Microstructural and compositional design of Cr2AlC MAX phases and their impact on oxidation resistance

被引:7
|
作者
Azina, Clio [1 ]
Poll, Melina [2 ]
Holzapfel, Damian M. [1 ]
Tailleur, Elodie [3 ]
Zuber, Axel [4 ]
Dubois, Sylvain [4 ]
Eklund, Per [5 ]
Gonzalez-Julian, Jesus [2 ,6 ]
机构
[1] Rhein Westfal TH Aachen, Mat Chem, Kopernikusstr 10, D-52074 Aachen, Germany
[2] Forschungszentrum Julich GmbH, Inst Energy & Climate Res Mat Synth & Proc IEK 1, D-52425 Julich, Germany
[3] Univ Lorraine, CRM2, Vandoeuvre Les Nancy, France
[4] Univ Poitiers, Inst PPRIME, CNRS, ENSMA,UPR 3346,TSA 41126, F-86073 Poitiers 9, France
[5] Linkoping Univ, Thin Film Phys Div, Dept Phys Chem & Biol IFM, SE-58183 Linkoping, Sweden
[6] Rhein Westfal TH Aachen, Inst Mineral Engn GHI, Chair Ceram, Forckenbeckstr 33, D-52074 Aachen, Germany
关键词
MAX phases; Reactive sintering; Microstructural design; Oxidation; HIGH-TEMPERATURE OXIDATION; COATINGS; BEHAVIOR; POWDER;
D O I
10.1016/j.jeurceramsoc.2024.02.037
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The oxidation of MAX phases has largely been investigated, but the effect of secondary phases and microstructure is still unclear. We report on the effect of reactive and non-reactive sintering, and starting powders, on the microstructure, phase formation, and chemical composition of Cr2AlC MAX phases. The grain sizes are shown to be sensitive to both the processing method and the starting powders. Secondary phases were observed mostly in reactively sintered samples as Cr7C3 and AlCr2 were identified, and Al contents varied between 24.4 and 28.0 at %. Finally, the oxidation behavior of the produced MAX phases was evaluated after 60 and 120 min at 1100 degrees C. The Al content, the average grain size of the as-sintered samples, and the presence of secondary phases affected the decomposition of the MAX phase into Cr-carbides in the vicinity of the oxide scale and the composition of the oxide scale, respectively.
引用
收藏
页码:4895 / 4904
页数:10
相关论文
共 50 条
  • [41] Sintering behavior of Cr2AlC MAX phase synthesized by Spark plasma sintering
    Zakeri-Shahroudi, Fatemeh
    Ghasemi, Behrooz
    Abdolahpour, Hassan
    Razavi, Mansour
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2022, 19 (03) : 1309 - 1318
  • [42] Manufacturing of High Purity Cr2AlC MAX Phase Material and Its Characterization
    Desai, Vyom
    Shrivastava, Aroh
    Zala, Arunsinh B.
    Parekh, Tejas
    Gupta, Surojit
    Jamnapara, N. I.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (18) : 9841 - 9849
  • [43] Effect of sintering method on the microstructure of pure Cr2AlC MAX phase ceramics
    Gonzalez-Julian, Jesus
    Onrubia, Sara
    Bram, Martin
    Guillon, Olivier
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2016, 124 (04) : 415 - 420
  • [44] Corrosion performance of Ti3SiC2, Ti3AlC2, Ti2AlC and Cr2AlC MAX phases in simulated primary water conditions
    Ward, Joseph
    Bowden, David
    Prestat, Eric
    Holdsworth, Sam
    Stewart, David
    Barsoum, Michel W.
    Preuss, Michael
    Frankel, Philipp
    CORROSION SCIENCE, 2018, 139 : 444 - 453
  • [45] Yttrium incorporation in Cr2AlC: On the metastable phase formation and decomposition of (Cr,Y)2AlC MAX phase thin films
    Azina, Clio
    Bartsch, Tim
    Holzapfel, Damian M.
    Dahlqvist, Martin
    Rosen, Johanna
    Lofler, Lukas
    Mendez, Alba San Jose
    Hans, Marcus
    Primetzhofer, Daniel
    Schneider, Jochen M.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2023, 106 (04) : 2652 - 2665
  • [46] Cyclic oxidation of Cr2AlC between 1000 and 1300 °C in air
    Lee, D. B.
    Nguyen, Thuan Dinh
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 464 (1-2) : 434 - 439
  • [47] Oxidation of Cr2AlC coatings in the temperature range of 1230 to 1410 °C
    Hajas, D. E.
    Baben, M. To
    Hallstedt, B.
    Iskandar, R.
    Mayer, J.
    Schneider, J. M.
    SURFACE & COATINGS TECHNOLOGY, 2011, 206 (04): : 591 - 598
  • [48] Oxidation and cracking behaviors of triple-layered Cr2AlC coating
    Li, Jingjing
    Xiang, Huimin
    Xu, Jingjun
    Zheng, Lili
    Qian, Yuhai
    SURFACE & COATINGS TECHNOLOGY, 2021, 422
  • [49] Bonding and oxidation protection of Ti2AlC and Cr2AlC for a Ni-based superalloy
    Sokol, Maxim
    Yang, Jian
    Keshavan, Hrishikesh
    Barsoum, Michel W.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (04) : 878 - 882
  • [50] Oxidation of Cr2AlC (0001): Insights from Ab Initio Calculations
    Neng Li
    Ridwan Sakidja
    Wai-Yim Ching
    JOM, 2013, 65 : 1487 - 1491