Bactericidal Activity of Copper and Niobium–Alloyed Austenitic Stainless Steel

被引:0
|
作者
M. I. Baena
M. C. Márquez
V. Matres
J. Botella
A. Ventosa
机构
[1] University of Sevilla,Department of Microbiology and Parasitology, Faculty of Pharmacy
[2] Acerinox,undefined
[3] S.A.,undefined
来源
Current Microbiology | 2006年 / 53卷
关键词
Niobium; Initial Cell Density; Control Slide; Stainless Steel Sample; Microbiologically Influence Corrosion;
D O I
暂无
中图分类号
学科分类号
摘要
Biofouling and microbiologically influenced corrosion are processes of material deterioration that originate from the attachment of microorganisms as quickly as the material is immersed in a nonsterile environment. Stainless steels, despite their wide use in different industries and as appliances and implant materials, do not possess inherent antimicrobial properties. Changes in hygiene legislation and increased public awareness of product quality makes it necessary to devise control methods that inhibit biofilm formation or to act at an early stage of the biofouling process and provide the release of antimicrobial compounds on a sustainable basis and at effective level. These antibacterial stainless steels may find a wide range of applications in fields, such as kitchen appliances, medical equipment, home electronics, and tools and hardware. The purpose of this study was to obtain antibacterial stainless steel and thus mitigate the microbial colonization and bacterial infection. Copper is known as an antibacterial agent; in contrast, niobium has been demonstrated to improve the antimicrobial effect of copper by stimulating the formation of precipitated copper particles and its distribution in the matrix of the stainless steel. Thus, we obtained slides of 3.8% copper and 0.1% niobium alloyed stainless steel; subjected them to three different heat treatment protocols (550°C, 700°C, and 800°C for 100, 200, 300, and 400 hours); and determined their antimicrobial activities by using different initial bacterial cell densities and suspending solutions to apply the bacteria to the stainless steels. The bacterial strain used in these experiments was Escherichia coli CCM 4517. The best antimicrobial effects were observed in the slides of stainless steel treated at 700°C and 800°C using an initial cell density of approximately 105 cells ml−1 and phosphate-buffered saline as the solution in which the bacteria came into contact with copper and niobium–containing steel.
引用
收藏
页码:491 / 495
页数:4
相关论文
共 50 条
  • [1] Bactericidal activity of copper and niobium-alloyed austenitic stainless steel
    Baena, M. I.
    Marquez, M. C.
    Matres, V.
    Botella, J.
    Ventosa, A.
    CURRENT MICROBIOLOGY, 2006, 53 (06) : 491 - 495
  • [2] ELECTROCHEMICAL CHARACTERIZATION OF VACUUM SINTERED COPPER ALLOYED AUSTENITIC STAINLESS-STEEL
    DEFLORIAN, F
    CIAGHI, L
    KAZIOR, J
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1992, 43 (09): : 447 - 452
  • [4] The corrosion resistance of austenitic stainless steel, alloyed with nitrogen
    Vehovar, L
    Vehovar, A
    Tandler, M
    METALURGIJA, 2001, 40 (04): : 195 - 200
  • [5] Austenitic-ferritic stainless steel containing niobium
    Itman Filho, Andre
    Cardoso, Wandercleiton da Silva
    Gontijo, Leonardo Cabral
    da Silva, Rosana Vilarim
    Casteletti, Luiz Carlos
    REM-REVISTA ESCOLA DE MINAS, 2013, 66 (04) : 467 - 471
  • [7] CREEP MECHANISMS IN A VANADIUM ALLOYED AUSTENITIC STAINLESS-STEEL
    BORGGREEN, K
    THOLEN, AR
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (11): : 1615 - 1620
  • [8] Peculiarities of DRX in a Highly-Alloyed Austenitic Stainless Steel
    Dolzhenko, Pavel
    Tikhonova, Marina
    Kaibyshev, Rustam
    Belyakov, Andrey
    MATERIALS, 2021, 14 (14)
  • [9] Development of stainless austenitic steel alloyed with carbon plus nitrogen
    Tyshchenko, A. I.
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 2006, 28 : 225 - 233
  • [10] Liquid phase sintering of a boron alloyed austenitic stainless steel
    Molinari, A.
    Menapace, C.
    Kazior, J.
    Pieczonka, T.
    PROGRESS IN POWDER METALLURGY, PTS 1 AND 2, 2007, 534-536 : 553 - +