High Temperature Erosion-Corrosion of Wear Protection Materials

被引:1
|
作者
Varga M. [1 ]
Rojacz H. [1 ]
Widder L. [1 ]
Antonov M. [2 ]
机构
[1] AC2T research GmbH, Wiener Neustadt
[2] School of Engineering: Department of Mechanical and Industrial Engineering, Tallinn University of Technology (TalTech), Tallinn
关键词
Erosion-corrosion; High temperature; Mechanically mixed layer (MML); Metal matrix composite (MMC); Solid particle erosion; Tribo-layer;
D O I
10.1007/s40735-021-00504-9
中图分类号
学科分类号
摘要
Solid particle erosion at high temperatures (HT) is a serious issue in various industrial applications, like ventilators, exhaust systems of HT reactors, incineration plants. Due to HT and process gases, erosion is accompanied with oxidation/corrosion. When erosive wear emerges as a lifetime-limiting process, wear protective materials are applied. The combined HT erosive and oxidative attack on these is of major interest and not sufficiently understood for typical wear protection materials. Thereto, we selected three standard wear protection materials and investigated their erosive-corrosive behaviour at 650 °C. Herein used solutions include an alumina, a hypereutectic metal matrix composite (MMC) and an oxidation resistant austenitic steel. Each material was tested in a HT centrifugal solid particle erosion test rig applying 45° and 90° impingement angle. Additional comparative tests were performed at room temperature. A high particle velocity of 65 m/s, as is typical in exhaust pipes, was selected for this study. Extensive post-test analyses of the surface changes and oxidation behaviour were performed to identify the main wear mechanisms. It was found that the alumina exhibited highest wear loss at all conditions investigated, due to its brittle behaviour. Oxidation played no role for this material. The MMC showed pronounced oxidation intensifying the wear loss at HT. Also, the austenite showed extensive tribo-oxidative behaviour, albeit due to erosive particle embedding and formation of an in situ wear protective tribo-layer, the most favourable results were obtained. At oblique impact it showed 3-times less volumetric wear loss than the alumina, and at normal impact 11-times less. © 2021, The Author(s), under exclusive licence to Springer Nature Switzerland AG.
引用
收藏
相关论文
共 50 条
  • [1] EROSION-CORROSION AND WEAR
    BIRKS, N
    PETTIT, FS
    RISHEL, DM
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C9): : 667 - 678
  • [2] Experimental study of erosion-corrosion wear of materials: A review
    Prozhega, M. V.
    Tatus, N. A.
    Samsonov, S. V.
    Kolyuzhni, O. Yu
    Smirnov, N. N.
    JOURNAL OF FRICTION AND WEAR, 2014, 35 (02) : 155 - 160
  • [3] Experimental study of erosion-corrosion wear of materials: A review
    M. V. Prozhega
    N. A. Tatus
    S. V. Samsonov
    O. Yu. Kolyuzhni
    N. N. Smirnov
    Journal of Friction and Wear, 2014, 35 : 155 - 160
  • [4] High temperature erosion-corrosion of superheater materials and coatings in chlorine containing environments
    Uusitalo, M
    Kaipiainen, M
    Vuoristo, P
    Mäntylä, T
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 5, PTS 1 AND 2, 2001, 369-3 : 475 - 482
  • [5] HIGH-TEMPERATURE EROSION AND EROSION-CORROSION IN COAL COMBUSTION SYSTEMS
    STRINGER, J
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1983, 130 (03) : C105 - C105
  • [6] HIGH-TEMPERATURE EROSION-CORROSION OF ALLOYS.
    Anon
    Electric Power Research Institute, Coal Combustion Systems Division, (Report) EPRI CS, 1980, (1454):
  • [7] Elimination of the high-pressure heater tube erosion-corrosion wear
    Belyakov, V.I.
    Bulatov, V.A.
    Kozlovskikh, I.I.
    Trifonov, N.N.
    Teploenergetika, 1997, (05): : 58 - 60
  • [8] Nanocrystalline Cermet Coatings for Erosion-Corrosion Protection
    Tiwari, Abhishek
    Seman, Saravanan
    Singh, Gaurav
    Jayaganthan, Rengaswamy
    COATINGS, 2019, 9 (06):
  • [9] DESIGN OF REFRACTORIES FOR RESISTANCE TO HIGH-TEMPERATURE EROSION-CORROSION
    VOJNOVICH, T
    AMERICAN CERAMIC SOCIETY BULLETIN, 1976, 55 (04): : 457 - 457
  • [10] INTERPRETATION OF WASTAGE MECHANISMS OF MATERIALS EXPOSED TO ELEVATED-TEMPERATURE EROSION-CORROSION USING EROSION-CORROSION MAPS AND COMPUTER-GRAPHICS
    STACK, MM
    BRAY, L
    WEAR, 1995, 186 (01) : 273 - 283