PROTECTIVENESS OF A CVD-AL2O3 FILM ON TIAL INTERMETALLIC COMPOUND AGAINST HIGH-TEMPERATURE OXIDATION

被引:52
|
作者
TANIGUCHI, S
SHIBATA, T
TAKEUCHI, K
机构
[1] Osaka Univ, Suita
来源
MATERIALS TRANSACTIONS JIM | 1991年 / 32卷 / 03期
关键词
CVD-AL2O3; TIAL; OXIDATION RESISTANCE; HIGH TEMPERATURE; PROTECTIVENESS;
D O I
10.2320/matertrans1989.32.299
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TiAl coupon specimens coated with Al2O3 films by a CVD technique were oxidized in a flow of purified oxygen at atmospheric pressure for 100 ks at 1073, 1173 and 1273 K. The mass gains due to the oxidation were negligible. The CVD Al2O3 films of about 3-mu-m thickness were protective and very adherent to the substrate even after the oxidation at all the temperatures tested except 1273 K. Irregularly shaped Al2O3 crystals grew on the specimen at 1273 K even though they were very small, showing a limited protection at this temperature.
引用
收藏
页码:299 / 301
页数:3
相关论文
共 50 条
  • [1] Protectiveness of CVD Al2O3 films against high-temperature oxidation
    Taniguchi, Shigeji
    Shibata, Toshio
    Horikawa, Yoshihiko
    Boshoku gijutsu, 1988, 37 (12): : 745 - 750
  • [2] PROTECTIVENESS OF CVD AL2O3 FILMS ON TIN AGAINST HIGH-TEMPERATURE OXIDATION
    TANIGUCHI, S
    SHIBATA, T
    OKADA, A
    MATERIALS TRANSACTIONS JIM, 1990, 31 (05): : 396 - 403
  • [3] MICROSTRUCTURE OF CVD-AL2O3
    CHATFIELD, C
    LINDSTROM, JN
    SJOSTRAND, ME
    JOURNAL DE PHYSIQUE, 1989, 50 (C-5): : 377 - 387
  • [4] HIGH-TEMPERATURE OXIDATION OF 2-PHASE (TI3AL + TIAL) INTERMETALLIC COMPOUNDS
    TAKASAKI, A
    OJIMA, K
    TANEDA, Y
    HOSHIYA, T
    MITSUHASHI, A
    SCRIPTA METALLURGICA ET MATERIALIA, 1992, 27 (04): : 401 - 405
  • [5] High temperature oxidation behaviour of a TiAl-Al2O3 intermetallic matrix composite
    Li, ZW
    Gao, W
    Zhang, DL
    Cai, ZH
    CORROSION SCIENCE, 2004, 46 (08) : 1997 - 2007
  • [6] High-Temperature Oxidation and Wear Behavior of (Fe,Cr)Al Intermetallic Compound and (Fe,Cr)Al-Al2O3 Nanocomposites
    Sourani, F.
    Enayati, M. H.
    Taghipour, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (05) : 3654 - 3669
  • [7] High-Temperature Oxidation and Wear Behavior of (Fe,Cr)Al Intermetallic Compound and (Fe,Cr)Al-Al2O3 Nanocomposites
    F. Sourani
    M. H. Enayati
    M. Taghipour
    Journal of Materials Engineering and Performance, 2021, 30 : 3654 - 3669
  • [8] SELF-PROPAGATING HIGH-TEMPERATURE SYNTHESIS OF TIAL-SIC AND TIAL-AL2O3 INTERMETALLIC COMPOSITES
    WRZESINSKI, WR
    RAWERS, JC
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1990, 9 (04) : 432 - 435
  • [9] High-temperature oxidation behavior of Al2O3/TiAl matrix composite in air
    TaoTao Ai
    Fen Wang
    XiaoMing Feng
    Science in China Series E: Technological Sciences, 2009, 52 : 1273 - 1282
  • [10] High-temperature oxidation behavior of Al2O3/TiAl matrix composite in air
    Ai TaoTao
    Wang Fen
    Feng XiaoMing
    SCIENCE IN CHINA SERIES E-TECHNOLOGICAL SCIENCES, 2009, 52 (05): : 1273 - 1282