摘要
A procedure based on the mechanical properties of a modified anelastic element (MAE) has already been developed to get a functional dependence of the real and imaginary components of the dynamical modulus or compliance. The MAE is essentially a standard anelastic element except for its characteristic time, which depends on the frequency. The analysis of this dependence provides an analytical description of not only the dynamical properties but also the distribution function. In this work it is shown that the procedure can be extended to internal friction peaks, yielding not only the parameters of the distribution function but also the relaxation strength. This procedure is applied to various materials and the results are compared with a previous method proposed in the literature.
引用
收藏
页码:529 / 533
页数:5
相关论文
共 50 条
  • [31] PRECIPITATION INTERNAL-FRICTION PEAK IN AL-MG-SI
    URRETA, SE
    DESALVA, AAG
    LOUCHET, F
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1993, 139 (02): : 345 - 360
  • [32] HYDROGEN INTERNAL-FRICTION PEAK AND THE EFFECT OF QUENCHING IN AMORPHOUS CUTI
    MIZUBAYASHI, H
    KATOH, Y
    OKUDA, S
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1987, 104 (01): : 469 - 485
  • [33] INTERNAL-FRICTION PEAK IN AMORPHOUS SELENIUM AT LOW-TEMPERATURE
    DUQUESNE, JY
    BELLESSA, G
    JOURNAL OF PHYSICS C-SOLID STATE PHYSICS, 1980, 13 (10): : L215 - L219
  • [34] CONCERNING BLOCK PEAK OF INTERNAL-FRICTION IN COPPER CRYSTAL WHISKERS
    POSTNIKO.VS
    YURYEV, VA
    BELIKOV, AM
    KOSILOV, AT
    PHYSICS OF METALS AND METALLOGRAPHY-USSR, 1971, 32 (03): : 218 - &
  • [35] INTERNAL-FRICTION AND STRENGTH OF WHISKER-CRYSTALS OF GERMANIUM
    POSTNIKOV, VS
    AMMER, SA
    DROZHZHI.AI
    KRISTALLOGRAFIYA, 1973, 18 (03): : 658 - 659
  • [36] A NEW INTERNAL-FRICTION PEAK EXCEEDING THE MARTENSITIC-TRANSFORMATION PEAK OF CUZNAL ALLOYS
    HARANGOZO, IZ
    CSERESNYES, Z
    DAROCZI, L
    KISS, S
    KEDVES, FJ
    SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (03): : 475 - 480
  • [37] INTERNAL-FRICTION, DIELECTRIC LOSS AND NMR RELAXATION IN IONIC CONDUCTORS
    GAO, GR
    NGAI, KL
    KEXUE TONGBAO, 1982, 27 (03): : 269 - 274
  • [38] INTERNAL-FRICTION DUE TO GRAIN-BOUNDARY RELAXATION IN ZIRCONIUM
    MOORTHY, SA
    RAO, CN
    ASUNDI, MK
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1986, 39 (03): : 232 - 234
  • [39] ANALYSIS OF ANELASTIC RELAXATION AND INTERNAL-FRICTION DATA OF AMORPHOUS MATERIALS
    VANDENBEUKEL, A
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1992, 129 (01): : 49 - 58
  • [40] ON THE GRAIN-BOUNDARY INTERNAL-FRICTION PEAK OF ALPHA-BRASSES
    FARID, ZM
    SALEH, S
    MAHMOUD, SA
    JOURNAL OF MATERIALS SCIENCE, 1990, 25 (1B) : 519 - 521