DAMAGE MECHANISMS OF SCS-6/TI-6AL-4V COMPOSITES UNDER THERMAL-MECHANICAL FATIGUE

被引:13
|
作者
JENG, SM [1 ]
YANG, JM [1 ]
AKSOY, S [1 ]
机构
[1] TEXTRON LYCOMING,STRATFORD,CT 06497
基金
美国国家科学基金会;
关键词
D O I
10.1016/0921-5093(92)90143-O
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The damage mechanisms of the unidirectional SCS-6/Ti-6Al-4V composites under thermal-mechanical fatigue loading and high temperature isothermal fatigue were studied. The maximum cyclic temperature varied from 370 to 650-degrees-C and maximum applied stresses ranged from 828 to 1180 MPa. The resulting thermal-mechanical fatigue life for each condition was plotted against the maximum stress in the matrix. The crack initiation and propagation mechanisms were identified. It was found that matrix cracking with unbroken fiber bridging is the major damage mode for the composites under thermal-mechanical fatigue and isothermal fatigue loading. Furthermore, oxidation-assisted matrix cracking and oxidation pitting on the fiber surface are the major damage mechanisms for high temperature oxidizing environments.
引用
收藏
页码:117 / 124
页数:8
相关论文
共 50 条
  • [31] Tool wear behavior of thermal-mechanical effect for milling Ti-6Al-4V alloy in cryogenic
    Wang, Fengbiao
    Wang, Yongqing
    Liu, Haibo
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 94 (5-8): : 2077 - 2088
  • [32] Tool wear behavior of thermal-mechanical effect for milling Ti-6Al-4V alloy in cryogenic
    Wang, Fengbiao (wangfb@dlut.edu.cn), 1600, Springer London (94): : 5 - 8
  • [33] Tool wear behavior of thermal-mechanical effect for milling Ti-6Al-4V alloy in cryogenic
    Fengbiao Wang
    Yongqing Wang
    Haibo Liu
    The International Journal of Advanced Manufacturing Technology, 2018, 94 : 2077 - 2088
  • [34] On the mechanisms of superplasticity in Ti-6Al-4V
    Alabort, E.
    Kontis, P.
    Barba, D.
    Dragnevski, K.
    Reed, R. C.
    ACTA MATERIALIA, 2016, 105 : 449 - 463
  • [35] Transformation superplasticity of Ti-6Al-4V and Ti-6Al-4V/TiC composites at high stresses
    Schuh, C
    Dunand, DC
    SUPERPLASTICITY IN ADVANCED MATERIALS, ICSAM-2000, 2001, 357-3 : 177 - 182
  • [36] EFFECT OF FIBER COATING ON THE FRACTURE AND FATIGUE RESISTANCE OF SCS-6/TI3AL COMPOSITES
    CHIU, HP
    YANG, JM
    ACTA METALLURGICA ET MATERIALIA, 1995, 43 (07): : 2581 - 2587
  • [37] Fatigue damage of Ti-6242/SCS-6 metal matrix composite
    Bettge, D
    Günther, B
    Wedell, W
    Portella, PD
    Hemptenmacher, J
    Peters, PWM
    AFFORDABLE METAL MATRIX COMPOSITES FOR HIGH-PERFORMANCE APPLICATIONS II, 2003, : 81 - 90
  • [39] Strength of SCS-6 fibers in a Tiβ21s/SCS-6 composite before and after fatigue
    Liu, J
    Bowen, P
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34A (05): : 1203 - 1213
  • [40] Fatigue Behavior and Damage Evolution of SiC Fiberreinforced Ti-6Al-4V Alloy Matrix Composites
    Feng Guanghai
    Yang Yanqing
    Li Jian
    Luo Xian
    Huang Bin
    Sun Qing
    Wu Chen
    Chen Yan
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (09) : 2049 - 2054