Activity of Iron Oxide in Slag with Nepheline Syenite Added as a Flux

被引:0
|
作者
Sakamoto, Yusaku [1 ,2 ]
Saito, Keijiro [3 ]
Hasegawa, Masakatsu [3 ]
机构
[1] Kyoto Univ, Kyoto, Japan
[2] TAKADA TAKAHASHI & PARTNERS, 12-22,Tsukiji 1 Chome,Chuo Ku, Tokyo 1040045, Japan
[3] Kyoto Univ, Dept Energy Sci & Technol, Yoshida Hon Machi,Sakyo Ku, Kyoto 6068501, Japan
关键词
nepheline syenite; phase diagram; FeO activity; reduction-oxidation reaction; CHEMICAL-POTENTIALS; SYSTEM; FEXO; FEO;
D O I
10.2355/isijinternational.ISIJINT-2023-452
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Although fluorspar has been widely used as a flux for steelmaking slag, there is a strong incentive to explore alternatives. As one of the candidates for such substances, "nepheline syenite" has been investigated in terms of slag fluidity and lime dissolution rate. The present study aimed at clarifying the homogeneous liquid region and FexO activities in the CaO-FexO slags with nepheline syenite added at 1 673 K. When the molar ratio of nepheline syenite/CaO was below 0.658, the substitution of CaO with nepheline syenite raised the FexO activity as well as CaF2. The effect of the nepheline syenite addition on slag basicity was discussed by means of the reduction-oxidation reaction of Fe3+/Fe2+.
引用
收藏
页码:901 / 908
页数:8
相关论文
共 50 条
  • [2] NEPHELINE SYENITE AS A SYNTHETIC SLAG ADDITION IN SECONDARY STEELMAKING
    KINGSTON, PW
    CALEY, WF
    MINERALS ENGINEERING, 1989, 2 (02) : 207 - 215
  • [3] Activity of Iron Oxide in Steelmaking Slag
    Somnath Basu
    Ashok Kumar Lahiri
    Seshadri Seetharaman
    Metallurgical and Materials Transactions B, 2008, 39 : 447 - 456
  • [4] Activity of iron oxide in steelmaking slag
    Basu, Somnath
    Lahiri, Ashok Kumar
    Seetharaman, Seshadri
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2008, 39 (03): : 447 - 456
  • [5] NEPHELINE SYENITE TALC MIXTURES AS A FLUX IN LOW-TEMPERATURE VITRIFIED BODIES
    LYNCH, ED
    ALLEN, AW
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1950, 33 (04) : 117 - 120
  • [6] Investigation of iron losses during desulphurisation of hot metal utilising nepheline syenite
    Magnelov, M.
    Eriksson, J.
    Drugge, J.
    Bjorkvall, J.
    Bjorkman, B.
    IRONMAKING & STEELMAKING, 2013, 40 (06) : 436 - 442
  • [7] Effect of Nepheline Syenite on Iron Losses in Slags during Desulphurization of Hot Metal
    Yang, Annika Fang
    Karasev, Andrey
    Jonsson, Par Goran
    STEEL RESEARCH INTERNATIONAL, 2016, 87 (05) : 599 - 607
  • [8] Effect of Temperature on Activity of Water Quenched Slag Prepared by Reducing Iron Oxide of Steel Slag with Coal Gangue
    Song Q.
    Nie J.
    Song T.
    Hu Y.
    Deng Y.
    Chen Y.
    Cheng F.
    Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2024, 52 (02): : 522 - 532
  • [9] ELECTROCHEMICAL MEASUREMENT OF ACTIVITY OF IRON OXIDE IN FEO-SIO2 LIQUID SLAG
    WANIBE, Y
    YAMAUCHI, Y
    KAWAI, K
    SAKAO, H
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1972, 12 (06) : 472 - 476
  • [10] OXIDATION RATE OF CARBON IN IRON BY IRON-OXIDE IN SLAG
    WEI, P
    SANO, M
    HIRASAWA, M
    MORI, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1990, 76 (04): : 552 - 559