EFFECT OF MICROSTRUCTURE ON SUSTAINED LOAD CRACKING BEHAVIOR OF TI-6AL-4V ALLOY

被引:0
|
作者
TAKATORI, H
CHIBA, Y
OGURA, T
机构
关键词
TI-6AL-4V; MICROSTRUCTURE; FRACTURE; FRACTURE TOUGHNESS; HEAT TREATMENT; QUASI-CLEAVAGE;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Sustained load cracking behavior of Ti-6Al-4V was studied by constant load testings and constant cross head speed tensile testings using compact tension specimens for four different microstructures. Annealed specimens and duplex annealed specimens showed stable crack growth without incubation time during constant load testings for initial K values which were considerably low, compared with K(IC), while beta annealed specimens and solution treated and aged specimens showed no such behaviors. In the stable crack growth, the rate of COD change decreased with decreasing the load. Fractography and micrography revealed that the stable crack propagation occurred with quasi-cleavage fracture of primary alpha phase. In constant cross head speed tensile testings, the fracture toughness of annealed specimen decreased with decreasing the cross head speed, while beta annealed specimens showed no such behavior. The stable crack growth of annealed specimen initiated at a stress intensity factor about half of K(IC) at the lowest cross head speed.
引用
收藏
页码:837 / 844
页数:8
相关论文
共 50 条
  • [1] SUSTAINED LOAD CRACKING IN A COMMERCIAL PRODUCTION TI-6AL-4V ALLOY
    YODER, GR
    CROOKER, TW
    GRIFFIS, CA
    REPORT OF NRL PROGRESS, 1972, (MAY): : 24 - &
  • [2] EFFECT OF HYDROGEN CONTENT ON SUSTAINED LOAD CRACKING IN TI-6AL-4V
    MEYN, DA
    REPORT OF NRL PROGRESS, 1972, (JUN): : 17 - +
  • [3] EFFECT OF HYDROGEN CONTENT ON FRACTOGRAPHY OF SUSTAINED LOAD CRACKING IN TI-6AL-4V
    MEYN, DA
    REPORT OF NRL PROGRESS, 1976, (APR): : 5 - 7
  • [4] Microstructure of Ti-6Al-4V alloy
    Kim, Tae Wan
    Yoon, Yo Han
    Oh, Ho Ra
    Park, Jong Bum
    Lee, Jung-Il
    Ryu, Jeong Ho
    JOURNAL OF THE KOREAN CRYSTAL GROWTH AND CRYSTAL TECHNOLOGY, 2016, 26 (03): : 126 - 130
  • [5] CHARACTERISTICS OF SUSTAINED-LOAD CRACKING AND HYDROGEN EFFECTS IN TI-6AL-4V
    BOYER, RR
    SPURR, WF
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (01): : 23 - 29
  • [6] Microstructure and Fatigue Behavior of EBSM Ti-6Al-4V Alloy
    Chen Wei
    Chen Zheyuan
    You Yang
    Li Jinshan
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 : 25 - 30
  • [7] Hot deformation behavior of Ti-6Al-4V alloy: Effect of initial microstructure
    Zhang, Z. X.
    Qu, S. J.
    Feng, A. H.
    Shen, J.
    Chen, D. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 718 : 170 - 181
  • [8] Hot deformation behavior of Ti-6Al-4V alloy: Effect of initial microstructure
    Zhang, Z.X.
    Qu, S.J.
    Feng, A.H.
    Shen, J.
    Chen, D.L.
    Journal of Alloys and Compounds, 2017, 718 : 170 - 181
  • [9] EFFECT OF MICROSTRUCTURE ON HYDRIDE PRECIPITATION IN TI-6AL-4V ALLOY
    ENJO, T
    KURODA, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1986, 50 (01) : 20 - 27
  • [10] Effect of hydrogen on the superplasticity and microstructure of Ti-6Al-4V alloy
    Shaoqing, Zhang, 1600, Elsevier Science S.A., Lausanne, Switzerland (218):