Technological Aspects of Minimization of the Sizes of a Continuous Casting-Rolling Unit in the Production of Wire Rods from Fire-Refined Copper

被引:0
|
作者
E. N. Smirnov
V. A. Skliar
A. S. Gorozhankin
A. N. Smirnov
V. A. Belevitin
G. A. Orlov
机构
[1] Ugarov Staryi Oskol Technological Institute,
[2] Branch of the “MISiS” National Research Technological University,undefined
[3] Physicotechnological Institute of Metals and Alloys,undefined
[4] National Academy of Sciences of Ukraine,undefined
[5] South-Ural State Humanitarian-Pedagogical University,undefined
[6] El’tsyn Ural Federal University,undefined
来源
Metallurgist | 2020年 / 64卷
关键词
copper wire rods; rolling; continuously cast billets in the form of a trapezoid; defects; reduction; elongation; pass overflow; spreading index;
D O I
暂无
中图分类号
学科分类号
摘要
In the production of wire rods made of fire-refined copper by minor and medium regional producers, the problem of minimization of the sizes of technological lines of continuous casting-rolling machines (CCRM) is most often solved by decreasing the number of structural components in the applied technological system, including the decrease in the number of rolling stands in the roll mill train. We estimate the influence of minimization of the number of rolling stands under the conditions of continuous casting-rolling in a 9-stand rolling mill of the Southwire Company on the ease of realization of the process of production and the quality of the products. It is shown that the realization of stable rolling process and the required quality of wire rods becomes possible as a result of decreasing the cross-sectional area of the original continuously cast ingots in the form of a trapezoid by 6.71% and an increase in the area of workpieces in all stands of the mill with an aim to prevent the overflow of the passes with the metal (the so-called “fin” defects), which enables one to get finished product with transformed “lap” defects. It is shown that the section of transition from the rough group of stands to the finishing group, i.e., the 3v stand (round pass), should be regarded as the most problematic from the viewpoint of formation of fin-type defects. We also perform the correction of the shape of plane oval specified for this stand. The practical implementation of the entire proposed complex of technological adjustments makes it possible to stabilize the process of rolling and to obtain copper wire rods 8 mm in diameter with regular geometric shapes and the required quality of macrostructure of the metal in the absence of lap-type defects.
引用
下载
收藏
页码:553 / 565
页数:12
相关论文
共 4 条
  • [1] Technological Aspects of Minimization of the Sizes of a Continuous Casting-Rolling Unit in the Production of Wire Rods from Fire-Refined Copper
    Smirnov, E. N.
    Skliar, V. A.
    Gorozhankin, A. S.
    Smirnov, A. N.
    Belevitin, V. A.
    Orlov, G. A.
    METALLURGIST, 2020, 64 (5-6) : 553 - 565
  • [2] Application of a casting-rolling unit in a combined process of production of high-quality products from copper scrap
    A. N. Smirnov
    I. V. Shutov
    S. V. Kuberskii
    S. M. Volkov
    Russian Metallurgy (Metally), 2012, 2012 (12) : 1027 - 1030
  • [3] Application of a Casting-Rolling Unit in a Combined Process of Production of High-Quality Products from Copper Scrap
    Smirnov, A. N.
    Shutov, I. V.
    Kuberskii, S. V.
    Volkov, S. M.
    RUSSIAN METALLURGY, 2012, (12): : 1027 - 1030
  • [4] Molecular Dynamic Simulation and Microstructure Analysis of Continuous Casting and Rolling CuAg Alloy Contact Wire from Yunnan Copper Industry Co. Ltd
    Zhou Xiaolong
    Hong Zhenjun
    Yang Jianjun
    Li Gang
    Yan Ming
    He Jianhui
    Chen Jingchao
    Wu Yucai
    Yang Yunchuan
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 286 - 289