Influence of matrix characteristics on fracture toughness of high volume fraction Al2O3/Al–AlN composites

被引:0
|
作者
N. Nagendra
V. Jayaram
机构
[1] Indian Institute of Science,Department of Metallurgy
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The role of matrix microstructure on the fracture of Al-alloy composites with 60 vol% alumina particulates was studied. The matrix composition and microstructure were systematically varied by changing the infiltration temperature and heat treatment. Characterization was carried out by a combination of metallography, hardness measurements, and fracture studies conducted on compact tension specimens to study the fracture toughness and crack growth in the composites. The composites showed a rise in crack resistance with crack extension (R curves) due to bridges of intact matrix ligaments formed in the crack wake. The steady-state or plateau toughness reached upon stable crack growth was observed to be more sensitive to the process temperature rather than to the heat treatment. Fracture in the composites was predominantly by particle fracture, extensive deformation, and void nucleation in the matrix. Void nucleation occurred in the matrix in the as-solutionized and peak-aged conditions and preferentially near the interface in the underaged and overaged conditions. Micromechanical models based on crack bridging by intact ductile ligaments were modified by a plastic constraint factor from estimates of the plastic zone formed under indentations, and are shown to be adequate in predicting the steady-state toughness of the composite.
引用
收藏
页码:1145 / 1153
页数:8
相关论文
共 50 条
  • [1] Influence of matrix characteristics on fracture toughness of high volume fraction Al2O3/Al-AlN composites
    Nagendra, N
    Jayaram, V
    JOURNAL OF MATERIALS RESEARCH, 2000, 15 (05) : 1145 - 1153
  • [2] Fracture and R-curves in high volume fraction Al2O3/Al composites
    N. Nagendra
    V. Jayaram
    Journal of Materials Research, 2000, 15 : 1131 - 1144
  • [3] Fracture and R-curves in high volume fraction Al2O3/Al composites
    Nagendra, N
    Jayaram, V
    JOURNAL OF MATERIALS RESEARCH, 2000, 15 (05) : 1131 - 1144
  • [4] Drilling of High Volume Fraction Al2O3 Metal Matrix Composites
    Bachchhav, B. D.
    Salunkhe, Sachin
    Naranje, Vishal
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2021, 10 (01) : 317 - 327
  • [5] Influence of volume fraction of Al2O3 particles on fracture of the Cu-Al2O3 system
    Besterci, M
    Ivan, J
    Kovác, L
    KOVOVE MATERIALY-METALLIC MATERIALS, 2000, 38 (01): : 21 - 28
  • [6] Analysis of fracture toughness and TiC/Al2O3 composites
    Kamiya, F
    Toda, H
    Kobayashi, T
    Takasu, M
    Okamoto, N
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2001, 65 (04) : 323 - 330
  • [7] Influence of Al2O3 particles volume fraction on fracture mechanism in the Cu-Al2O3 system
    Besterci, M
    Ivan, J
    Kovac, L
    MATERIALS LETTERS, 2000, 46 (2-3) : 181 - 184
  • [8] THE FRACTURE CHARACTERISTICS OF δ-Al2O3/AlALLOY COMPOSITES
    G.Z. Kang
    Q. Gao
    C. Yang and J.X. Zhang (Department of Applied Mechanics and Engineering
    ActaMetallurgicaSinica(EnglishLetters), 1999, (06) : 0 - 0
  • [9] Fracture toughness and surface morphology of Al2O3/Pt composites
    Lee, Dong-Jin
    Choi, Heung-Soap
    Jin, Fan-Long
    Park, Soo-Jin
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2015, 25 : 5 - 8
  • [10] Microstructural evolution and fracture toughness of Al2O3/Ti composites
    Vazquez-Villar, M.
    Romero-Romo, M.
    Altamirano-Torres, A.
    Rocha-Rangel, E.
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2008, 9 (03): : 330 - 333