Fundamental characteristics of high early strength low heat concrete according to mineral binder and high early strength material combination

被引:1
|
作者
Kim, Kyoungmin [1 ]
Son, Hojung [2 ]
机构
[1] Architectural Technol Res Team, Suwon 440210, South Korea
[2] Korea Concrete Testing Lab, Ansan 426220, South Korea
关键词
Early age strength; Low heat cement; Heat of hydration; Mass concrete;
D O I
10.6111/JKCGCT.2014.24.1.027
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
This study analyzed the fundamental characteristics of concrete according to a ternary system mixing in order to reduce hydration heat of mass concrete and to improve early age strength. The results are as follows. The fluidity of unconsolidated concrete satisfied the target scope regardless of the binder conditions. When the replacement ratio between FA and BS increased, the slump of low heat-A mix and low heat-B mix increased, and air content was not affected by the change of binders. As for setting time, low heat cement mix had the fastest regardless of W/B, and high early strength low heat mix achieved 6 hours' reduction compared with low heat-B mix at initial set, and 12 hours' reduction at the final set respectively. As for the simple hydration heat, the low mix peak temperature was the highest and low heat-B mix had the lowest temperature. And high early strength low heat mix was similar with that of low heat-B. The compressive strength of hardened concrete had similar strength scope in all mixes except for low heat-B mix at early ages, and had unexceptionally similar one without huge differences at long-term ages.
引用
收藏
页码:27 / 32
页数:6
相关论文
共 50 条
  • [21] Evaluation of capillary pore size characteristics in high-strength concrete at early ages
    Igarashi, S
    Watanabe, A
    Kawamura, M
    CEMENT AND CONCRETE RESEARCH, 2005, 35 (03) : 513 - 519
  • [23] Performances of the high strength low heat pump concrete (HLPC)
    Yun-sheng Z.
    Wei S.
    Shu-guang H.
    Qing-jun D.
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2002, 17 (3): : 56 - 59
  • [24] Performances of the high strength low heat pump concrete (HLPC)
    Zhang, YS
    Sun, W
    Hu, SG
    Ding, QJ
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2002, 17 (03): : 56 - 59
  • [25] Performances of the high strength low heat pump concrete (HLPC)
    Zhang, Yun-Sheng
    Sun, Wei
    Hu, Shu-Guang
    Ding, Qing-Jun
    Journal Wuhan University of Technology, Materials Science Edition, 2002, 17 (03): : 56 - 59
  • [26] Compressive strength performance of low- and high-strength concrete soaked in mineral oil
    Diab, Hesham
    CONSTRUCTION AND BUILDING MATERIALS, 2012, 33 : 25 - 31
  • [27] Early cover spalling in high-strength concrete columns
    Bae, S
    Bayrak, O
    JOURNAL OF STRUCTURAL ENGINEERING-ASCE, 2003, 129 (03): : 314 - 323
  • [28] High early strength latex-modified concrete overlay
    Sprinkel, Michael M.
    Transportation Research Record, 1988, (1204) : 42 - 51
  • [29] Technogenic anhydrite binder for high-strength concrete
    Ponomarenko, A. A.
    MAGAZINE OF CIVIL ENGINEERING, 2021, 107 (07):
  • [30] Development and Optimization of High Early Strength Concrete Mix Design
    Golaszewski, Jacek
    Cygan, Grzegorz
    Golaszewska, Malgorzata
    3RD WORLD MULTIDISCIPLINARY CIVIL ENGINEERING, ARCHITECTURE, URBAN PLANNING SYMPOSIUM (WMCAUS 2018), 2019, 471