Experimental Studies on the Phase Separation Behavior of Molten Benzenesulfonate-Modified PET/PA6 Blends

被引:0
|
作者
Ma, Xiao-Jun [1 ,2 ]
Ye, Qi-Yu [1 ,2 ]
Zheng, Shao-Jie [1 ,2 ]
Hu, Ji-Jiang [1 ,2 ]
Yao, Zhen [1 ,2 ]
机构
[1] Zhejiang Univ, State Key Lab Chem Engn, Hangzhou 310027, Peoples R China
[2] Zhejiang Univ, Inst Polymerizat & Polymer Engn, Hangzhou 310027, Peoples R China
来源
MACROMOL | 2023年 / 3卷 / 01期
关键词
CDP; PA6; reactive blends; phase separation; influencing factors; POLY(ETHYLENE-TEREPHTHALATE); COMPATIBILIZATION;
D O I
10.3390/macromol3010005
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this work, nylon 6 (PA6) and cationic dyeable polyester (CDP) modified with benzenesulfonate groups were reactively blended in a twin-screw extruder. The well-mixed CDP/PA6 blends were re-molten and statically kept for various amounts of time. The morphology evolution caused by phase separation was observed by a scanning electron microscope (SEM) and an atomic force microscopy-infrared (AFM-IR) technique. In the absence of shear force, the homogeneously mixed blends were found to separate rapidly into two phases because of the poor miscibility between polyester and polyamide. In the early stage, the dispersed phase was small in size and irregular in shape. With prolongation of the phase separation time, the dispersed phase turned into larger and spherical particles to minimize the interface between phases. The phase separation process typically lasted 2 to 7 min. This means that the effects of phase separation on the morphology of the blends cannot be ignored in injection molding, compression molding, or other processing processes short of shear force. The effects of the ratio between polyester and polyamide, the benzenesulfonate content, and the molecular weight of polymers on phase separation behavior were investigated.
引用
收藏
页码:54 / 64
页数:11
相关论文
共 50 条
  • [41] Double Yielding in PA6/TPV-MAH Blends: Effect of Crosslinking Degree of the Dispersed Phase
    Tang, Xue-Gang
    Yang, Wei
    Shan, Gui-Fang
    Xie, Bang-Hu
    Yang, Ming-Bo
    Hou, Meng
    [J]. JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2009, 47 (09) : 912 - 922
  • [42] Rheology, Phase Morphology and Crystallization Properties of PA6/PP-g-MAH/POE Blends
    Run, Ming-tao
    Han, Qing
    Xing, Bing-tao
    Yao, Meng
    [J]. ADVANCED RESEARCH ON ADVANCED STRUCTURE, MATERIALS AND ENGINEERING, 2012, 382 : 264 - 267
  • [43] Determination of a limiting dispersed phase concentration for coalescence in PA6/HDPE blends under extensional flow
    González-Nuñez, R
    Arellano, M
    Moscoso, FJ
    González-Romero, VM
    Favis, BD
    [J]. POLYMER, 2001, 42 (12) : 5485 - 5489
  • [44] Thermal behavior of PP/PA6 blends under dynamic conditions.: The effect of different interfacial agents based on chemically modified atactic polypropylene
    Collar, EP
    Marco, C
    Areso, S
    García-Martínez, JM
    [J]. JOURNAL OF MACROMOLECULAR SCIENCE-PHYSICS, 2001, B40 (3-4): : 369 - 385
  • [45] Effect of selective localization of carbon nanotubes in PA6 dispersed phase of PP/PA6 blends on the morphology evolution with time, part 1: Droplet deformation under simple shear flows
    Gooneie, A.
    Nazockdast, H.
    Shahsavan, F.
    [J]. POLYMER ENGINEERING AND SCIENCE, 2015, 55 (07): : 1504 - 1519
  • [46] Creating super-tough and strong PA6/ABS blends using multi-phase compatibilizers
    Sui, Xianwei
    Xie, Xu-Ming
    [J]. CHINESE CHEMICAL LETTERS, 2019, 30 (01) : 149 - 152
  • [47] Super Tough PA6/PP/ABS/SEBS Blends Compatibilized by a Combination of Multi-Phase Compatibilizers
    Yan, Jianhui
    Wang, Cuifang
    Zhang, Tongyu
    Xiao, Zijian
    Xie, Xuming
    [J]. Materials, 2024, 17 (21)
  • [49] Encapsulated Phase Structure and Morphology Evolution During Quiescent Annealing in Ternary Polymer Blends with PA6 as Matrix
    Dou, Rui
    Wang, Wei
    Zhou, Yan
    Gong, Lei
    Yin, Bo
    Yang, Ming-bo
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2014, 131 (04)
  • [50] Creating super-tough and strong PA6/ABS blends using multi-phase compatibilizers
    Xianwei Sui
    Xu-Ming Xie
    [J]. Chinese Chemical Letters, 2019, 30 (01) : 149 - 152