COLD WORK EFFECTS ON SULFIDE STRESS CRACKING OF PIPELINE STEEL EXPOSED TO SOUR ENVIRONMENTS

被引:29
|
作者
HUANG, H
SHAW, WJD
机构
[1] Department of Mechanical Engineering, The University of Calgary, Calgary
关键词
D O I
10.1016/0010-938X(93)90259-J
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Cold work effects on sulfide stress cracking of a pipeline steel were examined for exposure to a sour gas environment. Cold worked steel was found to be sensitive to hydrogen embrittlement. The fracture toughness decreases with increasing cold work. Sufficiently low values of fracture toughness may be achieved to promote plane strain fracture even in relatively thin laboratory specimens after a steady state level of hydrogen has occurred in the material. Sulfide stress cracking failure of steel with low amounts of cold work (<30%) is by transgranular cleavage fracture, while heavily cold worked steel shows secondary cracks and microvoid coalescence. The results indicate that sulfide stress cracking of the steel is a mixture of anodic stress corrosion cracking (SCC) and hydrogen embrittlement. The anodic SCC mechanism is mainly promoted by carbon dioxide and a high level of chloride.
引用
收藏
页码:61 / 78
页数:18
相关论文
共 50 条
  • [31] Role of Hydrogen in the Sulfide Stress-Corrosion Cracking of Pipeline Steels
    V. Yu. Chernov
    V. D. Makarenko
    L. S. Shlapak
    Materials Science, 2003, 39 : 144 - 147
  • [32] Effects of zinc injection on stress corrosion cracking of cold worked austenitic stainless steel in high-temperature water environments
    Zhang, Lefu
    Chen, Kai
    Wang, Jiamei
    Guo, Xianglong
    Du, Donghai
    Andresen, Peter L.
    SCRIPTA MATERIALIA, 2017, 140 : 50 - 54
  • [33] Investigation on cold cracking susceptibility of X100 pipeline steel
    Yan C.
    Yuan Y.
    Zhang K.
    Wu L.
    Wang B.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (12): : 41 - 46
  • [34] EFFECT OF COLD WORK ON STRESS-CORROSION CRACKING OF TYPE 302 AUSTENITIC STAINLESS STEEL
    GREELEY, PJ
    RUSSO, VJ
    SAXER, RK
    MYERS, JR
    CORROSION, 1965, 21 (10) : 327 - &
  • [35] Microstructural characterization of the API X-70 pipeline steel under sour environments
    Contreras, A
    Albiter, A
    Angeles-Chavez, C
    Pérez, R
    EMERGING FIELDS IN SOL-GEL SCIENCE AND TECHNOLOGY, 2003, : 381 - 391
  • [36] Definition of Factor Cracking Strength of High Tensile Strength Steel in Sour Hydrogen Sulfide Medium
    Shashkova, L. V.
    Savchenkov, E. A.
    MECHANIKA 2009 - PROCEEDINGS OF THE 14TH INTERNATIONAL CONFERENCE, 2009, : 361 - 363
  • [37] Effect of Pipe Steel Strength on Sulfide Stress Cracking Resistance
    A. A. Kholodnyi
    Yu. I. Matrosov
    Ya. S. Kuznechenko
    Metallurgist, 2018, 62 : 541 - 548
  • [38] SULFIDE STRESS-CORROSION CRACKING OF STEEL AND MEANS TO PREVENT IT
    NAZAROV, AA
    PROTECTION OF METALS, 1992, 28 (04): : 407 - 417
  • [39] Effect of Pipe Steel Strength on Sulfide Stress Cracking Resistance
    Kholodnyi, A. A.
    Matrosov, Yu. I.
    Kuznechenko, Ya. S.
    METALLURGIST, 2018, 62 (5-6) : 541 - 548
  • [40] Identifying sulfide stress cracking stages on a HSLA pipeline steel in H2S environment by electrochemical noise
    Li, Xiaohua
    Song, Jian
    Gan, Kefu
    Xia, Da-Hai
    Gao, Zhiming
    Liu, Chenxi
    Liu, Yongchang
    JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 2020, 876