Room temperature tensile creep behavior of Mg-6Zn-0.4Mn-0.3Al-0.2Ca (wt%) alloy containing icosahedral quasicrystals

被引:1
|
作者
Ying, Yu-Lei [1 ,2 ]
Guan, Zhi-Ping [1 ,2 ]
Wang, Xuan [1 ,2 ]
Wang, Gang [3 ]
Yan, Wei [4 ]
机构
[1] Jilin Univ, Key Lab Automobile Mat, Minist Educ, Nanling Campus,5988 Renmin St, Changchun 130025, Peoples R China
[2] Jilin Univ, Sch Mat Sci & Engn, Nanling Campus,5988 Renmin St, Changchun 130025, Peoples R China
[3] FAW Tooling Die Mfg Co Ltd, Res & Dev Dept, Changchun 130000, Jilin, Peoples R China
[4] FAW Tooling Die Mfg Co Ltd, Prod Dev Dept, Changchun 130000, Jilin, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Magnesium alloy; Creep mechanism; Dislocation; Quasicrystal; Room temperature; ZN-Y ALLOYS; DEFORMATION-BEHAVIOR; THRESHOLD STRESSES; NONBASAL SLIP; IN-SITU; MAGNESIUM; CA; TEXTURE; MICROSTRUCTURE; PRECIPITATION;
D O I
10.1016/j.mtcomm.2024.108602
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The poor creep resistance at room temperature is the critical issue limiting magnesium (Mg) alloys to be structural components in engineering fields. In this study, we designed a novel Mg-6Zn-0.4Mn-0.3Al-0.2Ca (ZMAX6000) alloy, which had superior creep properties at room temperature, and the steady creep rate of ZMAX6000 (2.52x10(-9) s(-1)) alloy was one order of magnitude lower than that of pure Mg (5.0x10(-8) s(-1)) and AZ31 alloy (1.5x10(-8) s(-1)), when the creep stress is equivalent to the 0.8 yield stress (YS). The ZMAX6000 alloy featured icosahedral quasicrystal phases (I-phases) distributed at almost all triangular grain boundaries. The room temperature creep threshold stress (sigma(0)) and stress exponent (n) for the I-phase enhanced ZMAX6000 alloy were sigma(0) = 209 MPa and n = 4.9, respectively. I-phases can act as barriers to grain boundary sliding, and the high-density nanoscale second phases inside the grains can impede the dislocation slip. Consequently, the ZMAX6000 alloy exhibits excellent creep properties at room temperature. The cross-slip consisting of basal < a > dislocation and prismatic < a > dislocation, as well as the pyramidal <c + a> slip are the main creep mechanisms of the ZMAX6000 alloy at room temperature.
引用
收藏
页数:8
相关论文
共 50 条
  • [31] Development of extruded Mg-6Er-3Y-1.5Zn-0.4Mn(wt.%) alloy with high strength at elevated temperature
    Mingquan Zhang
    Yan Feng
    Jinghuai Zhang
    Shujuan Liu
    Qiang Yang
    Zhuang Liu
    Rongguang Li
    Jian Meng
    Ruizhi Wu
    Journal of Materials Science & Technology, 2019, 35 (10) : 2365 - 2374
  • [32] Microstructural refinement and mechanical properties improvement of Mg-Al-Mn-Zn-Ca alloy processed by rotary swaging at room temperature
    Wang, Yongxin
    Yang, Yanmei
    Lin, Yini
    Chen, Hao
    Li, Guo
    Huang, Yuanding
    Xie, Weidong
    Wei, Guobing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 913
  • [33] The hot deformation behavior and microstructural evolution of as-cast Mg-2Zn-0.5Mn-0.2Ca-0.3Nd-0.7La alloy
    Mi, Jie
    Ma, Deqing
    Luan, Shiyu
    Jin, Peipeng
    Chen, Lijia
    Che, Xin
    Li, Xiaoqiang
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 : 1533 - 1545
  • [34] Microstructure and mechanical properties of non-flammable Mg-8Al-0.3Zn-0.1Mn-0.3Ca-0.2Y alloy subjected to low-temperature, low-speed extrusion
    Go, Yohan
    Jo, Su Mi
    Park, Sung Hyuk
    Kim, Ha Sik
    You, Bong Sun
    Kim, Young Min
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 739 : 69 - 76
  • [35] Microstructure, tensile properties and creep behavior of Mg-4Al-2Sn containing Ca alloy produced by different casting technologies
    Kim, Byeong Ho
    Jo, Su Mi
    Lee, Young Chul
    Park, Yong Ho
    Park, Ik Min
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 535 : 40 - 47
  • [36] Role of extrusion rate on the microstructure and tensile properties evolution of ultrahigh-strength low-alloy Mg-1.0Al-1.0Ca-0.4Mn (wt.%) alloy
    Liu, X. Q.
    Qiao, X. G.
    Pei, R. S.
    Chi, Y. Q.
    Yuan, L.
    Zheng, M. Y.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2023, 11 (02) : 553 - 561
  • [37] Role of extrusion rate on the microstructure and tensile properties evolution of ultrahigh-strength low-alloy Mg-1.0Al-1.0Ca-0.4Mn(wt.%)alloy
    XQLiu
    XGQiao
    RSPei
    YQChi
    LYuan
    MYZheng
    Journal of Magnesium and Alloys, 2023, 11 (02) : 553 - 561
  • [38] Role of extrusion rate on the microstructure and tensile properties evolution of ultrahigh-strength low-alloy Mg-1.0Al-1.0Ca-0.4Mn(wt.%)alloy
    X.Q.Liu
    X.G.Qiao
    R.S.Pei
    Y.Q.Chi
    L.Yuan
    M.Y.Zheng
    Journal of Magnesium and Alloys, 2023, (02) : 553 - 561
  • [39] Room-temperature stretch formability, tensile properties, and microstructures of precipitation hardenable Mg-6Zn-0.2Ca (mass%) alloy sheets micro-alloyed with Ce or Y
    Nakata, T.
    Li, Z. H.
    Sasaki, T. T.
    Hono, K.
    Kamado, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 804
  • [40] Effect of minor Sc addition on high temperature tensile behavior of Al-7Zn-2Mg-2Cu-0.2Zr alloy
    Lang, Mo
    Zhao, Ning
    Wang, Yingcai
    He, Min
    Zhu, Jing
    Qiao, Jun
    MATERIALS CHEMISTRY AND PHYSICS, 2022, 288