PHASE-TRANSFORMATIONS DURING THE DISPROPORTIONATION STAGE IN THE SOLID HDDR PROCESS IN A ND16FE76B8 ALLOY

被引:46
|
作者
GUTFLEISCH, O
MARTINEZ, N
VERDIER, M
HARRIS, IR
机构
[1] School of Metallurgy and Materials Science, University of Birmingham, Birmingham
关键词
D O I
10.1016/0925-8388(94)90845-1
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The phase transformations and the development of the microstructure of a Nd16Fe76B8 alloy during the disproportionation stage of the solid hydrogenation-disproportionation-desorption-recombination (S-HDDR) process have been studied in detail by means of conventional scanning electron microscopy (SEM) and high resolution SEM. In situ electrical resistivity measurements have been used as a means of monitoring and controlling the progress of the S-HDDR reaction. The non-decrepitated samples were quenched under vacuum from various stages (10, 20, 120 min and 20 h) of the disproportionation process at T=800 degrees C and p(H-2)=0.7 bar. Backscattered electron images reveal that the Nd2Fe14B matrix phase disproportionates from the Nd-rich grain boundary phase inwards, resulting in the development of a cellular, lamellar-type substructure. Spherical Nd-rich regions trapped along cracks during solidification also act as a starting point for the disproportionation reaction. The eutectoid-type transformation, initiated by the absorption of hydrogen, produces colonies of what appear to be alternating lamellae of Fe-rich and Nd-rich phases with an estimated width of 20 nm. Extended exposure to hydrogen results in the decomposition of the NdFe4B4 phase by reaction with the disproportionated matrix.
引用
收藏
页码:227 / 233
页数:7
相关论文
共 50 条
  • [31] The effects of long term annealing at 1000°C for 24 h on the microstructure and magnetic properties of Pr-Fe-B/Nd-Fe-B magnets based on Nd16Fe76B8 and Pr16Fe76B8
    Corfield, MR
    Williams, AJ
    Harris, IR
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 296 (1-2) : 138 - 147
  • [32] The production of a Nd16Fe76B8 sintered magnet by the hydrogen decrepitation/hydrogen vibration milling route
    Kianvash, A
    Harris, IR
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 282 (1-2) : 213 - 219
  • [33] The effects of blending additions of copper and cobalt to Nd16Fe76B8 milled powder to produce sintered magnets
    Mottram, RS
    Williams, AJ
    Harris, IR
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2001, 234 (01) : 80 - 89
  • [34] 机械力驱动下Nd16Fe76B8合金氢化-歧化反应机理研究
    李玉平
    胡连喜
    刘晓亚
    [J]. 稀有金属材料与工程, 2011, 40 (10) : 1762 - 1766
  • [35] HDDR processes in Nd16Fe76-xZrxB8 alloys and the production of anisotropic magnets
    Short, CL
    Guegan, P
    Gutfleisch, O
    Ragg, OM
    Harris, IR
    [J]. IEEE TRANSACTIONS ON MAGNETICS, 1996, 32 (05) : 4368 - 4370
  • [36] PHASE-TRANSFORMATIONS IN TITANIUM BT16 ALLOY DURING DEFORMATION
    MALTSEV, MV
    [J]. FIZIKA METALLOV I METALLOVEDENIE, 1990, (12): : 97 - 103
  • [37] Kinetics and thermodynamics of the solid-HDDR process in the Nd13Fe80.5B6.5 alloy
    Torres, CER
    Sánchez, FH
    van Raap, MBF
    Zélis, LM
    Actis, F
    Nagel, H
    [J]. MAGNETISM, MAGNETIC MATERIALS AND THEIR APPLICATIONS, 1999, 302-3 : 314 - 318
  • [38] Effect of the disproportionation and recombination stages of the HDDR process on the inducement of anisotropy in Nd-Fe-B magnets
    Sugimoto, S
    Nakamura, H
    Kato, K
    Book, D
    Kagotani, T
    Okada, M
    Homma, M
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 293 : 862 - 867
  • [39] TMA Study on Phase Evolution During Hydrogen-assisted Disproportionation of Nd-Fe-B Alloy
    Kwon, H. W.
    Yu, J. H.
    [J]. JOURNAL OF MAGNETICS, 2011, 16 (03) : 229 - 233
  • [40] EVOLUTION OF RECOMBINATION IN A SOLID HDDR PROCESSED ND14FE79B7 ALLOY
    MARTINEZ, N
    JONES, DGR
    GUTFLEISCH, O
    LAVIELLE, D
    PERE, D
    HARRIS, IR
    [J]. JOURNAL OF APPLIED PHYSICS, 1994, 76 (10) : 6825 - 6827