Activity of Iron Oxide in Slag with Nepheline Syenite Added as a Flux

被引:0
|
作者
Sakamoto, Yusaku [1 ,2 ]
Saito, Keijiro [3 ]
Hasegawa, Masakatsu [3 ]
机构
[1] Kyoto Univ, Kyoto, Japan
[2] TAKADA TAKAHASHI & PARTNERS, 12-22,Tsukiji 1 Chome,Chuo Ku, Tokyo 1040045, Japan
[3] Kyoto Univ, Dept Energy Sci & Technol, Yoshida Hon Machi,Sakyo Ku, Kyoto 6068501, Japan
关键词
nepheline syenite; phase diagram; FeO activity; reduction-oxidation reaction; CHEMICAL-POTENTIALS; SYSTEM; FEXO; FEO;
D O I
10.2355/isijinternational.ISIJINT-2023-452
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Although fluorspar has been widely used as a flux for steelmaking slag, there is a strong incentive to explore alternatives. As one of the candidates for such substances, "nepheline syenite" has been investigated in terms of slag fluidity and lime dissolution rate. The present study aimed at clarifying the homogeneous liquid region and FexO activities in the CaO-FexO slags with nepheline syenite added at 1 673 K. When the molar ratio of nepheline syenite/CaO was below 0.658, the substitution of CaO with nepheline syenite raised the FexO activity as well as CaF2. The effect of the nepheline syenite addition on slag basicity was discussed by means of the reduction-oxidation reaction of Fe3+/Fe2+.
引用
收藏
页码:901 / 908
页数:8
相关论文
共 50 条
  • [21] ELECTROCHEMICAL MEASUREMENT OF THE ACTIVITY OF IRON OXIDE IN FeO-SiO2 LIQUID SLAG.
    Wanibe, Yoshimoto
    Yamauchi, Yutaka
    Kawai, Kenji
    Sakao, Hiroshi
    1600, (12):
  • [22] A Thermodynamic Model for Prediction of Iron Oxide Activity in Some FeO-Containing Slag Systems
    Yang, Xue-min
    Shi, Cheng-bin
    Zhang, Meng
    Zhang, Jian
    STEEL RESEARCH INTERNATIONAL, 2012, 83 (03) : 244 - 258
  • [23] Iron losses during desulphurisation of hot metal utilising co-injection of Mg and CaC2 combined with nepheline syenite
    Magnelov, M.
    Carlsson-Dahlberg, A.
    Gustavsson, L.
    Bjorkvall, J.
    Bjorkman, B.
    IRONMAKING & STEELMAKING, 2015, 42 (07) : 525 - 532
  • [24] Iron oxide slag nanocomposites in removal of hexavalent chromium
    Baalamurugan, J.
    Kumar, V. Ganesh
    Senthilkumar, P.
    Govindaraju, K.
    Dhas, T. Stalin
    INTERNATIONAL JOURNAL OF NANOTECHNOLOGY, 2021, 18 (5-8) : 436 - 448
  • [25] Foaming during reduction of iron oxide in molten slag
    Jouhari, AK
    Galgali, RK
    Datta, P
    Bhattacharjee, S
    Gupta, RC
    Ray, HS
    IRONMAKING & STEELMAKING, 2000, 27 (01) : 27 - 31
  • [26] Reduction of iron oxide in sulfur bearing slag by graphite
    Hong, L
    Hirasawa, M
    Yamada, S
    Sano, M
    ISIJ INTERNATIONAL, 1996, 36 (10) : 1237 - 1244
  • [27] Reduction of iron oxide in liquid slag by solute carbon
    Regional Research Laboratory, Bhubaneswar 761 013, India
    不详
    J Inst Eng India Part MM, 2006, OCT. (7-12):
  • [28] RATE OF REDUCTION OF IRON-OXIDE IN MOLTEN SLAG
    SHINOTAKE, A
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (04): : S121 - S121
  • [29] Dielectrical and structural characterization of iron oxide added to hydroxyapatite
    C. C. Silva
    F. P. Filho
    M. F. P. Graça
    M. A. Valente
    A. S. B. Sombra
    Bulletin of Materials Science, 2008, 31 : 635 - 638
  • [30] Dielectrical and structural characterization of iron oxide added to hydroxyapatite
    Silva, C. C.
    Filho, F. P.
    Graca, M. F. P.
    Valente, M. A.
    Sombra, A. S. B.
    BULLETIN OF MATERIALS SCIENCE, 2008, 31 (04) : 635 - 638