摘要
The growth of (100) diamond/iron/copper multilayer structures has been examined by reflection high energy electron diffraction, extended X-ray absorption fine structure, and scanning electron microscopy in an effort to determine the thickness limit for metastable face-centered-cubic Fe on (100) diamond. Both copper films deposited on iron layers with thicknesses below 1.4 nm and the iron layers themselves were found to be face-centered cubic single crystal, while films grown on iron that was 2.0 nm and thicker and the iron itself were found to be polycrystalline. This critical thickness range of 1.4-2.0 nm compares well with the theoretically calculated value of 1.8 nm. This value was determined using the mechanical equilibrium theories (Matthews-Blakeslee and van der Merwe) with a lattice parameter for face-centered cubic iron that was derived by estimating the functional form of the linear thermal expansion coefficient and extrapolating the Poisson's ratio for austenitic stainless steel to the temperature of interest. The shear modulus, and intrinsic stacking fault energy for fcc Fe from similar to 1350 degrees C down to below room temperature have also been estimated. A more likely room temperature lattice parameter for fcc Fe than is usually assumed was estimated to be 0.3579 nm. The measured in-plane lattice parameter of strained fcc Fe on diamond was 3.54 +/- 0.1 Angstrom.
引用
收藏
页码:252 / 266
页数:15
相关论文
共 50 条
  • [1] DETERMINATION OF CRITICAL THICKNESS OF SINGLE-CRYSTAL (001)-FILMS OF NICKEL
    PYNKO, VG
    KAN, SV
    DYMPILOV, RM
    [J]. FIZIKA TVERDOGO TELA, 1973, 15 (10): : 3100 - 3100
  • [2] Porous single-crystal diamond
    Wang, Junpu
    Su, Yuzhu
    Tian, Yi
    Xiang, Xiaojun
    Zhang, Jiawei
    Li, Shuaiqi
    He, Duanwei
    [J]. CARBON, 2021, 183 : 259 - 266
  • [3] Constitutive model for an FCC single-crystal material
    Ding Z.-P.
    Liu Y.-L.
    Yin Z.-Y.
    Yang Z.-G.
    Cheng X.-M.
    [J]. Frontiers of Mechanical Engineering in China, 2006, 1 (1): : 40 - 47
  • [4] Catalytic graphitization of single-crystal diamond
    Tulić, Semir
    Waitz, Thomas
    Čaplovičová, Mária
    Habler, Gerlinde
    Vretenár, Viliam
    Susi, Toma
    Skákalová, Viera
    [J]. Skákalová, Viera (viera.skakalova@univie.ac.at), 1600, Elsevier Ltd (185): : 300 - 313
  • [5] FABRICATION OF SINGLE-CRYSTAL DIAMOND MICROCOMPONENTS
    HUNN, JD
    WITHROW, SP
    WHITE, CW
    CLAUSING, RE
    HEATHERLY, L
    CHRISTENSEN, CP
    [J]. APPLIED PHYSICS LETTERS, 1994, 65 (24) : 3072 - 3074
  • [6] Catalytic graphitization of single-crystal diamond
    Tulic, Semir
    Waitz, Thomas
    Caplovicova, Maria
    Habler, Gerlinde
    Vretenar, Viliam
    Susi, Toma
    Skakalova, Viera
    [J]. CARBON, 2021, 185 : 300 - 313
  • [7] RAPID GROWTH OF SINGLE-CRYSTAL DIAMOND ON DIAMOND SUBSTRATES
    JANSSEN, G
    VOLLENBERG, W
    GILING, LJ
    VANENCKEVORT, WJP
    SCHAMINEE, JJD
    SEAL, M
    [J]. SURFACE & COATINGS TECHNOLOGY, 1991, 47 (1-3): : 113 - 126
  • [8] THICKNESS MEASURES OF SINGLE-CRYSTAL SILICON
    OKSANICH, AP
    BABADZHANOV, LS
    [J]. MEASUREMENT TECHNIQUES, 1978, 21 (08) : 1098 - 1099
  • [9] COMPARISON OF VARIOUS ANISOTROPIC CRITERIA FOR FCC SINGLE-CRYSTAL
    NOUAILHAS, D
    CAILLETAUD, G
    [J]. COMPTES RENDUS DE L ACADEMIE DES SCIENCES SERIE II, 1992, 315 (13): : 1573 - 1579
  • [10] ANALYSIS OF DYNAMIC SHEAR BANDS IN AN FCC SINGLE-CRYSTAL
    ZHU, ZG
    BATRA, RC
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 1993, 9 (06) : 653 - 696