Effect of Laser Shock Peening on Commercially Pure Titanium-1 Weldment Fabricated by Gas Tungsten Arc Welding Technique

被引:0
|
作者
Sandeep Varin
Mayank Agarwal
Aditya Chugh
M. Manikandan
S. Prabhakaran
S. Kalainathan
Pratik Shukla
Jonathan Lawrence
N. Arivazhagan
机构
[1] VIT,School of Mechanical Engineering
[2] VIT,Center for Crystal Growth
[3] Coventry University,School of Mechanical, Aerospace and Automotive Engineering
关键词
Commercial pure titanium; Residual stress; Laser shock peening; Gas tungsten arc welding;
D O I
暂无
中图分类号
学科分类号
摘要
This research work investigates the effect of laser shock peening (LSP) on commercially pure titanium grade 1 (CP Ti-1) weldment. The welding was done using gas tungsten arc welding (GTAW) with ERTi-2 filler wire. LSP was carried out on the cap surface of the weldment. The optical microstructure showed the Widmanstatten-type martensitic structure in the fusion zone (as-welded). The LSP fusion zone showed a refined microstructure compared to that of as-welded condition. Scanning electron microscope (SEM) of LSP weldment showed the indentation on the surface of the weld. This was a result of the surface ablation that occurred during LSP. X-ray diffraction analysis showed the absence of transformation of phases in the weldment. A reduction of 14.8% of crystalline size was observed in LSP weldment. A higher compressive residual stress was observed in LSP weldment than the as-welded condition. Tensile test showed the occurrence of failure in the base metal region in the case of LSP weldment, as against the failure in the case of as-welded condition in the fusion zone.
引用
收藏
页码:1569 / 1573
页数:4
相关论文
共 50 条
  • [1] Effect of Laser Shock Peening on Commercially Pure Titanium-1 Weldment Fabricated by Gas Tungsten Arc Welding Technique
    Varin, Sandeep
    Agarwal, Mayank
    Chugh, Aditya
    Manikandan, M.
    Prabhakaran, S.
    Kalainathan, S.
    Shukla, Pratik
    Lawrence, Jonathan
    Arivazhagan, N.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (06) : 1569 - 1573
  • [2] Keyhole gas tungsten arc welding of commercially pure zirconium
    Lathabai, S.
    Jarvis, B. L.
    Barton, K. J.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2008, 13 (06) : 573 - 581
  • [3] Effect of laser shock peening on microstructural, mechanical and corrosion properties of laser beam welded commercially pure titanium
    Chattopadhyay, Angshuman
    Muvvala, Gopinath
    Sarkar, Sagar
    Racherla, Vikranth
    Nath, Ashish Kumar
    OPTICS AND LASER TECHNOLOGY, 2021, 133
  • [4] Effect of laser shock peening on microstructural, mechanical and corrosion properties of laser beam welded commercially pure titanium
    Chattopadhyay, Angshuman
    Muvvala, Gopinath
    Sarkar, Sagar
    Racherla, Vikranth
    Nath, Ashish Kumar
    Optics and Laser Technology, 2021, 133
  • [5] Development of Thick-Section Commercially Pure Titanium Welds using Gas Tungsten Arc Welding Process
    Harikrishna G.
    Pavan A.H.V.
    Swamy M.
    Devi R.S.R.
    Journal of The Institution of Engineers (India): Series D, 2024, 105 (01) : 201 - 210
  • [6] Comparison of keyhole and conventional gas tungsten arc welds in commercially pure titanium
    Lathabai, S
    Jarvis, BL
    Barton, KJ
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 299 (1-2): : 81 - 93
  • [7] Phase transformations mechanism in commercially pure titanium subjected to multiple laser shock peening
    Li, Lei
    Jia, Weiju
    Ji, Vincent
    SURFACE & COATINGS TECHNOLOGY, 2022, 450
  • [8] On the Use of Gas Metal Arc Welding for Manufacturing Beams of Commercially Pure Titanium and a Titanium Alloy
    Patnaik, Anil
    Poondla, Narendra
    Bathini, Udaykar
    Srivatsan, T. S.
    MATERIALS AND MANUFACTURING PROCESSES, 2011, 26 (02) : 311 - 318
  • [9] Electron beam welding, laser beam welding and gas tungsten arc welding of titanium sheet
    Qi, YL
    Deng, J
    Hong, Q
    Zeng, LY
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 280 (01): : 177 - 181
  • [10] Evaluation of Anodic Behavior of Commercially Pure Titanium in Tungsten Inert Gas and Laser Welds
    Orsi, Iara Augusta
    Raimundo, Larica B.
    Bezzon, Osvaldo Luiz
    de Arruda Nobilo, Mauro Antonio
    Kuri, Sebastiao E.
    Rovere, Carlos Alberto D.
    Pagnano, Valeria Oliveira
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2011, 20 (08): : 628 - 631