Aging Precipitation Behavior of 18Cr-16Mn-2Mo-1. 1N High Nitrogen Austenitic Stainless Steel and Its Influences on Mechanical Properties

被引:0
|
作者
Hua-bing Li
Zhou-hua Jiang
Hao Feng
Qi-feng Ma
Dong-ping Zhan
机构
[1] Northeastern University,School of Materials and Metallurgy
关键词
solution-treated condition; aging precipitation behavior; time-temperature-precipitation curve; high nitrogen austenitic stainless steel; mechanical property;
D O I
暂无
中图分类号
学科分类号
摘要
The solution-treated (ST) condition and aging precipitation behavior of 18Cr-16Mn-2Mo-1. 1N high nitrogen austenitic stainless steel (HNS) were investigated by optical microscope (OM), scanning electron microscope (SEM), and transmission electron microscope (TEM). The results show that the ST condition of 18Cr-16Mn-2Mo-1. 1N HNS with wN above 1% is identified as 1 100 °C for 90 min, followed by water quenching to make sure the secondary phases completely dissolve into austenitic matrix and prevent the grains coarsening too much. Initial time-temperature-precipitation (TTP) curve of aged 18Cr-16Mn-2Mo-1. 1N HNS which starts with precipitation of 0.05% in volume fraction is defined and the “nose” temperature of precipitation is found to be 850 °C with an incubation period of 1 min. Hexagonal intergranular and cellular Cr2N with a = 0.478 nm and c = 0.444 nm precipitates gradually increase in the isothermal aging treatment. The matrix nitrogen depletion due to the intergranular and a few cellular Cr2N precipitates induces the decay of Vickers hardness, and the increment of cellular Cr2N causes the increase in the values. Impact toughness presents a monotonie decrease and SEM morphologies show the leading brittle intergranular fracture. The ultimate tensile strength (UTS), yield strength (YS) and elongation (El) deteriorate obviously. Stress concentration occurs when the matrix dislocations pile up at the interfaces of precipitation and matrix, and the interfacial dislocations may become precursors to the misfit dislocations, which can form small cleavage facets and accelerate the formation of cracks.
引用
收藏
页码:43 / 51
页数:8
相关论文
共 50 条
  • [1] Aging Precipitation Behavior of 18Cr-16Mn-2Mo-1. 1N High Nitrogen Austenitic Stainless Steel and Its Influences on Mechanical Properties
    Li Hua-bing
    Jiang Zhou-hua
    Feng Hao
    Ma Qi-feng
    Zhan Dong-ping
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2012, 19 (08) : 43 - 51
  • [3] Aging precipitation behavior and its influence on mechanical properties of Mn18Cr18N austenitic stainless steel
    Qin, Fengming
    Li, Yajie
    He, Wenwu
    Zhao, Xiaodong
    Chen, Huiqin
    METALS AND MATERIALS INTERNATIONAL, 2017, 23 (06) : 1087 - 1096
  • [4] Aging precipitation behavior and its influence on mechanical properties of Mn18Cr18N austenitic stainless steel
    Fengming Qin
    Yajie Li
    Wenwu He
    Xiaodong Zhao
    Huiqin Chen
    Metals and Materials International, 2017, 23 : 1087 - 1096
  • [5] Effect of Nitrogen Content on Precipitation Behavior and Mechanical Properties of Mn18Cr18N Austenitic Stainless Steel
    Qin Fengming
    Li Yajie
    Zhao Xiaodong
    He Wenwu
    Chen Huiqin
    ACTA METALLURGICA SINICA, 2018, 54 (01) : 55 - 64
  • [6] Precipitation of σ-phase in high-nitrogen austenitic 18Cr-18Mn-2Mo-0.9N stainless steel during isothermal aging
    Lee, TH
    Oh, CS
    Lee, CG
    Kim, SJ
    Takaki, S
    SCRIPTA MATERIALIA, 2004, 50 (10) : 1325 - 1328
  • [7] Effects of aging precipitates on the mechanical and corrosion resistance properties of 18Cr-18Mn-2Mo-0.96N super high nitrogen austenitic stainless steel
    Zhang, Zurui
    Zhao, Zhenye
    Li, Chunzhi
    Jiang, Zhouhua
    Li, Huabing
    ADVANCED MATERIALS AND PROCESSES III, PTS 1 AND 2, 2013, 395-396 : 284 - +
  • [8] Effects of Cold Deformation and Aging Process on Precipitation Behavior and Mechanical Properties of Fe-18Cr-18Mn-0.63N High-Nitrogen Austenitic Stainless Steel
    Shi Feng
    Li XiaoWu
    Qi Yang
    Liu ChunMing
    STEEL RESEARCH INTERNATIONAL, 2013, 84 (10) : 1034 - 1039
  • [9] Research on the Thermal Plasticity of the 18Mn-18Cr-0.77N-2Mo High Nitrogen Austenitic Stainless Steel
    Li, Wan-ming
    Li, Hua-bing
    Jiang, Zhou-hua
    TMS 2010 139TH ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 3: GENERAL PAPER SELECTIONS, 2010, : 347 - 355
  • [10] Pitting susceptibility and semiconducting properties of passive films of 18Cr-18Mn-2Mo-0.9N high nitrogen austenitic stainless steel
    Bing, Li Hua
    Hua, Jiang Zhou
    Zhen, Li
    Rui, Zhang Zu
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES II, PTS 1 AND 2, 2009, 79-82 : 993 - 996