INFLUENCE OF NITRIDE (CR2N) PRECIPITATION ON THE PLASTIC-FLOW BEHAVIOR OF HIGH-NITROGEN AUSTENITIC STAINLESS-STEEL

被引:66
|
作者
SIMMONS, JW
机构
[1] U.S. Bureau of Mines, Albany Research Center, Albany
来源
SCRIPTA METALLURGICA ET MATERIALIA | 1995年 / 32卷 / 02期
关键词
D O I
10.1016/S0956-716X(99)80048-X
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Aging at 700 °C results in grain boundary nitride precipitation only, while aging at 900 °C results in grain boundary and cellular precipitation (40 vol%). These thermal treatments have a small but positive effect on YS, no effect on the UTS, but dramatically reduce the ability of the material to deform under localized plastic deformation (necking), leading to reduced tensile ductility. The plastic flow behavior of all annealed and aged high-nitrogen samples were modeled using the modified Ludwik relation (equation 2). Below the UTS, grain boundary nitride precipitation at 700 °C has no measurable effect on the plastic flow behavior of the material, and the modeling parameters n1, K1, n2, and K2 have values which do not deviate significantly from the behavior of the un-aged material. Cellular precipitation, caused by aging at 900 °C, does significantly affect the plastic flow behavior of the material at both low and high strains. Cellular precipitation causes both increased strengthening of the matrix in the low strain regime (0.001 < ε < 0.03) and systematic decreases in the strain hardening exponent (n1) and strength coefficient (K1) with increased aging. The rate of strain hardening ( dσ dε) measured from the σ-ε plots is unaffected by isothermal aging and nitride formation. © 1994.
引用
收藏
页码:265 / 270
页数:6
相关论文
共 50 条
  • [1] Influence of nitride (Cr2N) precipitation on the plastic flow behavior of high-nitrogen austenitic stainless steel
    Simmons, J.W., 1600, Pergamon Press Inc, Tarrytown, NY, United States (32):
  • [2] Precipitation Kinetics of Cr2N in High Nitrogen Austenitic Stainless Steel
    Feng Shi
    Li-jun Wang
    Wen-fang Cui
    Chun-ming Liu
    Journal of Iron and Steel Research International, 2008, 15 : 72 - 77
  • [4] On the crystal structure of Cr2N precipitates in high-nitrogen austenitic stainless steel
    Lee, TH
    Oh, CS
    Han, HN
    Lee, CG
    Kim, SJ
    Takaki, S
    ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE CRYSTAL ENGINEERING AND MATERIALS, 2005, 61 : 137 - 144
  • [5] Effect of Cr2N precipitation on deformed microstructure in high nitrogen austenitic stainless steel
    Lee, Tae-Ho
    Kim, Sung-Tae
    Bang, Hae-Jung
    Oh, Chang-Seok
    Kim, Sung-Joon
    Takaki, Setsuo
    MECHANICAL BEHAVIOR OF MATERIALS X, PTS 1AND 2, 2007, 345-346 : 161 - +
  • [6] MATRIX PRECIPITATION OF CR2N IN A PHOSPHORUS-CONTAINING AUSTENITIC STAINLESS-STEEL
    KIKUCHI, M
    NISHIMURA, T
    TANAKA, T
    TANAKA, R
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (09): : 1337 - 1339
  • [7] Kinetics of Cr2N Precipitation and Its Effect on Pitting Corrosion of Nickel-Free High-Nitrogen Austenitic Stainless Steel
    Krishna Kumar, K.
    Anburaj, J.
    Dhanasekar, R.
    Satishkumar, T.
    Abuthakir, J.
    Manikandan, P.
    Subramanian, R.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (09) : 6044 - 6052
  • [8] Kinetics of Cr2N Precipitation and Its Effect on Pitting Corrosion of Nickel-Free High-Nitrogen Austenitic Stainless Steel
    K. Krishna Kumar
    J. Anburaj
    R. Dhanasekar
    T. Satishkumar
    J. Abuthakir
    P. Manikandan
    R. Subramanian
    Journal of Materials Engineering and Performance, 2020, 29 : 6044 - 6052
  • [9] Discontinuous precipitation of Cr2N in a high nitrogen, chromium-manganese austenitic stainless steel
    Vanderschaeve, F
    Taillard, R
    Foct, J
    JOURNAL OF MATERIALS SCIENCE, 1995, 30 (23) : 6035 - 6046
  • [10] ON THE LOCALIZATION OF THE PLASTIC-FLOW IN POLYCRYSTALS OF AUSTENITIC STAINLESS-STEEL
    KURZYDLOWSKI, KJ
    CZEREPKO, W
    PLASTICITY OF METALS AND ALLOYS - ISPMA 6, 1994, 97-9 : 501 - 505