Load-controlled isothermal and non-isothermal fatigue lives of a [0-degrees]8 SiC/Ti-15-3 were evaluated at temperatures between 150 and 550-degrees-C and a target strain range of about 0.45%. In non-isothermal fatigue tests, load was first cycled at minimum temperature and then temperature was cycled at zero load. For fatigue tests with peak temperatures at or above 300-degrees-C, fatigue life was dramatically reduced compared to that at 150-degrees-C. The shortest life was produced by the non-isothermal test with the greatest temperature range (DELTAT = 400-degrees-C) and highest peak temperature (T(max) = 550-degrees-C). Vacuum testing showed that much of the life reduction under isothermal and non-isothermal conditions was related to environmental effects, although the nature of the fatigue-environment interaction was decidedly different for the isothermal and non-isothermal test cycles which were studied.
引用
收藏
页码:41 / 45
页数:5
相关论文
共 50 条
  • [41] Ti-15-3/SiC复合材料基体的显微组织特性
    刘晋伟
    稀有金属快报, 1999, (07) : 20 - 21
  • [42] The effect of heat treatment on Young's modulus, damping, and microhardness of SiC/Ti-15-3
    Wolfenden, A
    Hall, KD
    Lerch, BA
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (06) : 1489 - 1493
  • [43] Study on the superplastic behavior of Ti-15-3 alloy
    Faculty of Materials and Meiallurgic Engineering, Kunming University of Science and Technology, Kunming 650093, China
    不详
    Cailiao Kexue yu Gongyi, 2007, 3 (319-324):
  • [44] Fully coupled micro/macro deformation, damage, and failure prediction for SiC/Ti-15-3 laminates
    Bednarcyk, BA
    Arnold, SM
    JOURNAL OF AEROSPACE ENGINEERING, 2002, 15 (03) : 74 - 83
  • [45] Study of Ti-15-3 titanium alloy sheet
    Zhu, JW
    Qi, YL
    Li, MQ
    Zhao, YQ
    Wang, QR
    RARE METAL MATERIALS AND ENGINEERING, 2006, 35 : 213 - 216
  • [46] Ti-15-3合金的超塑性
    潘雅琴
    杨昭苏
    稀有金属, 1992, (05) : 346 - 349
  • [47] Ti-15-3合金的性能数据
    王庆如,张庆玲,陈玉文,储俊鹏,居学宁,魏寿庸,王鼎春,史正敏,高颀,宋晋
    材料工程, 1996, (11) : 17 - 21
  • [48] Prediction and simulation of microstructure of Ti-15-3 alloy
    Li, P
    Xue, KM
    Lu, Y
    Tan, JR
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2003, 19 : 161 - 163
  • [49] Aging characterization and application of Ti-15-3 alloy
    Ma, JM
    Wang, QR
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2): : 150 - 154
  • [50] DYNAMIC FRACTURE-BEHAVIOR OF SICF/TI-15-3 METAL-MATRIX COMPOSITE
    KLOPP, RW
    CROCKER, JE
    INTERNATIONAL JOURNAL OF FRACTURE, 1993, 61 (04) : R77 - R83