Development of a New Wrought Magnesium-Aluminum-Manganese Alloy AM30

被引:0
|
作者
Alan A. Luo
Anil K. Sachdev
机构
[1] General Motors Research & Development Center,
关键词
Magnesium Alloy; AZ31 Alloy; Extrusion Speed; AM30 Alloy; AZ31 Sheet;
D O I
暂无
中图分类号
学科分类号
摘要
A new wrought magnesium alloy, AM30 (Mg-3 pct Al-0.4 pct Mn), has been developed. Compared to the current workhorse commercial wrought magnesium alloy AZ31 (Mg-3 pct Al-1 pct Zn), the new AM30 alloy has 20 to 50 pct higher maximum extrusion speed, up to 50 pct ductility improvement at temperatures up to 200 °C, with similar yield and tensile strengths. The tensile behavior of AM30 and AZ31 magnesium alloy tubes suggests a moderate temperature forming range of 100 °C to 175 °C in which strain hardening offsets plastic instability until fracture by cavity coalescence occurs. The AM30 alloy has slightly better formability than AZ31 at room and moderate temperatures, due to higher strain-hardening rates (dσ/dε) and exponents (n). Microstructural evaluation indicates that twinning is the major deformation mechanism for these alloys at room and moderate temperatures in addition to slip mechanisms. Dynamic recrystallization (DRX) is observed at temperatures greater than ∼150 °C, which causes local instabilities to occur, leading to failure.
引用
收藏
页码:1184 / 1192
页数:8
相关论文
共 50 条
  • [1] Development of a new wrought magnesium-aluminum-manganese alloy AM30
    Luo, Alan A.
    Sachdev, Anil K.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (06): : 1184 - 1192
  • [2] Bendability of the wrought magnesium alloy AM30 tubes using a rotary draw bender
    Wu, Wenyun
    Zhang, Ping
    Zeng, Xiaoqin
    Jin, Li
    Yao, Shoushan
    Luo, Alan A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 486 (1-2): : 596 - 601
  • [3] Deformation Behavior of AM30 Magnesium Alloy
    A. Bisht
    V. Yadav
    S. Suwas
    U. S. Dixit
    Journal of Materials Engineering and Performance, 2018, 27 : 4900 - 4910
  • [4] Deformation Behavior of AM30 Magnesium Alloy
    Bisht, A.
    Yadav, V.
    Suwas, S.
    Dixit, U. S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (09) : 4900 - 4910
  • [5] AM30 - A new wought mgnesium alloy
    Luo, Alan A.
    Sachdev, Anil K.
    MAGNESIUM TECHNOLOGY 2007, 2007, : 321 - +
  • [6] Effects of aluminum and copper cover tube casing on the ECAP process of AM30 magnesium alloy
    Jahadi, R.
    Sedighi, M.
    Jahed, H.
    MATERIALS AND MANUFACTURING PROCESSES, 2017, 32 (12) : 1375 - 1383
  • [7] Extrusion welding in a magnesium alloy (AM30) hollow section extrudate
    Alharthi, Nabeel H.
    Misiolek, Wojciech Z.
    1600, ASM International (172): : 16 - 17
  • [8] Cyclic deformation of extruded AM30 magnesium alloy in the transverse direction
    Chen, D. L.
    Emami, A. R.
    Luo, A. A.
    15TH INTERNATIONAL CONFERENCE ON THE STRENGTH OF MATERIALS (ICSMA-15), 2010, 240
  • [9] EQUILIBRIUM RELATIONS IN MAGNESIUM-ALUMINUM-MANGANESE ALLOYS
    NELSON, BJ
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1951, 191 (09): : 797 - 799
  • [10] Numerical modelling of large strain deformation in magnesium alloy AM30
    Levesque, Julie
    Inal, Kaan
    Neale, Kenneth W.
    Mishra, Raja K.
    Luo, Alan A.
    Jiang, Lan