摘要
A powder metallurgy-based rapid consolidation technique, Plasma Pressure Compaction ((PC)-C-2 (R)), was utilized to produce near-net shape parts of gamma titanium aluminides (gamma-TiAl). Micron-sized gamma-TiAl powders, composed of Ti-50% Al and Ti-48% Al-2% Cr-2% Nb (at%), were rapidly consolidated to form near-net shape gamma-TiAl parts in the form of 1.0" (25.4 mm) diameter discs, as well as 3" x2.25" (76.2 mm x 57.2 mm) tiles, having a thickness of 0.25" (6.35 mm). The gamma-TiAl parts were consolidated to near theoretical density. The microstructural morphology of the consolidated parts was found to vary with consolidation conditions. Mechanical properties exhibited a strong dependence on microstructural morphology and grain size. Because of the rapid consolidation process used here, grain growth during consolidation was minimal, which in turn led to enhanced mechanical properties. Consolidated.-TiAl samples corresponding to Ti-48% Al-2% Cr-2% Nb composition with a duplex microstructure (with an average grain size of 5 mu m) exhibited superior mechanical properties. Flexural strength, ductility, elastic modulus and fracture toughness for these samples were as high as 1238 MPa, 2.3%, 154.58 GPa and 17.95 MPa m 1/2, respectively. The high temperature mechanical properties of the consolidated gamma-TiAl samples were characterized in air and vacuum and were found to retain flexural strength and elastic modulus for temperatures up to 700 degrees C. At high temperatures, the flexural strength of gamma-TiAl samples with Ti-50% Al composition deteriorated in air by 10% as compared to that in vacuum. gamma-TiAl samples with Ti-48% Al-2% Nb-2% Cr composition exhibited better if not equal flexural strength in air than in vacuum at high temperatures.
引用
收藏
页码:51 / 74
页数:24
相关论文
共 50 条
  • [1] TEM INVESTIGATION OF RAPIDLY QUENCHED METASTABLE GAMMA-TIAL PHASES
    SHAO, G
    GROSDIDIER, T
    TSAKIROPOULOS, P
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C7): : 465 - 468
  • [2] Electron microscopic characterization of a gamma-TiAl alloy
    Suryanarayana, C
    MATERIALS LETTERS, 1996, 29 (4-6) : 281 - 284
  • [3] Characterization of gamma-TiAl castings for engine blade components
    Nishikiori, S
    Yunoki, N
    Miyazawa, H
    Hosoyo, M
    GAMMA TITANIUM ALUMINIDES 2003, 2003, : 417 - 424
  • [4] HOT ISOSTATIC PRESSING OF GAMMA-TIAL ALLOYS AND GAMMA-TIAL METAL MATRIX COMPOSITES
    SHONG, DS
    KIM, YW
    YOLTON, CF
    FROES, FH
    1989 ADVANCES IN POWDER METALLURGY, VOLS 1-3, 1989, 1-3 : C359 - C371
  • [5] Energetics of point defects in gamma-TiAl
    Raju, S
    Mohandas, E
    Raghunathan, VS
    SCRIPTA MATERIALIA, 1996, 34 (04) : 585 - 593
  • [6] Synthesis of gamma-TiAl by Thermal Explosion
    Lagos, M. A.
    Agote, I.
    Gutierrez, M.
    Sargsyan, A.
    Pambaguian, L.
    INTERNATIONAL JOURNAL OF SELF-PROPAGATING HIGH-TEMPERATURE SYNTHESIS, 2010, 19 (01) : 23 - 27
  • [7] THE EFFECT OF NITROGEN ON THE OXIDATION OF GAMMA-TIAL
    RAKOWSKI, JM
    PETTIT, FS
    MEIER, GH
    DETTENWANGER, F
    SCHUMANN, E
    RUHLE, M
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 33 (06): : 997 - 1003
  • [8] INTERACTION OF TANTALUM WITH REINFORCEMENTS IN GAMMA-TIAL
    NEWKIRK, J
    DIXON, D
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 153 (1-2): : 662 - 667
  • [9] CARBIDE PRECIPITATION IN GAMMA-TIAL ALLOYS
    CHEN, S
    BEAVEN, PA
    WAGNER, R
    SCRIPTA METALLURGICA ET MATERIALIA, 1992, 26 (08): : 1205 - 1210
  • [10] Influence of moisture on the oxidation of gamma-TiAl
    Kremer, R
    Auer, W
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1997, 48 (01): : 35 - 39