共 50 条
- [21] EFFECT OF PRETREATMENT TEMPERATURE ON PROTECTION OF 70-30 BRASS WITH BENZOTRIAZOLE [J]. DENKI KAGAKU, 1979, 47 (10): : 592 - 596
- [23] MICROSTRUCTURAL DAMAGE ADJACENT TO BULLET HOLES IN 70-30 BRASS [J]. JOURNAL OF THE AUSTRALASIAN INSTITUTE OF METALS, 1970, 15 (01): : 1 - &
- [24] SURFACE EFFECTS DURING THE ANNEALING OF 70-30 BRASS - DISCUSSION [J]. JOURNAL OF THE INSTITUTE OF METALS, 1947, 73 (09): : 873 - 874
- [25] Stress-corrosion cracking of 70-30 brass by amines [J]. TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1944, 156 : 212 - 220
- [26] NUCLEATION AND ANNEALING TEXTURE DEVELOPMENT IN ROLLED 70-30 BRASS [J]. ZEITSCHRIFT FUR METALLKUNDE, 1980, 71 (01): : 15 - 20
- [27] RECRYSTALLIZATION OF 70-30 BRASS DURING INDUCTION-HEATING [J]. JOURNAL OF MATERIALS SCIENCE, 1980, 15 (07) : 1804 - 1813
- [28] ROLLING AND ANNEALING OF FINE-GRAINED 70-30 BRASS [J]. TEXTURES AND MICROSTRUCTURES, 1989, 10 (02): : 135 - 152
- [30] ANNEALING TWINS IN COPPER AND 70-30 ALPHA-BRASS [J]. JOURNAL OF METALS, 1950, 2 (08): : 1020 - 1022