Determination of optimal EDM machining parameters for machined pure titanium-porcelain adhesion

被引:0
|
作者
Asli Secilmis
A. Murat Olmez
Murat Dilmec
H. Selcuk Halkaci
Ozgur Inan
机构
[1] University of Gaziantep,Faculty of Dentistry, Department of Prosthodontics
[2] Mechanical Engineer,Faculty of Engineering and Architecture, Department of Mechanical Engineering
[3] University of Selcuk,Faculty of Dentistry, Department of Prosthodontics
[4] University of Selcuk,Dişhekimliği Fakültesi
[5] Gaziantep Üniversitesi,undefined
关键词
Titanium; Titanium–porcelain adhesion; Taguchi method; Electrical discharge machining; EDM;
D O I
暂无
中图分类号
学科分类号
摘要
The objective of this experimental study is to determine electrical discharge machining (EDM) parameters that offer the best adhesion at the interface of a machined titanium–porcelain composite. First of all, with Taguchi method, machining parameters that will be effective in the bonding strength as well as their interactions on each other were determined in the test. Then, multiple level experiments were conducted to determine how the effective parameters varied over a wide area. Slopes of the curves obtained in these tests were studied, and then, final tests were conducted to obtain the best bonding strength possible. In this way, machining parameters that would offer the highest bonding strength of the titanium–porcelain matrix in a stepwise adjustable EDM machine were obtained. By taking into consideration the steps on the EDM machine where the tests were conducted, it is seen that, when a full factorial experiment is undertaken, 5 power × 2 polarity × 2 type of dielectric × 2 sandblasting or non-sandblasting × 2 kind of electrode × 10 pulse-on time, it necessitates 800 different tests to be executed, but, with the applied method, 16 + 18 + 3 yields 37 different tests where the results that include all possible alternatives were obtained. As a result, EDM machining parameters that offer the highest adhesion and are relatively higher, 31.5 N/mm2, than the acceptable minimum value of 25 N/mm2 were specified.
引用
收藏
页码:55 / 61
页数:6
相关论文
共 47 条
  • [1] Determination of optimal EDM machining parameters for machined pure titanium-porcelain adhesion
    Secilmis, Asli
    Olmez, A. Murat
    Dilmec, Murat
    Halkaci, H. Selcuk
    Inan, Ozgur
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2009, 45 (1-2): : 55 - 61
  • [2] Gold and titanium nitride coatings on cast and machined commercially pure titanium to improve titanium-porcelain adhesion
    Park, Sangwon
    Kim, Yeonmi
    Lim, Hyunpil
    Oh, Gyejeong
    Kim, Hyunseung
    Ong, Joo L.
    Lee, Kwangmin
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (20-21): : 3243 - 3249
  • [3] Titanium-porcelain system .2. Bond strength of fired porcelain on nitrided pure titanium
    Oshida, Y
    Fung, LW
    Isikbay, SC
    BIO-MEDICAL MATERIALS AND ENGINEERING, 1997, 7 (01) : 13 - 34
  • [4] Effects of sandblasting and electrical discharge machining on porcelain adherence to cast and machined commercially pure titanium
    Inan, Ozgur
    Acar, Asli
    Halkaci, Selcuk
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2006, 78B (02) : 393 - 400
  • [5] Effect of bonding agent on bond strength of pure titanium-porcelain system.
    Hung, CC
    Okazaki, M
    Takahashi, J
    JOURNAL OF DENTAL RESEARCH, 1997, 76 : 374 - 374
  • [6] EFFECT OF GOLD SPUTTERING ON THE ADHESION OF PORCELAIN TO CAST AND MACHINED TITANIUM
    Khung, Rathanak
    Suansuwan, Napa Sukjai
    JOURNAL OF PROSTHETIC DENTISTRY, 2013, 110 (01): : 41 - 46
  • [7] The effect of Goldbonder™ on the adhesion between porcelain and pure titanium
    Yamada, K
    Onizuka, T
    Sumii, T
    Swain, MV
    JOURNAL OF ORAL REHABILITATION, 2004, 31 (08) : 775 - 784
  • [8] Influence of the bonder on the adhesion of porcelain to machined titanium as determined by the strain energy release rate
    Tholey, M. J.
    Waddell, J. N.
    Swain, M. V.
    DENTAL MATERIALS, 2007, 23 (07) : 822 - 828
  • [9] Evaluation of optimal parameters for machining brass with wire cut EDM
    Rao, C. V. S. Parameswara
    Sarcar, M. M. M.
    JOURNAL OF SCIENTIFIC & INDUSTRIAL RESEARCH, 2009, 68 (01): : 32 - 35
  • [10] Influence of chromium interlayer on the adhesion of porcelain to machined titanium as determined by the strain energy release rate
    Elsaka, Shaymaa E.
    Hamouda, Ibrahim M.
    Elewady, Yehia A.
    Abouelatta, Ossama B.
    Swain, Michael V.
    JOURNAL OF DENTISTRY, 2010, 38 (08) : 648 - 654