Experimental strength characterisation of thin chemically pre-stressed glass based on laser-induced flaws

被引:4
|
作者
Nategh, Shahryar [1 ,2 ]
Zaccaria, Marco [3 ]
Missinne, Jeroen [2 ]
Belis, Jan [1 ]
机构
[1] Univ Ghent, Magnel Vandepitte Lab, Dept Struct Engn & Bldg Mat, Technol Pk 60, B-9052 Ghent, Belgium
[2] Univ Ghent, ELIS, CMST, IMEC, Technol Pk 126, B-9052 Ghent, Belgium
[3] AGC Glass Europe, Ottignies, Belgium
关键词
Chemically strengthened glass; Thin glass; Surface flaw; Laser ablation; Bending strength; ION-EXCHANGE; STRESS BUILDUP; STATE;
D O I
10.1007/s40940-022-00205-w
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The strength of chemically pre-stressed glass depends on the depth of surface flaws and the value of the pre-stress. So far, some research has been conducted on this topic; however, there were always uncertainties regarding the flaw depth and the pre-stress profile. Consequently, this research characterises the pre-stress profile using experimental methods. The latter include measuring the depth of layer (DoL) and the surface compressive pre-stress (C-S) with FSM-7000 h and verifying the achieved DoL with the Na+ and K+ distribution through the thickness obtained from the SEM/EDS analysis. Results demonstrate that the amount of K decreases parabolically (second-order) to a certain value and then remains constant. Based on this observation and some boundary conditions, the equation of the pre-stress profile was obtained for thin chemically pre-stressed aluminosilicate glass (Falcon (R)) with 8 h and 24 h processing durations in molten salt at 460 degrees C. A non-strengthened glass (NSG) was also used as a reference for comparison. Then, three artificial laser-induced flaws with accurately controlled depths is tested by means of a clamp bender. The results of the strength tests demonstrated very low deviations in the failure stress. It was shown that even when the depth of the flaw is higher than the DoL, which means that the flaw tip enters the zone with the pre-tensile stress, there is still considerable resistance from the surrounding intact area. Furthermore, it was confirmed that the pre-stress strain energy for 24 h processing is larger than for 8 h, leading to more fragmentation after failure under a similar loading condition. Finally, it was found that the fracture toughness is not constant through the pre-stressed glass thickness, and it is dependent on the pre-stress profile with the peak value at the glass surface.
引用
收藏
页码:471 / 486
页数:16
相关论文
共 50 条
  • [1] Experimental strength characterisation of thin chemically pre-stressed glass based on laser-induced flaws ( vol 7 , pg 471 , 2022)
    Nategh, Shahryar
    Zaccaria, Marco
    Missinne, Jeroen
    Belis, Jan
    GLASS STRUCTURES & ENGINEERING, 2024, 9 (3-4) : 729 - 729
  • [2] Effect of ultrashort laser-induced surface flaws on architectural glass strength
    Nategh, Shahryar
    Missinne, Jeroen
    Vijverman, Pieter
    Van Steenberge, Geert
    Belis, Jan
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 295
  • [3] A novel experimental method to characterise the shear strength of concrete based on pre-stressed samples
    Forquin, Pascal
    Abdul-Rahman, Reem
    Saletti, Dominique
    STRAIN, 2022, 58 (02)
  • [4] Molecular simulations of the strength enhancement of pre-stressed silica glass upon exposure to moisture
    Garofalini, Stephen H.
    JOURNAL OF NON-CRYSTALLINE SOLIDS-X, 2023, 18
  • [5] Laser bending of pre-stressed thin-walled nickel micro-tubes
    Jamil, M. S. Che
    Fauzi, E. R. Imam
    Juinn, C. S.
    Sheikh, M. A.
    OPTICS AND LASER TECHNOLOGY, 2015, 73 : 105 - 117
  • [6] Experimental investigation and Mohr-Coulomb plasticity modeling of glass fragments from pre-stressed glass panes
    Pauli, Alexander
    Kraus, Michael A.
    Siebert, Geralt
    ce/papers, 2021, 4 (06) : 107 - 121
  • [7] A novel experimental method to characterise the shear strength of concrete based on pre-stressed samples. A comparison with existing techniques
    Forquin, Pascal
    Abdul-Rahman, Reem
    Saletti, Dominique
    12TH INTERNATIONAL CONFERENCE ON THE MECHANICAL AND PHYSICAL BEHAVIOUR OF MATERIALS UNDER DYNAMIC LOADING (DYMAT 2018), 2018, 183
  • [8] Potential Induced Degradation of Pre-Stressed Photovoltaic Modules: Effect of Glass Surface Conductivity Disruption
    Tatapudi, S.
    Ebneali, F.
    Kuitche, J.
    TamizhMani, G.
    2013 IEEE 39TH PHOTOVOLTAIC SPECIALISTS CONFERENCE (PVSC), 2013, : 1604 - 1609
  • [9] Nominal Flexural Strength of Thin-walled Steel Girders with Deviators Pre-stressed by Rectilinear Cables
    Mehdi, Agha Intizar
    Kim, Moon-Young
    INTERNATIONAL JOURNAL OF STEEL STRUCTURES, 2025, 25 (01) : 22 - 43
  • [10] EXPERIMENTAL AND NUMERICAL STUDY OF LASER-INDUCED SPALLATION IN GLASS
    DERESSEGUIER, T
    COTTET, F
    JOURNAL OF APPLIED PHYSICS, 1995, 77 (08) : 3756 - 3761