Comparative analysis of flexural strength of 3D printed and milled 4Y-TZP and 3Y-TZP zirconia

被引:2
|
作者
Kyung, Kyu-Young [1 ]
Park, Ji-Man [1 ]
Heo, Seong-Joo [1 ]
Koak, Jai-Young [1 ]
Kim, Seong-Kyun [1 ]
Ahn, Jin-Soo [2 ]
Yi, Yuseung [1 ]
机构
[1] Seoul Natl Univ, Dent Res Inst, Dept Prosthodont, Sch Dent, Seoul, South Korea
[2] Seoul Natl Univ, Dept Dent Biomat Sci, Dent Res Inst, Sch Dent, Seoul, South Korea
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2024年 / 131卷 / 03期
关键词
TRANSLUCENT ZIRCONIA; TOUGHNESS; CERAMICS;
D O I
10.1016/j.prosdent.2023.12.020
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. The mechanical properties of 3 dimensionally (3D) printed zirconia have been reported to be comparable with those of milled zirconia, except for the flexural strength. However, most previous studies tested 3 mol% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP), making it necessary to study 3D printed zirconia with 4 mol% yttria content (4Y-TZP). Purpose. The purpose of this in vitro study was to compare the flexural strength of 3D printed 4Y-TZP with 3Y-TZP materials and milled 4Y-TZP. Material and methods. A total of 80 disk specimens (& Oslash;15x1.5 mm) were fabricated and divided into 4 groups (n=20) using the fabrication method and yttria content: milled 3Y-TZP (Katana HT; Kuraray Noritake), 3D printed 3Y-TZP (TZ-3Y-E; Tosoh), milled 4Y-TZP (Katana STML; Kuraray Noritake), and 3D printed 4Y-TZP (3DMAT; Genoss). The biaxial flexural strength was determined with a piston-on-3-ball test (n=15). The flexural strength of each specimen was measured, and the Weibull modulus (m) and characteristic strength (sigma(0)) were estimated from the fracture load distribution. Two intact and fractured specimens were examined with scanning electron microscopy (SEM). The crystalline phase of the specimens in each group was identified through X-ray diffraction (XRD) analysis (n=5). A 1-way ANOVA was used to compare the flexural strength among different groups. Subsequently, pairwise comparisons were conducted with the Tukey post hoc method (alpha=.05). Results. The flexural strength of 3D printed 4Y-TZP was significantly higher than that of milled 4Y-TZP (P<.001). In contrast, the flexural strength of 3D printed 3Y-TZP was significantly lower than that of milled 3Y-TZP (P<.001). X-ray diffraction (XRD) analysis revealed that the tetragonal phase was the dominant phase in all groups, with the identification of some cubic phase peaks. Conclusions. Three dimensionally printed 4Y-TZP showed significantly higher flexural strength than milled 4Y-TZP and exhibited a clinically acceptable flexural strength exceeding 800 MPa.
引用
收藏
页码:529.e1 / 529.e9
页数:9
相关论文
共 50 条
  • [31] Fused filament fabrication of partially stabilized zirconia (3Y-TZP) parts
    Camargo, Italo Leite de
    Verza, Jhonata R.
    Garcia, Joaquin
    Di Federico, Denise
    Fortulan, Carlos A.
    Luz, Ana Paula da
    Materials Letters, 2024, 355
  • [32] Effect of firing temperature on the interface between 3Y-TZP zirconia and porcelain
    Seto, Munetsugu
    Ueda, Kazuhiko
    Katsuta, Yasuhiro
    Suzuki, Shohei
    Ozawa, Makoto
    Outaki, Rina
    Hiroyasu, Kazuhiko
    Watanabe, Fumihiko
    JOURNAL OF ORAL SCIENCE, 2022, 64 (02) : 135 - 138
  • [33] Impact of High-Speed Sintering of Three-Unit 3Y-TZP and 4Y-TZP Fixed Dental Prostheses on Fracture Load With and Without Artificial Aging
    Mayinger, Felicitas
    Pfefferle, Regina
    Reichert, Axel
    Stawarczyk, Bogna
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2021, 34 (01) : 47 - 53
  • [34] Effect of milled and lithography-based additively manufactured zirconia (3Y-TZP) on the biological properties of human osteoblasts
    Rodriguez-Lozano, Francisco Javier
    Lopez-Garcia, Sergio
    Sanchez-Bautista, Sonia
    Perez-Lopez, Javier
    Raigrodski, Ariel J.
    Revilla-Leon, Marta
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (06): : 889 - 896
  • [35] Sinterability of alumina-dispersed 3Y-TZP
    Cho, Bum-Rae
    Yeoum, Dong-Guk
    SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 37 - 40
  • [36] Contact damage in artificially aged 3Y-TZP
    de Armas Sancho, Z.
    Jimenez-Pique, E.
    Mestra, A.
    Anglada, M.
    5TH INTERNATIONAL EEIGM/AMASE/FORGEMAT CONFERENCE ON ADVANCED MATERIALS RESEARCH, 2009, 5
  • [37] Comparison of Testing Designs for Flexural Strength of 3Y-TZP and 5Y-PSZ Considering Different Surface Treatment
    Hergeroder, Carsten
    Wille, Sebastian
    Kern, Matthias
    MATERIALS, 2022, 15 (11)
  • [38] Preparation and properties of 3Y-TZP/CMS material
    Wang Yinling
    Chen SenFeng
    Lu Difen
    Zhang Liwei
    Chen Wenwei
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 : 348 - 350
  • [39] Glycothermal Synthesis and Characterization of 3Y-TZP Nanoparticles
    Song, Jeong-Hwan
    Lee, Ju-Hee
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2009, 19 (08): : 412 - 416
  • [40] ON THE ISOTHERMAL MARTENSITIC-TRANSFORMATION IN 3Y-TZP
    BEHRENS, G
    DRANSMANN, GW
    HEUER, AH
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (04) : 1025 - 1030