Effects of Cr and Ni addition on critical crack tip opening displacement (CTOD) and supercritical CO2 corrosion resistance of high-strength low-alloy steel (HSLAs)

被引:0
|
作者
Ma, Qilin [1 ,2 ]
Jia, Shujun [1 ]
Liu, Qingyou [1 ]
Shang, Chengjia [2 ]
机构
[1] Cent Iron & Steel Res Inst Co Ltd, Beijing 100081, Peoples R China
[2] Univ Sci & Technol Beijing, Collaborat Innovat Ctr Steel Commonal, Beijing 100083, Peoples R China
关键词
High-strength low alloy steel (HSLAs); Crack tip opening displacement (CTOD); Supercritical CO 2 corrosion; Cr -Ni composite; CARBON-DIOXIDE; MECHANISM; SCALE;
D O I
10.1016/j.msea.2024.146772
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of Cr and Ni content on the low-temperature toughness and supercritical CO 2 corrosion resistance of high-strength low-alloy steel (HSLAs) were investigated by optical microscopy, scanning electron microscope, electron backscattered diffraction, transmission electron microscope, X-ray Photoelectron Spectroscopy, electron probe X-ray micro-analyzer, critical crack tip opening displacement, and supercritical CO 2 corrosion experiments. In this study, the complex structure of high-strength low-alloy steel is identified and quantified, and related to the critical crack tip opening displacement (CTOD). The further addition of Ni and Cr promotes the formation of granular bainite (GB) and martensite-austenite (MA). The proportion of high-angle grain boundaries in the GB structure is small and does not significantly hinder crack expansion, while MA frequently leads to the initiation and expansion of cracks, deteriorating the low-temperature toughness of the material. Supercritical CO 2 corrosion experiments displayed that further addition of Cr and Ni will improve the density and protection of corrosion products. But high-density dislocations will destroy the integrity of the lattice structure of the material and may serve as diffusion channels to affect the formation of the passivation layer and repair. Moreover, dislocation -dense areas are more likely to capture impurity elements, forming a micro-battery effect and accelerating local corrosion. This reduces the extent to which Cr and Ni alloy elements improve the corrosion resistance of HSLA steel.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Effect of calcium ions on CO2 corrosion of 3Cr low-alloy steel
    Jia, Zhijun
    Du, Cuiwei
    Liu, Zhiyong
    Gao, Jim
    Li, Xiaogang
    [J]. ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2011, 24 (05) : 373 - 380
  • [22] Corrosion Behavior of Low-Alloy Pipeline Steel with 1% Cr Under CO2 Condition
    Zhen-Guang Liu
    Xiu-Hua Gao
    Chi Yu
    Lin-Xiu Du
    Jian-Ping Li
    Ping-Ju Hao
    [J]. Acta Metallurgica Sinica (English Letters), 2015, 28 : 739 - 747
  • [23] Effects of heat input on microstructure evolution and corrosion resistance of underwater laser cladding high-strength low-alloy steel coating
    Cheng, Qi
    Guo, Ning
    Xue, Zhenyu
    Chen, Hao
    Tong, Junhui
    Ding, Yuchao
    Fu, Yunlong
    Zhou, Guanchen
    [J]. Materials Characterization, 2024, 218
  • [24] Investigation of Corrosion Resistance of High-Strength Low-Alloy (HSLA) Steel in Fresh and Salt Water for Pipeline Application
    Qaban, Abdullah
    Naher, Sumsun
    [J]. INTERNATIONAL CONFERENCE ON KEY ENABLING TECHNOLOGIES (KEYTECH 2019), 2019, 2146
  • [25] Hot Deformation Behavior and Dynamic Recrystallization Characteristics in a Low-Alloy High-Strength Ni–Cr–Mo–V Steel
    Chuan Wu
    Shuang Han
    [J]. Acta Metallurgica Sinica (English Letters), 2018, 31 : 963 - 974
  • [26] Hot Deformation Behavior and Dynamic Recrystallization Characteristics in a Low-Alloy High-Strength Ni–Cr–Mo–V Steel
    Chuan Wu
    Shuang Han
    [J]. Acta Metallurgica Sinica(English Letters), 2018, 31 (09) : 963 - 974
  • [27] Effects of Nanosized Nb Carbide Precipitates on the Corrosion Behavior of High-Strength Low-Alloy Steel in Simulated Seawater
    Zhao, Qiyue
    Wang, Zihao
    Fan, Endian
    Wu, Xiaoguang
    Huang, Yunhua
    Li, Xiaogang
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (09): : 7989 - 7996
  • [28] STUDY OF CORROSION FATIGUE CRACK PROPAGATION IN SEA WATER IN 80 kgf/mm2 HIGH-STRENGTH LOW-ALLOY STEEL.
    Okamoto, Tarou
    Takagi, Tomio
    [J]. 1984, (45):
  • [29] Effects of Small Ni Addition on the Microstructure and Toughness of Coarse-Grained Heat-Affected Zone of High-Strength Low-Alloy Steel
    Huang, Gang
    Wan, Xiangliang
    Wu, Kaiming
    Zhao, Huazhong
    Misra, Raja Devesh Kumarmr
    [J]. METALS, 2018, 8 (09):
  • [30] CORRELATION OF MODIFIED CRACK-TIP OPENING DISTANCE WITH HEAT INPUT TO THE HEAT-AFFECTED ZONE OF HIGH-STRENGTH LOW-ALLOY STEELS
    SUAREZ, JC
    MOLLEDA, F
    GONZALES, R
    JIMENEZ, R
    [J]. THEORETICAL AND APPLIED FRACTURE MECHANICS, 1994, 21 (01) : 17 - 22