HIGH-TEMPERATURE STABILITY OF NICALON UNDER AR OR O-2 ATMOSPHERE

被引:37
|
作者
SHIMOO, T
CHEN, H
OKAMURA, K
机构
[1] Department of Metallurgy and Materials Science, College of Engineering, University of Osaka Prefecture, Osaka-fu, 593, Gakuen-cho, Sakai-shi
关键词
D O I
10.1007/BF01162506
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The thermal stability of Nicalon NL400 at 1573, 1673 and 1773 K has been studied by TGA and XRD. Under an Ar atmosphere, Nicalon pyrolysed severely to crystallize into beta-SiC involving the generation of both SiO and CO. Under an O-2 atmosphere, the oxide film which formed around Nicalon retarded the pyrolytic reaction of the core. Nicalon coated with a silica film by the previous oxidation treatment pyrolysed hardly at all under an Ar atmosphere, because the film restricted the escape of SiO and CO. Nicalon which was oxidation-treated at 1773 K retained 63% of its original strength after heating at 1773 K under an Ar atmosphere. The amorphous silica film was found to resist rapid thermal cycling between room temperature and elevated temperatures.
引用
收藏
页码:456 / 463
页数:8
相关论文
共 50 条
  • [1] Experimental and modeling study of the low to high-temperature oxidation of the methyl isopropyl ketone in O-2/N-2/Ar and O-2/CO2/Ar atmospheres
    Lin, Qianjin
    Liao, Wanxiong
    Cheng, Jia
    Zou, Chun
    Yang, Bin
    Xia, Wenxiang
    [J]. PROCEEDINGS OF THE COMBUSTION INSTITUTE, 2023, 39 (01) : 315 - 324
  • [2] High-temperature reaction of (U,Gd)O-2 with zirconium
    Yamanaka, S
    Tsujimoto, K
    Yamanaka, T
    Uno, M
    Miyake, M
    Katsura, M
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1997, 247 : 252 - 257
  • [3] STABILITY OF FERRITES IN HIGH-TEMPERATURE OXYGEN ATMOSPHERE
    OTA, K
    ARAI, H
    [J]. DENKI KAGAKU, 1985, 53 (12): : 993 - 994
  • [4] HIGH-TEMPERATURE KINETIC-STUDY FOR THE REACTIVE ION ETCHING OF INP IN BCL3/AR/O-2
    DEMOS, AT
    FOGLER, HS
    FOURNIER, J
    ELTA, ME
    [J]. AICHE JOURNAL, 1995, 41 (03) : 658 - 665
  • [5] The effect of high-temperature annealing on tensile strength and its mechanism of Hi-Nicalon SiC fibres under inert atmosphere
    Yao, R. Q.
    Wang, Y. Y.
    Feng, Z. D.
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2008, 31 (09) : 777 - 787
  • [6] HIGH-TEMPERATURE ACTIVE OXIDATION OF CVD-SI3N4 IN AR-O2 ATMOSPHERE
    NARUSHIMA, T
    IGUCHI, Y
    GOTO, T
    HIRAI, T
    YOKOYAMA, Y
    [J]. SOLID STATE IONICS, 1992, 53 : 265 - 269
  • [7] HIGH-TEMPERATURE OXIDATION OF FE-CR ALLOYS IN AR-10-PERCENT-H2O ATMOSPHERE
    KUSABIRAKI, K
    TOKI, H
    ASAMI, K
    ISHIGURO, T
    OOKA, T
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1988, 74 (05): : 863 - 870
  • [8] THE HIGH-TEMPERATURE SLIDING WEAR OF STAINLESS-STEEL IN A CO2 ATMOSPHERE - THE EFFECT OF ADDING LOW CONCENTRATIONS OF O-2
    NEWMAN, PT
    SKINNER, J
    [J]. WEAR, 1986, 112 (3-4) : 291 - 325
  • [9] EXISTENCE OF DEFLAGRATION WAVES IN O-2 H-2 MIXTURES AT HIGH-TEMPERATURE
    DAOU, J
    GAUDUCHEAU, JL
    HALDENWANG, P
    [J]. COMBUSTION SCIENCE AND TECHNOLOGY, 1994, 100 (1-6) : 363 - 369
  • [10] HIGH-TEMPERATURE ACTIVE OXIDATION AND ACTIVE-TO-PASSIVE TRANSITION OF CHEMICALLY VAPOR-DEPOSITED SILICON-NITRIDE IN N-2 O-2 AND AR O-2 ATMOSPHERES
    NARUSHIMA, T
    GOTO, T
    YOKOYAMA, Y
    HAGIWARA, J
    IGUCHI, Y
    HIRAI, T
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (09) : 2369 - 2375