    Fan W.
    Bai Y.
    Wang Y.
    Zhongguo Xitu Xuebao/Journal of the Chinese Rare Earth Society, 2023, 41 (04): : 757 - 764