摘要
High-temperature microstructures of an MgO-hot-pressed Si3N4 and a Yb2O3 + Al2O3-sintered/annealed Si3N4 were obtained by quenching thin specimens from temperatures between 1350-degrees and 1550-degrees-C. Quenching materials from 1350-degrees-C produced no observable changes in the secondary phases at triple-grain junctions or along grain boundaries. Although quenching from temperatures of approximately 1450-degrees-C also showed no significant changes in the general microstructure or morphology of the Si3N4 grains, the amorphous intergranular film thickness increased substantially from an initial approximately 1 nm in the slowly cooled material to 1.5-9 nm in the quenched materials. The variability of film thickness in a given material suggests a nonequilibrium state. Specimens quenched froin 1550-degrees-C revealed once again thin (1-nm) intergranular films at all high-angle grain boundaries, indicating an equilibrium condition. The changes observed in intergranular-film thickness by high-resolution electron microscopy can be related to the eutectic temperature of the system and to diffusional and viscous processes occurring in the amorphous intergranular film during the high-temperature anneal prior to quenching.
引用
收藏
页码:2801 / 2808
页数:8
相关论文
共 50 条
  • [1] IMPURITY-ENHANCED INTERGRANULAR CAVITY FORMATION IN SILICON-NITRIDE AT HIGH-TEMPERATURES
    TANAKA, I
    PEZZOTTI, G
    MATSUSHITA, K
    MIYAMOTO, Y
    OKAMOTO, T
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (04) : 752 - 759
  • [2] CORROSION BEHAVIOR OF SILICON-NITRIDE CERAMICS IN CAUSTIC ALKALINE-SOLUTIONS AT HIGH-TEMPERATURES
    SATO, T
    SATO, S
    TAMURA, K
    OKUWAKI, A
    [J]. BRITISH CERAMIC TRANSACTIONS AND JOURNAL, 1992, 91 (04): : 117 - 120
  • [3] EFFECTS OF OXIDATION ON INTERGRANULAR PHASES IN SILICON-NITRIDE CERAMICS
    CINIBULK, MK
    KLEEBE, HJ
    [J]. JOURNAL OF MATERIALS SCIENCE, 1993, 28 (21) : 5775 - 5782
  • [4] RETAINER-DEPENDENT WEAR OF SILICON-NITRIDE BEARINGS AT HIGH-TEMPERATURES
    MUTOH, Y
    TANAKA, K
    UENOHARA, M
    [J]. JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 1994, 116 (03): : 463 - 469
  • [5] FRACTURE ENERGY AND TENSILE-STRENGTH OF SILICON-NITRIDE AT HIGH-TEMPERATURES
    OHJI, T
    SAKAI, S
    ITO, M
    YAMAUCHI, Y
    KANEMATSU, W
    ITO, S
    [J]. NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1990, 98 (03): : 235 - 242
  • [6] QUANTITATIVE ESTIMATION OF INTERGRANULAR GLASSY PHASE OF SILICON-NITRIDE CERAMICS
    TAKATORI, K
    WADA, S
    KOBAYASHI, N
    [J]. NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1993, 101 (04): : 480 - 483
  • [7] DEFECTS IN AMORPHOUS HYDROGENATED SILICON-NITRIDE FILMS
    KANICKI, J
    WARREN, WL
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 1993, 166 : 1055 - 1060
  • [8] CONTROLLED CRYSTALLIZATION OF THE AMORPHOUS PHASE IN SILICON-NITRIDE CERAMICS
    BONNELL, DA
    TIEN, TY
    RUHLE, M
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1987, 70 (07) : 460 - 465
  • [9] ANELASTIC RELAXATION ASSOCIATED WITH THE INTERGRANULAR PHASE IN SILICON-NITRIDE AND ZIRCONIA CERAMICS
    LAKKI, A
    SCHALLER, R
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1994, 211 : 365 - 368
  • [10] STATISTICAL-ANALYSIS OF THE INTERGRANULAR FILM THICKNESS IN SILICON-NITRIDE CERAMICS
    KLEEBE, HJ
    CINIBULK, MK
    CANNON, RM
    RUHLE, M
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (08) : 1969 - 1977