摘要
Supersolidus Liquid Phase Sintering of a high refractory metal Ni-based superalloy revealed that the liquid fraction and associated grain growth behaviour was dependent on the time at a given sintering temperature. This also led to a time dependence of part distortion and slumping. An existing SLPS model was modified to account for time dependent densification and distortion and compared to experimental measurements. Model and experimental agreement were very good and indicated no distortion after sintering at 1340 °C for 120 minutes, a transition to distortion after 30 to 45 minutes at 1345 °C and nearly immediate distortion at 1350 °C. These results indicate that a sintering time-temperature processing window can be defined where densification can be maximized without unwanted component distortion.
引用
收藏
页码:3158 / 3165
页数:7
相关论文
共 42 条
  • [1] Sintering Time Dependent Supersolidus Liquid Phase Sintering Behaviour of a Metal Injection Molded Nickel-Base Superalloy
    Rayner, Addison J.
    Corbin, Stephen F.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2022, 53 (08): : 3158 - 3165
  • [2] Grain growth activation during supersolidus liquid phase sintering in a metal injection molded nickel-base superalloy
    Rayner, Addison J.
    Corbin, Stephen F.
    MATERIALS TODAY COMMUNICATIONS, 2021, 26
  • [3] Supersolidus liquid phase sintering process for injection molded TiAl
    Zhao, Liming
    Qu, Xuanhui
    Li, Shiqiong
    He, Xinbo
    Fenmo Yejin Jishu/Powder Metallurgy Technology, 2008, 26 (02): : 134 - 137
  • [4] Supersolidus liquid phase sintering of injection molded M2 tool steel
    Myers, NS
    German, RM
    INTERNATIONAL JOURNAL OF POWDER METALLURGY, 1999, 35 (06): : 45 - 51
  • [5] Supersolidus liquid phase sintering of injection molded M2 tool steel
    Myers, Neal S.
    German, Randall M.
    International Journal of Powder Metallurgy (Princeton, New Jersey), 1999, 35 (06): : 45 - 51
  • [6] Supersolidus Liquid Phase Sintering Modeling of Inconel 718 Superalloy
    David Levasseur
    Mathieu Brochu
    Metallurgical and Materials Transactions A, 2016, 47 : 869 - 876
  • [7] Supersolidus Liquid Phase Sintering Modeling of Inconel 718 Superalloy
    Levasseur, David
    Brochu, Mathieu
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2016, 47A (02): : 869 - 876
  • [8] Supersolidus liquid phase sintering of moulded metal components
    Chan, JL
    Alcock, JR
    Stephenson, DJ
    JOURNAL OF MATERIALS SCIENCE, 1998, 33 (21) : 5131 - 5136
  • [9] Supersolidus liquid phase sintering of moulded metal components
    J. L. Chan
    J. R. Alcock
    D. J. Stephenson
    Journal of Materials Science, 1998, 33 : 5131 - 5136
  • [10] Supersolidus-transient liquid phase sintering using superalloy powders
    Tandon, Rajiv
    German, Randall M.
    International Journal of Powder Metallurgy (Princeton, New Jersey), 1994, 30 (04): : 435 - 443