摘要
The fatigue crack growth behavior of forged Ti-46.5Al-3Nb-2Cr-0.2W (at.%) was investigated. Heat treatments were used to generate both a nearly fully lamellar microstructure (grains of alpha(2)-gamma lamellae) and a duplex microstructure (equiaxed gamma and lamellar grains) to span the wide range of microstructural conditions available through thermomechanical processing of these alloys. Fatigue crack growth tests using load-shedding threshold and constant-load-amplitude techniques were conducted at room temperature, 600 degrees C (below the ductile-to-brittle transition temperature (DBTT)) and 800 degrees C (above the DBTT). Results show that the fatigue crack growth resistance of the lamellar microstructure is superior to that of the duplex microstructure. The nature of fatigue crack advance depends strongly on microstructure, which explains, at least in part, the differences observed in crack growth rates for the lamellar and duplex microstructures. Fractography was conducted to identify the dominant crack growth mechanisms in both the lamellar and duplex microstructures.
引用
收藏
页码:457 / 464
页数:8
相关论文
共 50 条
  • [1] Effects of microstructure and temperature on fatigue crack growth in the TiAl alloy Ti-46.5Al-3Nb-2Cr-0.2W
    Balsone, Stephen J.
    Larsen, James M.
    Maxwell, David C.
    Jones, J.Wayne
    Materials Science and Engineering A, 1995, A192-19 (pt 1): : 457 - 464
  • [2] Effects of microstructure, temperature and environment on fatigue crack growth in Ti-46.5Al-3Nb-2Cr-0.2Wγ titanium aluminide
    Rosenberger, AH
    Worth, BD
    Larsen, JM
    STRUCTURAL INTERMETALLICS 1997, 1996, : 555 - 561
  • [3] Mechanisms of ambient temperature fatigue crack growth in Ti-46.5Al-3Nb-2Cr-0.2W
    B. D. Worth
    J. M. Larsen
    S. J. Balsone
    J. W. Jones
    Metallurgical and Materials Transactions A, 1997, 28 : 825 - 835
  • [4] Mechanisms of ambient temperature fatigue crack growth in Ti-46.5Al-3Nb-2Cr-0.2W
    Worth B.D.
    Larsen J.M.
    Balsone S.J.
    Jones J.W.
    Metallurgical and Materials Transactions A, 1997, 28 (13) : 825 - 835
  • [5] Mechanisms of ambient temperature fatigue crack growth in Ti-46.5Al-3Nb-2Cr-0.2W
    Worth, BD
    Larsen, JM
    Balsone, SJ
    Jones, JW
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1997, 28 (3A): : 825 - 835
  • [6] Mechanisms of ambient temperature fatigue crack growth in Ti-46.5Al-3Nb-2Cr-0.2W
    Worth, B.D.
    Larsen, J.M.
    Balsone, S.J.
    Jones, J.W.
    Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1997, 28 (03): : 825 - 835
  • [7] Mechanisms of ambient temperature fatigue crack growth in Ti-46.5Al-3Nb-2Cr-0.2W
    Worth, B.D.
    Larsen, J.M.
    Balsone, S.J.
    Jones, J.W.
    Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1997, 28 A (3 A): : 825 - 835
  • [8] Threshold fatigue crack growth behavior of the gamma titanium aluminide alloy Ti-46.5Al-3Nb-2Cr-0.2W under high cycle fatigue conditions
    Worth, BD
    Larsen, JM
    Rosenberger, AH
    STRUCTURAL INTERMETALLICS 1997, 1996, : 563 - 569
  • [10] EFFECT OF MICROSTRUCTURE ON FATIGUE AND TENSILE PROPERTIES OF THE GAMMA-TIAL ALLOY TI-46.5AL-3.ONB-2.1CR-0.2W
    KUMPFERT, J
    KIM, YW
    DIMIDUK, DM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 192 : 465 - 473