INHIBITION OF RADIOACTIVE CONTAMINATION OF STAINLESS-STEEL IN BOILING WATER-REACTOR

被引:12
|
作者
HONDA, T
MINATO, A
IZUMIYA, M
OHSUMI, K
MATSUBAYASHI, H
机构
[1] HITACHI LTD, DIV NUCL POWER GENERAT, HITACHI 317, JAPAN
[2] CHUGOKU ELECT POWER CO INC, SHIMANE NUCL POWER STN, KASHIMA, SHIMANE 69003, JAPAN
关键词
D O I
10.1080/18811248.1983.9733480
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
引用
收藏
页码:871 / 873
页数:3
相关论文
共 50 条
  • [1] RADIOACTIVE CONTAMINATION OF CARBON-STEEL IN A BOILING WATER-REACTOR
    HONDA, T
    MINATO, A
    OHSUMI, K
    MATSUBAYASHI, H
    [J]. NUCLEAR TECHNOLOGY, 1984, 65 (03) : 438 - 443
  • [2] SUPPRESSION OF RADIATION BUILDUP ON STAINLESS-STEEL IN A BOILING WATER-REACTOR
    HONDA, T
    OHASHI, K
    FURUTANI, Y
    MINATO, A
    [J]. CORROSION, 1987, 43 (09) : 564 - 570
  • [3] RADIATION BUILDUP ON STAINLESS-STEEL IN A BOILING WATER-REACTOR ENVIRONMENT
    HONDA, T
    IZUMIYA, M
    MINATO, A
    OHSUMI, K
    MATSUBAYASHI, H
    [J]. NUCLEAR TECHNOLOGY, 1984, 64 (01) : 35 - 42
  • [4] CHARACTERIZATION OF OXIDE-FILMS ON STAINLESS-STEEL SURFACES OF BOILING WATER-REACTOR PRIMARY COOLING SYSTEMS
    ASAHI, K
    KITAMURA, M
    IBE, E
    ASAKURA, Y
    UCHIDA, S
    [J]. NUCLEAR SCIENCE AND ENGINEERING, 1987, 95 (04) : 257 - 265
  • [5] DEPOSITION OF CO-60 ON THE STAINLESS-STEEL SURFACE USED FOR THE PRIMARY COOLING SYSTEM OF A BOILING WATER-REACTOR
    UCHIDA, S
    KITAMURA, M
    MATSUSHIMA, Y
    YONEZAWA, K
    OHSUMI, K
    MIKI, M
    [J]. NUCLEAR SCIENCE AND ENGINEERING, 1981, 77 (04) : 496 - 501
  • [6] FATIGUE CRACK GROWTH OF STAINLESS-STEEL PIPING IN A PRESSURIZED WATER-REACTOR ENVIRONMENT
    BAMFORD, WH
    [J]. JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 1979, 101 (01): : 73 - 79
  • [7] DEPOSITION OF RADIOACTIVE IONS ON BOILING WATER-REACTOR COMPONENT MATERIALS
    HONDA, T
    MINATO, A
    OHSUMI, K
    MATSUBAYASHI, H
    [J]. CORROSION, 1987, 43 (03) : 179 - 185
  • [8] APPLICATION OF PREOXIDATION TREATMENT TO SUPPRESS CO-60 DEPOSITION ON STAINLESS-STEEL SURFACES OF BOILING WATER-REACTOR PRIMARY COOLING SYSTEMS
    KITAMURA, M
    IBE, E
    UCHIDA, S
    HONDA, T
    ROMEO, G
    COWAN, RL
    [J]. NUCLEAR SCIENCE AND ENGINEERING, 1985, 89 (01) : 61 - 69
  • [9] THE BENEFIT OF HYDROGEN ADDITION TO THE BOILING WATER-REACTOR ENVIRONMENT ON STRESS-CORROSION CRACK INITIATION AND GROWTH IN TYPE-304 STAINLESS-STEEL
    JEWETT, CW
    PICKETT, AE
    [J]. JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1986, 108 (01): : 10 - 19
  • [10] STATISTICAL PATTERNS OF FUEL FAILURE IN STAINLESS-STEEL CLAD LIGHT WATER-REACTOR FUEL-RODS
    WAS, GS
    CHRISTENSEN, R
    PARK, C
    SMITH, RW
    [J]. NUCLEAR TECHNOLOGY, 1985, 71 (02) : 445 - 457