Under 14 MeV neutron irradiation, hydrogen is produced due to the (n, p) reaction. One of the significant effects of hydrogen is austenitic steels is a decrease in ductility. In this investigation the objective is to clarify the behavior of hydrogen and to investigate the effect on the ductility in Fe-Cr-Mn austenitic steel. Hydrogen doping was simulated by electrolytic charging. In internal friction measurements, the hydrogen peak was found at 300 K, when the frequency was 600 Hz. This peak increased with charging time and saturated. The saturated peak height increased with the degree of cold work. This suggests that more hydrogen atoms are absorbed into cold worked materials. The work hardening coefficient and the ductility at the maximum load decreased with increasing hydrogen amount. The mechanism of the decrease in ductility is discussed in terms of dislocations behavior.
引用
下载
收藏
页码:656 / 658
页数:3
相关论文
共 50 条
  • [21] Irradiation damage behavior of aging precipitated carbide in Fe-Cr-Mn steel
    Hu, BF
    Hkinoshita, H
    Sakaguchi, K
    Takahashi, H
    ACTA METALLURGICA SINICA, 2006, 42 (03) : 234 - 238
  • [22] SOLUBILITY OF NITROGEN IN FE-CR-MN ALLOYS
    NIZHELSKIY, PE
    NIZHELSKAYA, SG
    RUSSIAN METALLURGY, 1976, (02): : 51 - 55
  • [23] Hydrogen effect on thermodynamic stability of γ- and ε-phases in a Fe-Cr-Mn solid solution
    Movchan, D. N.
    Shanina, B. D.
    Gavriljuk, V. G.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (20) : 8471 - 8477
  • [24] NITROGEN CONCENTRATION IN FE-CR-MN ALLOYS
    RAWERS, JC
    KIKUCHI, M
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1993, 2 (05) : 651 - 658
  • [25] Change in the properties of Fe-Cr-Ni and Fe-Cr-Mn austenitic steels under mixed and fast neutron irradiation
    Shamardin, VK
    Bulanova, TM
    Golovanov, VN
    Neustroyev, VS
    Povstyanko, AV
    Ostrovsky, ZE
    JOURNAL OF NUCLEAR MATERIALS, 1996, 233 : 162 - 168
  • [26] Phase stability in sub-stable austenitic Fe-Cr-Mn(W,V) alloy
    Jia, Chengchang
    Lu, Lin
    Sun, Jingyuan
    Hu, Benfu
    Jinshu Rechuli Xuebao/Transactions of Metal Heat Treatment, 2000, 21 (01): : 12 - 19
  • [27] Irradiation damage behavior of aging precipitated carbide in Fe-Cr-Mn steel
    Hu, Benfu
    Hkinoshita, Hiroshi
    Sakaguchi, Kisiki
    Takahashi, Heishichiro
    Jinshu Xuebao/Acta Metallurgica Sinica, 2006, 42 (03): : 234 - 238
  • [28] High damping Fe-Cr-Mn alloy
    Igata, N.
    Aoyama, H.
    Kanja, Y.
    Habara, Y.
    Journal De Physique. IV : JP, 1996, 6 (08): : 791 - 794
  • [30] VAPORIZATION OF MN FROM SURFACE OF FE-CR-MN ALLOY
    TADA, K
    HISATSUNE, Y
    FUJIWARA, T
    YAMAMOTO, M
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (02) : 168 - 174