Highly improved electrochemical performances of the nanocrystalline and amorphous Mg2Ni-type alloys by substituting Ni with M (M = Cu, Co, Mn)

被引:0
|
作者
Yanghuan Zhang
Zeming Yuan
Tai Yang
Tinging Zhai
Zhuocheng Liu
Shihai Guo
机构
[1] Inner Mongolia University of Science and Technology,Key Laboratory of Integrated Exploitation of Baiyun Obo Multi
[2] Central Iron and Steel Research Institute,Metal Resources
关键词
Mg; Ni-type alloy; element substitution; melt spinning; nanocrystalline and amorphous; electrochemical performances;
D O I
暂无
中图分类号
学科分类号
摘要
The element Ni in the Mg2Ni alloy is partially substituted by M (M = Cu, Co, Mn) in order to ameliorate the electrochemical hydrogen storage performances of Mg2Ni-type electrode alloys. The nanocrystalline and amorphous Mg20Ni10-xMx (M = None, Cu, Co, Mn; x = 0-4) alloys were prepared by melt spinning. The effects of the M (M = Cu, Co, Mn) content on the structures and electrochemical hydrogen storage characteristics of the as-cast and spun alloys were comparatively studied. The analyses by XRD, SEM and HRTEM reveal that all the as-cast alloys have a major phase of Mg2Ni but the M (M = Co, Mn) substitution brings on the formation of some secondary phases, MgCo2 and Mg for the (M = Co) alloy, and MnNi and Mg for the (M = Mn) alloy. Besides, the as-spun (M = None, Cu) alloys display an entirely nanocrystalline structure, whereas the as-spun (M = Co, Mn) alloys hold a nanocrystalline/amorphous structure, suggesting that the substitution of M (M = Co, Mn) for Ni facilitates the glass formation in the Mg2Ni-type alloys. The electrochemical measurements indicate that the variation of M (M = Cu, Co, Mn) content engenders an obvious effect on the electrochemical performances of the as-cast and spun alloys. To be specific, the cyclic stabilities of the alloys augment monotonously with increasing M (M = Cu, Co, Mn) content, and the capacity retaining rate (S20) is in an order of (M = Cu) > (M = Co) > (M = Mn) > (M = None) for x≤1 but changes to (M = Co) > (M = Mn) > (M = Cu) > (M = None) for x≥2. The discharge capacities of the as-cast and spun alloys always grow with the rising of M (M = Co, Mn) content but first mount up and then go down with increasing M (M = Cu) content. Whatever the M content is, the discharge capacities are in sequence: (M = Co) > (M = Mn) > (M = Cu) > (M = None). The high rate discharge abilities (HRDs) of all the alloys grow clearly with rising M (M = Cu, Co) content except for (M = Mn) alloy, whose HRD has a maximum value with varying M (M = Mn) content. Furthermore, for the as-cast alloys, the HRD is in order of (M = Co) > (M = Mn) > (M = Cu) > (M = None), while for the as-spun (20 m·s-1) alloys, it changes from (M = Co) > (M = Mn) > (M = Cu) > (M = None) for x = 1 to (M = Cu) > (M = Co) > (M = None) > (M = Mn) for x = 4.
引用
收藏
页码:685 / 694
页数:9
相关论文
共 50 条
  • [1] Highly Improved Electrochemical Performances of the Nanocrystalline and Amorphous Mg2Ni-type Alloys by Substituting Ni with M (M=Cu,Co,Mn)
    张羊换
    YUAN Zeming
    YANG Tai
    ZHAI Tinging
    LIU Zhuocheng
    GUO Shihai
    [J]. Journal of Wuhan University of Technology(Materials Science), 2017, 32 (03) : 685 - 694
  • [2] Highly Improved Electrochemical Performances of the Nanocrystalline and Amorphous Mg2Ni-type Alloys by Substituting Ni with M (M = Cu, Co, Mn)
    Zhang Yanghuan
    Yuan Zeming
    Yang Tai
    Zhai Tinging
    Liu Zhuocheng
    Guo Shihai
    [J]. JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2017, 32 (03): : 685 - 694
  • [3] Improved physical and electrochemical hydrogen storage kinetics of the as-spun Mg2Ni-type alloys by substituting Ni with M (M=Co, Cu)
    Zhang, Yang-huan
    Li, Bao-wei
    Ren, Hui-ping
    Pang, Zai-guang
    Hou, Zhong-hui
    Zhao, Dong-liang
    [J]. FRONTIERS OF ADVANCED MATERIALS AND ENGINEERING TECHNOLOGY, PTS 1-3, 2012, 430-432 : 423 - +
  • [4] Enhanced electrochemical hydrogen storage characteristics of the as-spun Mg2Ni-type alloys by substituting Ni with M (M=Cu, Co)
    Zhang, Yang-huan
    Li, Bao-wei
    Ren, Hui-ping
    Pang, Zai-guang
    Hou, Zhong-hui
    Zhao, Dong-liang
    [J]. ADVANCED MATERIALS AND ENGINEERING MATERIALS, PTS 1 AND 2, 2012, 457-458 : 572 - +
  • [5] Electrochemical hydrogen storage performances of the nanocrystalline and amorphous Mg2Ni-type alloys
    Zhang, Yang-huan
    Xu, Chao
    Yang, Tai
    Hou, Zhong-hui
    Zhang, Guo-fang
    Zhao, Dong-liang
    [J]. ADVANCED MATERIALS AND PROCESSES II, PTS 1-3, 2012, 557-559 : 1169 - +
  • [6] Impact of substitution of M (M=Mn, Cu) for Ni on hydriding and dehydriding kinetics of as-spun nanocrystalline and amorphous Mg2Ni-type alloys
    Zhang, Yanghuan
    Ren, Huiping
    Li, Baowei
    Hou, Zhonghui
    Zhang, Guofang
    Zhao, Dongliang
    [J]. PROGRESS IN RENEWABLE AND SUSTAINABLE ENERGY, PTS 1 AND 2, 2013, 608-609 : 1347 - +
  • [7] Influence of substituting Ni with Co on hydriding and dehydriding kinetics of melt spun nanocrystalline and amorphous Mg2Ni-type alloys
    张羊换
    赵栋梁
    李保卫
    马志鸿
    郭世海
    王新林
    [J]. Journal of Central South University, 2011, 18 (02) : 303 - 309
  • [8] Impacts of melt spinning and Mn replacement on electrochemical hydrogen storage performances of nanocrystalline and amorphous Mg2Ni-type alloys
    Zhang, Yang-huan
    Cai, Ying
    Yang, Tai
    Hou, Zhong-hui
    Zhang, Guo-fang
    Zhao, Dong-liang
    [J]. NEW TRENDS IN MECHANICAL ENGINEERING AND MATERIALS, 2013, 251 : 323 - +
  • [9] Influence of substituting Ni with Co on hydriding and dehydriding kinetics of melt spun nanocrystalline and amorphous Mg2Ni-type alloys
    Yang-huan Zhang
    Dong-liang Zhao
    Bao-wei Li
    Zhi-hong Ma
    Shi-hai Guo
    Xin-lin Wang
    [J]. Journal of Central South University, 2011, 18 : 303 - 309
  • [10] Influence of substituting Ni with Co on hydriding and dehydriding kinetics of melt spun nanocrystalline and amorphous Mg2Ni-type alloys
    Zhang Yang-huan
    Zhao Dong-liang
    Li Bao-wei
    Ma Zhi-hong
    Guo Shi-hai
    Wang Xin-lin
    [J]. JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY, 2011, 18 (02): : 303 - 309