VICKERS AND KNOOP INDENTATION BEHAVIOR OF CUBIC AND PARTIALLY-STABILIZED ZIRCONIA CRYSTALS

被引:43
|
作者
GOGOTSI, GA
DUB, SN
LOMONOVA, EE
OZERSKY, BI
机构
[1] Institute for Problems of Strength, the Academy of Sciences of Ukraine, Kiev, 252014
关键词
D O I
10.1016/0955-2219(95)91431-M
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hardness and fracture toughness of cubic zirconia crystals (CZC) doped with yttria and partially stabilized zirconia crystals (PSZC) doped with yttria, terbia and ceria were studied at indentation loads of 0.1-300 N. MOR and K-1c of these materials were measured under bending conditions. A maximum hardness value of H-K = 21.2 GPa was obtained for CZC at a 0.1 N indentation load when a longer diagonal of the Knoop indenter being directed along [110]. Starting from a 2 N load, PSZC exhibited lateral cracks and phase transition zones. Radial cracks in Vickers indentation tests of Y-Tb-PSZC and Y-Ce-PSZC appeared above 40 N and 50 N respectively. Such cracks in Knoop indentation tests were observed above 300 N. Orientation anisotropy of lateral cracks was noticed in all crystals, radial ones were revealed only in CZC. After grinding off the specimen surfaces, lateral cracks were found to be present under the impressions. The calculations of fracture toughness K-1c(v) using the equation proposed by the authors gave a value corresponding to those materials determined on bending.
引用
收藏
页码:405 / 413
页数:9
相关论文
共 50 条
  • [1] SHAPE MEMORY BEHAVIOR IN PARTIALLY-STABILIZED ZIRCONIA CERAMICS
    SWAIN, MV
    NATURE, 1986, 322 (6076) : 234 - 236
  • [2] STRONG AND PARTIALLY-STABILIZED ZIRCONIA CERAMICS
    GARVIE, RC
    HANNINK, RHJ
    HUGHAN, RR
    MCKINNON, NA
    PASCOE, RT
    STRINGER, RK
    JOURNAL OF THE AUSTRALASIAN CERAMIC SOCIETY, 1977, 13 (01): : 8 - 11
  • [3] MICROSTRUCTURE OF TERNARY PARTIALLY-STABILIZED ZIRCONIA
    LENZ, L
    HEUER, AH
    JOURNAL OF METALS, 1981, 33 (09): : A39 - A39
  • [4] SLIP CASTING OF PARTIALLY-STABILIZED ZIRCONIA
    NIKUMBH, AK
    SCHMIDT, H
    MARTIN, K
    PORZ, F
    JOURNAL OF MATERIALS SCIENCE, 1991, 26 (13) : 3649 - 3656
  • [5] CORRELATION OF ELECTRICAL-PROPERTIES AND MICROSTRUCTURES OF PARTIALLY-STABILIZED EXPANDED CUBIC ZIRCONIA
    CHILDERHOSE, T
    SAYER, M
    SMITH, RW
    CIM BULLETIN, 1987, 80 (902): : 100 - 100
  • [6] BLACK COLOR IN PARTIALLY-STABILIZED ZIRCONIA - REPLY
    SORIA, J
    MOYA, JS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (07) : 1747 - 1748
  • [7] MIXED-MODE FRACTURE-BEHAVIOR OF PARTIALLY-STABILIZED ZIRCONIA
    KOGO, Y
    KAGAWA, Y
    HATTA, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (11) : 1272 - 1279
  • [8] LAPPING OF COMPOSITES OF ALUMINA AND PARTIALLY-STABILIZED ZIRCONIA
    SORNAKUMAR, T
    ANNAMALAI, VE
    KRISHNAMURTHY, R
    GOKULARATHNAM, CV
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 1994, 12 (04): : 207 - 210
  • [9] PARTIALLY-STABILIZED ZIRCONIA PISTON BOWL RELIABILITY
    HARTSOCK, DL
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1987, 109 (04): : 367 - 373
  • [10] Sintering of partially-stabilized zirconia and partially-stabilized zirconia-hydroxyapatite composites by hot isostatic pressing and pressureless sintering
    Li, J
    Liao, H
    Hermansson, L
    BIOMATERIALS, 1996, 17 (18) : 1787 - 1790