Control of Glass Infiltration at the Al2O3/Glass/Al2O3 Interface

被引:1
|
作者
Jo, Tae-Jin [1 ]
Yeo, Dong-Hun [1 ]
Shin, Hyo-Soon [1 ]
Hong, Youn-Woo [1 ]
Cho, Yong-Soo [2 ]
机构
[1] Korea Inst Ceram Engn & Technol, Bio IT Convergence Ctr, Seoul 153801, South Korea
[2] Yonsei Univ, Dept Mat Sci & Engn, Seoul 120749, South Korea
关键词
Zero shrinkage; Glass infiltration; Al2O3/Glass/Al2O3; De-lamination; Low temperature co-fired ceramic;
D O I
10.4313/TEEM.2011.12.1.32
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A zero-shrinkage sintering process in which the shrinkage of the x-y axis is controlled to be zero is in great demand due to the high integration trend in ceramic modules. Among the zero-shrinkage sintering processes available, the glass infiltration method proposed in the preliminary study with an Al2O3/ Glass/ Al2O3 structure is one promising method. However, problems exist in regard to the glass infiltration method, including partially incomplete joining between Al2O3 and glass layers due to the precipitate of Ti-Pb rich phase during the sintering process. Therefore, we wish to solve the de-lamination problems and suggest a mechanism for delamination and the solutions in the zeroshrinkage low temperature co-fired ceramic (LTCC) layers. The de-lamination problems diminished using the Pb-BSi- O glass without TiO2 in Pb-B-Ti-Si-O glass and produced a very dense zero-shrinkage LTCC.
引用
下载
收藏
页码:32 / 34
页数:3
相关论文
共 50 条
  • [31] Metastable superconductivity of the Al/Al2O3 interface
    Sidorov, N. S.
    Palnichenko, A. V.
    Khasanov, S. S.
    JETP LETTERS, 2011, 94 (02) : 134 - 136
  • [32] Sintering behaviour and microstructures of Ti(Al,O)/Al2O3, Ti3Al(O)/Al2O3 and TiAl(O)/Al2O3 in situ composites
    Cai, ZH
    Zhang, DL
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 419 (1-2): : 310 - 317
  • [33] Role of Ti diffusion on the formation of phases in the Al2O3–Al2O3 brazed interface
    Abhijit Kar
    Sudipta Mandal
    Rabindra N. Ghosh
    Tamal K. Ghosh
    Ajoy Kumar Ray
    Journal of Materials Science, 2007, 42 : 5556 - 5561
  • [34] ON THE ATOMIC-STRUCTURE OF THE NB/AL2O3 INTERFACE AND THE GROWTH OF AL2O3 PARTICLES
    KUWABARA, M
    SPENCE, JCH
    RUHLE, M
    JOURNAL OF MATERIALS RESEARCH, 1989, 4 (04) : 972 - 977
  • [35] Boron Emitter Passivation With Al2O3 and Al2O3/SiNx Stacks Using ALD Al2O3
    Richter, Armin
    Benick, Jan
    Hermle, Martin
    IEEE JOURNAL OF PHOTOVOLTAICS, 2013, 3 (01): : 236 - 245
  • [36] Oxidation of volatile organic compounds on Al2O3, Pd/Al2O3, and PdO/Al2O3 catalysts
    Cordi, EM
    Falconer, JL
    JOURNAL OF CATALYSIS, 1996, 162 (01) : 104 - 117
  • [37] H2S ADSORPTION ON AL2O3, MODIFIED AL2O3, AND MOO3/AL2O3
    OKAMOTO, Y
    OHHARA, M
    MAEZAWA, A
    IMANAKA, T
    TERANISHI, S
    JOURNAL OF PHYSICAL CHEMISTRY, 1986, 90 (11): : 2396 - 2407
  • [38] RADIAL PROFILES IN PT/AL2O3, RE/AL2O3, AND PT-RE/AL2O3
    DEMIGUEL, SR
    SCELZA, OA
    CASTRO, AA
    BARONETTI, GT
    ARDILES, DR
    PARERA, JM
    APPLIED CATALYSIS, 1984, 9 (03): : 309 - 315
  • [39] Oxidation of Volatile Organic Compounds on Al2O3, Pd/Al2O3, and PdO/Al2O3 Catalysts
    Cordi, E. M.
    Falconer, J. L.
    Journal of Catalysis, 162 (01):
  • [40] Low cost Ti(Al,O)/Al2O3 and TixAly/Al2O3 composites
    Zhang, DL
    Cai, ZH
    Newby, M
    MATERIALS TECHNOLOGY, 2003, 18 (02) : 94 - 98