- [33] X-RAY-MEASUREMENT OF HEAT-TREATED AL-4.0 WT-PERCENT CU-0.2 WT-PERCENT TI ALLOY CASTINGS ZEITSCHRIFT FUR METALLKUNDE, 1989, 80 (09): : 653 - 657
- [35] EFFECT OF DISSOLUTION OF THE BETA-PHASE ON THE WORK-HARDENING CHARACTERISTICS OF AL-4.5 WT-PERCENT MG ALLOY PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1990, 120 (01): : K31 - K35
- [37] FRACTION EUTECTIC MEASUREMENTS IN SLOWLY COOLED PB-15 WT-PERCENT SN AND SN-15 WT-PERCENT PB ALLOYS JOURNAL OF METALS, 1987, 39 (07): : A62 - A62
- [38] EFFECT OF LOADING ON THE RECOVERY OF INTERNAL-FRICTION OF AN A1-1.0 WT-PERCENT MN-0.28 WT-PERCENT FE ALLOY PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1988, 110 (02): : 481 - 487