A leaching process was established based on the ability of platinum-group metals to form stable chloro-complexes in acidic chloride solutions. Industrial catalyst losses were examined for the recovery of platinum, palladium, and rhodium by leaching with a mixture of sulfuric acid and sodium chloride to avoid using aqua regia or autoclave conditions. Extraction of platinum and rhodium in 60% H2SO4 at 135°C steadily increased with increasing NaCl concentrations reaching 95% and 85%, respectively, at 0.1 M NaCl after two hours. By comparison, palladium was dissolved more quickly but also reached 85% under the same conditions. Extraction of each metal increased with temperatures up to 125°C but plateaued at higher temperatures. Similar behavior was observed with increasing H2SO4 concentrations up to 60%. More than 99% extraction of each metal was obtained after ten hours using 0.1 M NaCl and 60% H2SO4 at 125°C.
引用
收藏
页码:37 / 40
页数:3
相关论文
共 50 条