CORROSION FATIGUE BEHAVIOR OF 13CR MARTENSITIC STAINLESS-STEELS IN 3-PERCENT NACL SOLUTION WITH A SPECIAL REFERENCE TO THEIR INTERGRANULAR CORROSION SUSCEPTIBILITY

被引:1
|
作者
OZAKI, T [1 ]
ISHIKAWA, Y [1 ]
MUKAI, Y [1 ]
机构
[1] OSAKA UNIV,FAC ENGN,OSAKA,JAPAN
关键词
D O I
10.2355/tetsutohagane1955.75.3_523
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
引用
收藏
页码:523 / 528
页数:6
相关论文
共 50 条
  • [41] Effect of Tempering Treatment on Atmospheric Corrosion Behavior of 3Cr13 Martensitic Stainless Steel in Marine Environment
    Lian, Yong
    Zhang, Jin
    Ji, Pengfei
    Zhang, Zunjun
    Ma, Minyu
    Zhao, Chao
    Huang, Jinfeng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (06) : 4963 - 4973
  • [42] Effect of Tempering Treatment on Atmospheric Corrosion Behavior of 3Cr13 Martensitic Stainless Steel in Marine Environment
    Yong Lian
    Jin Zhang
    Pengfei Ji
    Zunjun Zhang
    Minyu Ma
    Chao Zhao
    Jinfeng Huang
    Journal of Materials Engineering and Performance, 2022, 31 : 4963 - 4973
  • [43] CORROSION FATIGUE BEHAVIOR OF THE AUSTENITIC STEEL X-6 CRNIMOTI 17-12-2 IN 3-PERCENT NACL-SOLUTION UNDER ROTATING BENDING LOAD
    ROEDER, E
    BASSLER, HJ
    HUBER, M
    VOLLMAR, J
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1992, 43 (09): : 426 - 431
  • [44] ELECTROCHEMICAL STUDY ON STRESS-CORROSION CRACKING OF TYPE-430 FERRITIC STAINLESS-STEEL BY POTENTIOSTATIC CERT METHOD IN 3-PERCENT NACL SOLUTION
    OKI, T
    KONDOW, H
    KUWANO, S
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1982, 46 (01) : 73 - 77
  • [45] LOW-RATE FATIGUE CRACK-PROPAGATION PROPERTIES IN 3-PERCENT SODIUM-CHLORIDE AQUEOUS-SOLUTION FOR VARIOUS HIGH-STRENGTH AND STAINLESS-STEELS
    MATSUOKA, S
    SHIMODAIRA, M
    MASUDA, H
    TAKEUCHI, E
    NISHIJIMA, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (06): : 707 - 714
  • [46] Localized Corrosion Behavior of 6% Mo Super Austenitic & 316L Stainless Steels in Low pH 3% NaCl Solution
    M.M.A.Gad
    H.G.Salem
    A.M.Nasreldin
    H.Sabry
    A.A.EI-Sayed
    Journal of Materials Science & Technology, 2005, (04) : 465 - 469
  • [47] Localized corrosion behavior of 6% Mo super austenitic & 316L stainless steels in low pH 3% NaCl solution
    Gad, MMA
    Salem, HG
    Nasreldin, AM
    Sabry, H
    El-Sayed, AA
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 21 (04) : 465 - 469
  • [48] ON THE STRESS-CORROSION CRACKING BEHAVIOR OF ALUMINUM-ALLOY SHEET IN AN AQUEOUS-SOLUTION OF 3-PERCENT NACL+0.3-PERCENT H2O2
    BRAUN, R
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1994, 45 (05): : 255 - 263
  • [49] Corrosion Behavior of Supermartensitic Stainless Steel 13Cr and Stainless Steel 316L Under Chloride Solution and H2S/CO2 Environments
    Costa, Josiane Soares
    Altenhofen, Aldo
    CORROSION, 2024, 80 (09) : 880 - 888
  • [50] Effect of nitrogen on corrosion behavior of 28Cr-7Ni duplex and microduplex stainless steels in air-saturated 3.5 wt% NaCl solution
    Lothongkum, G
    Wongpanya, P
    Morito, S
    Furuhara, T
    Maki, T
    CORROSION SCIENCE, 2006, 48 (01) : 137 - 153