- [21] SUBCRITICAL CRACK GROWTH IN TI-6A1-4V PLATE MATERIALS UNDER SUSTAINED LOAD REPORT OF NRL PROGRESS, 1972, (NMAR): : 26 - &
- [22] METALLURGICAL OPTIMIZATION OF COMMERCIAL PURITY TI-6AL-6V-2SN ALLOY REPORT OF NRL PROGRESS, 1975, (SEP): : 18 - 20
- [23] HYDROGEN-INDUCED SLOW CRACK-GROWTH IN TI-6A1-6V-2SN METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1980, 11 (06): : 973 - 981
- [24] CYCLIC CRACK GROWTH AND FRACTURE RESISTANCE OF TI-6AL-6V-2SN AS INFLUENCED BY RECRYSTALLIZATION ANNEAL AND INTERSTITIAL OXYGEN-CONTENT REPORT OF NRL PROGRESS, 1974, (DEC): : 32 - 33
- [25] Load partition and microstructural evolution during in situ hot deformation of Ti-6Al-6V-2Sn alloys MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 657 : 244 - 258
- [26] EFFECT OF MICROSTRUCTURE AND COOLING RATE ON MECHANICAL PROPERTIES OF TI-6AL-6V-2SN MATERIALS RESEARCH AND STANDARDS, 1965, 5 (05): : 257 - +
- [28] INFLUENCE OF MICROSTRUCTURE AND TESTING TEMPERATURE ON MECHANICAL PROPERTIES AND FRACTURE TOUGHNESS OF TI-6AL-6V-2SN MATERIALS RESEARCH AND STANDARDS, 1965, 5 (05): : 257 - +
- [29] STRUCTURE-PROPERTY RELATIONSHIPS IN DUPLEX ANNEALED TI-6AL-6V-2SN JOURNAL OF METALS, 1979, 31 (08): : F21 - F22