The solidification characteristics of highly undercooled Cu-7.77% Co peritectic alloy has been examined by glass fluxing technique. The obtained undercoolings vary from 93 to 203 K(0.14 T). It is found that the a(Co) phase always nucleates and grows preferentially, which is followed by peritectic transformation. This means that the peritectic phase cannot form directly, even though the alloy melt is undercooled to a temperature far below its peritectic point. The maximum recalescence temperature measured experimentally decreases as undercooling increases, which is lower than the thermodynamic calculation result owing to the actual non-adiabatic nature of recalescence process. The dendritic fragmentation of primary α(Co) phase induced by high undercooling is found to enhance the completion of peritectic transformation. In addition, the LKT/BCT dendrite growth model is modified in order to make it applicable to those binary alloy systems with seriously curved liquidus and solidus lines. The dendrite gr
引用
收藏
页码:1338 / 1343
页数:6
相关论文
共 50 条
  • [21] Eutectic and peritectic solidification patterns
    Akamatsu, Silvere
    Plapp, Mathis
    CURRENT OPINION IN SOLID STATE & MATERIALS SCIENCE, 2016, 20 (01): : 46 - 54
  • [22] Peritectic solidification of superconducting oxides
    Shiohara, Y
    Kambara, M
    Izumi, T
    Nakamura, Y
    SOLIDIFICATION AND CASTING, 2003, : 402 - 413
  • [23] Isothermal solidification in peritectic systems
    Boussinot, G.
    Hueter, C.
    Spatschek, R.
    Brener, E. A.
    ACTA MATERIALIA, 2014, 75 : 212 - 218
  • [24] CONTROLLED SOLIDIFICATION OF PERITECTIC ALLOYS
    DAVID, SA
    BRODY, HD
    JOM-JOURNAL OF METALS, 1975, 27 (12): : A43 - A43
  • [25] Rapid growth of FeAl inter-metallic compound under high undercooling conditions
    L?Yongjun & WEI Bingbo Department of Applied Physics
    Chinese Science Bulletin, 2004, (06) : 547 - 551
  • [26] Rapid solidification of Cu-Pb hypomonotectic alloy at high undercooling
    Department of Mechanical Engineering, Branch of North University of China, Taiyuan 030008, China
    不详
    不详
    Zhuzao, 2006, 5 (444-447):
  • [27] Cell tip undercooling in directional solidification
    Pocheau, A
    Georgelin, M
    JOURNAL OF CRYSTAL GROWTH, 1999, 206 (03) : 215 - 229
  • [28] CONTAINERLESS UNDERCOOLING AND SOLIDIFICATION IN DROP TUBES
    LACY, LL
    ROBINSON, MB
    RATHZ, TJ
    JOURNAL OF CRYSTAL GROWTH, 1981, 51 (01) : 47 - 60
  • [29] The Effect of Undercooling on Solidification of YSZ Splats
    Haibo Liu
    Markus Bussmann
    Javad Mostaghimi
    Journal of Thermal Spray Technology, 2008, 17 : 646 - 654
  • [30] RAPID SOLIDIFICATION, UNDERCOOLING AND METASTABLE EQUILIBRIUM
    SHINGU, PH
    ISHIHARA, KN
    NISHITANI, SR
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 26 (06) : B183 - B184