Failure Analysis of Nitrile Rubber O-Rings Static Sealing for Packaging Barrel

被引:5
|
作者
Wei X.-Q. [1 ]
Wu H.-L. [1 ]
Zhang L.-W. [1 ]
Zhang S.-Y. [1 ]
Xiao Y. [1 ]
Luo T.-Y. [1 ]
机构
[1] Chongqing Engineering Research Center for Environmental Corrosion and Protection, Southwest Technology and Engineering Research Institute, Chongqing
关键词
Characterization; Compression; Failure analysis; Failure mechanism; Microstructure; Oxidation;
D O I
10.1007/s11668-018-0451-3
中图分类号
学科分类号
摘要
Nitrile rubber O-rings seals for packaging barrel was stored in China tropical marine atmosphere environments for 10 years, and then the sealing function of nitrile rubber O-ring was failed. By comparing the molecular structure, cross-link density, thermal decomposition, content of elements and chemical functional groups of the original nitrile rubber seals, the surface and interior of nitrile rubber seals storage for 10 years, a long-term natural failure mechanism was studied. The results showed that: the surface content of dibutyl phthalate and dibutyl sebacate, the surface carbonyl peak height and the surface content of oxygen element were higher than that in internal; the surface cross-link density was lower than that in internal but still higher than in original sample; and surface carbon- to-oxygen ratio were lower than that in internal and original sample. After aging for 10 years, the weight loss of plasticizer decreased, and the main chain content increased. It can be inferred that nitrile rubber mainly undergoes oxygen-absorbing cross-linking reaction to form carboxylic acids and esters, which is accompanied by the migration and enrichment of two plasticizers to the surface, causing reductions in elasticity and elasticity. The residual permanent compression set was lower than the design critical value, and the sealing function for the packaging barrel was lost, and a leak occurred. © 2018, ASM International.
引用
收藏
页码:628 / 634
页数:6
相关论文
共 50 条
  • [1] BETTER SEALING WITH RUBBER O-RINGS
    ABRAMOV, EI
    RUSSIAN ENGINEERING JOURNAL, 1973, 53 (08): : 30 - 34
  • [2] A critical examination of the shelf life of nitrile rubber O-Rings used in aerospace sealing applications
    Porter, Christopher
    Zaman, Badruz
    Pazur, Richard
    Polymer Degradation and Stability, 2022, 206
  • [3] A critical examination of the shelf life of nitrile rubber O-Rings used in aerospace sealing applications
    Porter, Christopher
    Zaman, Badruz
    Pazur, Richard
    POLYMER DEGRADATION AND STABILITY, 2022, 206
  • [4] Accelerated thermal ageing studies on nitrile rubber O-rings
    Morrell, PR
    Patel, M
    Skinner, AR
    POLYMER TESTING, 2003, 22 (06) : 651 - 656
  • [5] SEALING ROTARY SHAFTS WITH O-RINGS
    MARTINI, LJ
    MACHINE DESIGN, 1977, 49 (12) : 97 - 99
  • [6] The Effect of Accelerated Aging on the Properties of Nitrile Butadiene Rubber (NBR) O-Rings
    Zhang, Weifang
    Lou, Weitao
    Liu, Xuerong
    Xu, Dan
    Zhang, Jingyu
    JOURNAL OF TESTING AND EVALUATION, 2019, 47 (02) : 1533 - 1550
  • [7] Reliability Analysis of Rubber O-rings Used in the Rockets
    Sun, L.
    Gu, X. H.
    Feng, L.
    Di, Y.
    2016 IEEE INTERNATIONAL CONFERENCE ON INDUSTRIAL ENGINEERING AND ENGINEERING MANAGEMENT (IEEM), 2016, : 1392 - 1396
  • [8] Influence of hydraulic oil on degradation behavior of nitrile rubber O-rings at elevated temperature
    Lou, Weitao
    Zhang, Weifang
    Wang, Hongxun
    Jin, Tingzhu
    Liu, Xuerong
    ENGINEERING FAILURE ANALYSIS, 2018, 92 : 1 - 11
  • [9] Investigation on thermal oxidative aging of nitrile rubber (NBR) O-rings under compression stress
    Liu, X. R.
    Zhang, W. F.
    Lou, W. T.
    Huang, Y. X.
    Dai, W.
    2017 INTERNATIONAL CONFERENCE ON MATERIAL ENGINEERING AND MANUFACTURING (ICMEM 2017), 2017, 265
  • [10] Thermodynamic and Sealing Performance Analysis of Reciprocating O-Rings in Hydraulic Cylinders
    Tao, Nana
    INTERNATIONAL JOURNAL OF HEAT AND TECHNOLOGY, 2023, 41 (03) : 694 - 700