INFLUENCE OF HEAT-TREATMENT CONDITIONS ON THE PROPERTIES OF CAST VNL-3 STEEL

被引:0
|
作者
BRATUKHIN, AG
机构
关键词
D O I
10.1007/BF00703629
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
1. An optimum combination of mechanical properties for the VNL-3 steel grade composition is achieved by a double heat treatment: heating to 1100°C (1 h) with air cooling, annealing at 600°C for 1/2 h plus quenching from 970°C, cold treatment at -50 to -70°C and annealing at 450°C. This heat treatment system can be recommended for obtaining high strength, although in order to secure better ductility, a strengthening heat treatment is carried out as follows: quenching from 970°C, annealing at 450°C and cold treatment at -50 to -70°C. 2. The heating temperature for the second heat-treatment stage is increased to 1100°C in order to correct casting defects (carburization). This yields σB ≥ 1000 N/mm2, σ≥18%, and a1=90-110 J/cm2. 3. Heating of the VNL-3 steel should be carried out in a shielding atmosphere or in a vacuum. The component surface can also be protected by applying the ÉVT-10 enamel. © 1992 Plenum Publishing Corporation.
引用
收藏
页码:164 / 165
页数:2
相关论文
共 50 条
  • [21] TIME-TEMPERATURE TRANSFORMATION CURVES FOR USE IN THE HEAT-TREATMENT OF CAST STEEL
    EDDY, CT
    MARCOTTE, RJ
    SMITH, RJ
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1945, 162 : 250 - 267
  • [22] HEAT-TREATMENT AND PROPERTIES OF MODIFIED HEAT-RESISTANT BEARING STEEL
    KONTER, LY
    FEDOTOVA, VD
    LEVITIN, VS
    METAL SCIENCE AND HEAT TREATMENT, 1981, 23 (9-10) : 697 - 699
  • [23] INFLUENCE OF HEAT-TREATMENT CONDITIONS ON THE PROPERTIES OF MGO-C BRICKS CONTAINING ALUMINUM
    HAYASHI, S
    TAKAHASHI, H
    WATANABE, A
    OSAKA, A
    MIURA, Y
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1994, 102 (05): : 476 - 481
  • [24] Influence of Heat-treatment on the Microstructure and Properties of Hypereutectic High-Chromium Cast Iron Containing Ti
    Han Yanjun
    Zhi Xiaohui
    Guo Wenwu
    Xing Jiandong
    Gao Yimin
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 : 142 - 145
  • [25] EFFECT OF HEAT-TREATMENT ON STRUCTURE AND PROPERTIES OF MANGANESE CAST-IRON
    STANCHEV, DI
    RUBLEV, VI
    SEDNEV, YG
    FILATOV, AM
    METAL SCIENCE AND HEAT TREATMENT, 1976, 18 (5-6) : 514 - 516
  • [26] EFFECT OF COMPOSITION AND HEAT-TREATMENT ON THE STRUCTURE AND PROPERTIES OF CAST CHROMIUM STEELS
    MALINOV, LS
    CHEILYAKH, AP
    MAKMAK, GI
    KANTOR, SI
    FUCHILO, SM
    STEEL IN TRANSLATION, 1994, 24 (11) : 38 - 41
  • [27] Effect of heat-treatment conditions on surface properties and corrosion behavior of orthodontic stainless steel wires
    Oh, KT
    Joo, UH
    Kim, KN
    CORROSION, 2005, 61 (07) : 639 - 647
  • [28] SPECIFYING FOR HEAT-TREATMENT OF STEEL
    WAINMAN, G
    CME-CHARTERED MECHANICAL ENGINEER, 1978, 25 (09): : 61 - 62
  • [29] INFLUENCE OF HEAT-TREATMENT ON THE STRENGTH AND DUCTILITY OF 85 SPRING STEEL
    BASHNIN, YA
    LISITSKAYA, LA
    KUMINOV, ES
    METAL SCIENCE AND HEAT TREATMENT, 1982, 24 (1-2) : 109 - 111
  • [30] IMPROVEMENT OF STEEL BY HEAT-TREATMENT
    TIETZ, HD
    NEUE HUTTE, 1981, 26 (09): : 356 - 356