摘要
Laser beam welding of aluminium alloys becomes increasingly important. However, in welding of high-strength aluminium alloys one main problem is hot cracking in the weld metal. Increasing the silicon content in the weld metal by introducing filler wire can reduce the occurrence of hot cracking. Today available filler wires are limited to 12 % Si since materials having higher Si content cannot be processed into wire. Spray forming is capable of producing hypereutectic Al-Si wires with a fine-grained microstructure in comparison with conventional cast alloys. In this investigation, the performance of spray formed AISi18 wire was compared to standard AISi12 wire. In view of process behaviour, no significant effect of the increased silicon content was observed. Furthermore, it was proven that the hot cracking susceptibility was decreased with increasing silicon content.
引用
收藏
页码:3 / 8
页数:5
相关论文
共 50 条
  • [1] Laser welding with filler wire
    Dilthey, U
    Fuest, D
    Scheller, W
    OPTICAL AND QUANTUM ELECTRONICS, 1995, 27 (12) : 1181 - 1191
  • [2] Investigation of filler wire melting and transfer behaviors in laser welding with filler wire
    Huang, Wenhao
    Chen, Shujun
    Xiao, Jun
    Jiang, Xiaoqing
    Jia, Yazhou
    OPTICS AND LASER TECHNOLOGY, 2021, 134
  • [3] Investigation of filler wire melting and transfer behaviors in laser welding with filler wire
    Huang, Wenhao
    Chen, Shujun
    Xiao, Jun
    Jiang, Xiaoqing
    Jia, Yazhou
    Optics and Laser Technology, 2021, 134
  • [4] Filler wire melting dynamics during laser beam welding with filler wire
    Liu, Hongbing
    Tao, Wang
    Chen, Jie
    Yang, Zhibin
    Chen, Lei
    Zhan, Xiaohong
    Li, Liqun
    Hanjie Xuebao/Transactions of the China Welding Institution, 2013, 34 (11): : 73 - 77
  • [5] Reduction of hot cracking susceptibility during laser welding of aluminum by vibrations
    Radel, Tim
    Woizeschke, Peer
    WELDING IN THE WORLD, 2019, 63 (03) : 599 - 606
  • [6] Reduction of hot cracking susceptibility during laser welding of aluminum by vibrations
    Tim Radel
    Peer Woizeschke
    Welding in the World, 2019, 63 : 599 - 606
  • [7] Application of Arc Welding with Hot Filler Wire.
    Ruckdeschel, Walter E.W.
    Zeitschrift fuer Schweisstechnik, Journal de la Soudure, 1973, 63 (08): : 229 - 236
  • [8] Laser welding with filler material in the form of a wire
    Banasik, Marek
    Dworak, Jerzy
    Stano, Sebastian
    Welding International, 2012, 26 (07) : 516 - 520
  • [9] Effect of wire feed position on laser welding with filler wire
    Salminen, AS
    Kujanpää, VP
    JOURNAL OF LASER APPLICATIONS, 2003, 15 (01) : 2 - 10
  • [10] The filler wire - laser beam interaction during laser welding with low alloyed steel filler wire
    Salminen, A.
    MECHANIKA, 2010, (04): : 67 - 74